摘要:
The present invention discloses a process for forming a biaxially oriented film. The process includes first selecting a polyolefin resin wherein said polyolefin resin comprises a linear low density polyethylene resin characterized by having from 9 to 35 weight percent of the total weight of linear low density polyethylene resin eluting from a CEF at a temperature greater than 97.0° C.; and further characterized by having a CDR of from 33 to 80 and a Mw Ratio of from 0.15 to 0.45. Next a film is formed from the polyolefin resin selected in the first step. Finally the film formed in the second step is oriented in a sequential manner. The films produced by this process are characterized by having an ultimate elongation at least 1.5 times greater in the MD as compared to the CD and the 2% secant modulus is a least 1.25 times greater in the CD as compared to the MD. The films are further characterized by having free residual shrinkage of less than 10% in the MD and less than 10% in the CD when exposed to a temperature of 90° C. for 10 minutes.
摘要:
The invention is related to an ethylene/α-olefin interpolymer having at least a hard segment and at least a soft segment. The soft segment contains a higher amount of comonomers than the hard segment. The hard segment has low crystallinity. The copolymer has a number of unique characteristics disclosed herein. ethylene/α-olefin interpolymers containing low crystallinity hard blocks.
摘要:
The present disclosure provides propylene-based polymers which exhibit a strain hardening distribution factor that is less than zero and/or a strain hardening factor greater than 1.5. The propylene-based polymers are rheology-modified by way of silane coupling to improve melt strength.
摘要:
An ethylene-based polymer composition has been discovered and is characterized by a Comonomer Distribution Constant greater than about 45. The new ethylene-based polymer compositions are useful for making many articles, especially including films. Formulations made into films comprising the new polymers are also disclosed, especially blends with synthetic polymer like LDPE where the % LDPE is less than 50% in which the MD shrink tension is greater than 15 cN, puncture is greater than 75 ft-lb/in3, and haze is less than 20%. The polymers are made using a metal complex of a polyvalent aryloxyether.
摘要:
A lubricant composition comprises a base oil and a viscosity modifier including an ethylene/α-olefin interpolymer. The ethylene/α-olefin interpolymer has at least a hard segment and at least a soft segment. The soft segment contains a higher amount of comonomers than the hard segment. The hard segment has low crystallinity. The copolymer has a number of unique characteristics disclosed herein. Such copolymers offer the possibility of improved low temperature performance and flexibility in formulating motor oil, gear lubricants and greases, etc.
摘要:
The invention is related to catalytic olefin block copolymers with a controlled block sequence distribution and at least one low crystallinity hard block. The block copolymer has a number of unique characteristics disclosed here.
摘要:
The instant invention is a sealant composition, method of producing the same, articles made therefrom, and method for forming such articles. The sealant composition according to the present invention comprises: (a) from 70 to 99.5 percent by weight of an ethylene/α-olefin interpolymer composition, based on the total weight of the sealant composition, wherein said ethylene/α-olefin interpolymer composition comprises an ethylene/α-olefin interpolymer, wherein ethylene/α-olefin interpolymer has a Comonomer Distribution Constant (CDC) in the range of from 15 to 250, and a density in the range of from 0.875 to 0.963 g/cm3, a melt index (I2) in a range of from 0.2 to 20 g/10 minutes, and long chain branching frequency in the range of from 0.02 to 3 long chain branches (LCB) per 1000C; (b) from 0.5 to 30 percent by weight of a propylene/α-olefin interpolymer composition, wherein said propylene/α-olefin interpolymer composition comprises a propylene/α-olefin copolymer or a propylene/ethylene/butene terpolymer, wherein said propylene/α-olefin copolymer has a crystallinity in the range of from 1 percent by weight to 30 percent by weight, a heat of fusion in the range of from 2 Joules/gram to 50 Joules/gram, and a DSC melting point in the range of 25° C. to 110° C.
摘要:
The present invention provides an ethylene-based polymer composition characterized by a Comonomer Distribution Constant in the range of from greater than 45 to less than 400, wherein the composition has less than 120 total unsaturation unit/1,000,000C, and method of producing the same.
摘要:
The invention is related to catalytic olefin block copolymers with a controlled block sequence distribution and at least one low crystallinity hard block. The block copolymer has a number of unique characteristics disclosed here.
摘要:
The instant invention is a sealant composition, method of producing the same, articles made therefrom, and method for forming such articles. The sealant composition according to the present invention comprises: (a) from 70 to 99.5 percent by weight of an ethylene/α-olefin interpolymer composition, based on the total weight of the sealant composition, wherein said ethylene/α-olefin interpolymer composition comprises an ethylene/α-olefin interpolymer, wherein ethylene/α-olefin interpolymer has a Comonomer Distribution Constant (CDC) in the range of from 15 to 250, and a density in the range of from 0.875 to 0.963 g/cm3, a melt index (I2) in a range of from 0.2 to 20 g/10 minutes, and long chain branching frequency in the range of from 0.02 to 3 long chain branches (LCB) per 1000 C; (b) from 0.5 to 30 percent by weight of a propylene/α-olefin interpolymer composition, wherein said propylene/α-olefin interpolymer composition comprises a propylene/α-olefin copolymer or a propylene/ethylene/butene terpolymer, wherein said propylene/α-olefin copolymer has a crystallinity in the range of from 1 percent by weight to 30 percent by weight, a heat of fusion in the range of from 2 Joules/gram to 50 Joules/gram, and a DSC melting point in the range of 25° C. to 110° C.