Abstract:
The present invention relates to a method of acrylonitrile-butadiene-styrene (ABS) rubber latex, and the acrylonitrile-butadiene-styrene (ABS) latex is prepared by graft-polymerizing butadiene rubber with the monomers of acrlylonitrile and styrene through emulsion-polymerization, so that the ABS rubber latex of the present invention has high solid content. The method of ABS rubber latex of the present invention comprises the step of emulsion-polymerizing i) polybutadiene rubber latex; ii) aromatic vinyl compound; and iii) vinyl cyanide with the addition of a reactive emulsifier. According to the method of the present invention, the ABS rubber latex has high solid content due to a decrease in the amount of coagulated materials and film, which formed on the rubber latex during polymerization, and an increase in the production volume.
Abstract:
A method of preparing rubber substrate is provided. In the method, 50 to 95 parts by weight of conjugated diene monomer is first-polymerized, until the resulting first rubber substrate has gel content of 5 to 70 wt %. Thereafter, the first rubber substrate is second-polymerized with 5 to 50 parts by weight to obtain a second rubber substrate. The obtained second rubber substrate has higher gel content in core than outer layer.
Abstract:
The present invention relates to an optical film, comprising a copolymer that comprises (a) a (meth)acrylic monomer, (b) an aromatic vinyl monomer, (c) at least one monomer of an acid anhydride monomer and an unsaturated organic acid monomer, and (d) a vinylcyan monomer, a protection film for a polarizer, a polarizing plate fabricated therefrom, and a display device employing the same.
Abstract:
The present invention relates to a styrenic thermoplastic resin composition, and more particularly to a styrenic thermoplastic resin composition comprising a non-halogen flame-retardant having superior flame-retarding properties and impact strength.The present invention provides a flame-retarding styrenic thermoplastic resin composition comprising a) 100 weight parts of a base resin comprising i) 10 to 50 weight parts of a rubber-modified styrene-containing graft copolymer, ii) 5 to 20 weight parts of phenol novolac resin, and iii) 20 to 70 weight parts of a styrene-containing copolymer; and b) 5 to 20 weight parts of an aromatic phosphate. In addition, the a) base resin may further comprise iv) 10 to 40 weight parts of a thermoplastic polyurethane resin.
Abstract:
The present invention relates to a styrenic thermoplastic resin composition, and more particularly to a styrenic thermoplastic resin composition comprising a non-halogen flame-retardant having superior flame-retarding properties and impact strength. The present invention provides a flame-retarding styrenic thermoplastic resin composition comprising a) 100 weight parts of a base resin comprising i) 10 to 50 weight parts of a rubber-modified styrene-containing graft copolymer, ii) 5 to 20 weight parts of phenol novolac resin, and iii) 20 to 70 weight parts of a styrene-containing copolymer; and b) 5 to 20 weight parts of an aromatic phosphate. In addition, the a) base resin may further comprise iv) 10 to 40 weight parts of a thermoplastic polyurethane resin.
Abstract:
The present invention relates to a nanocomposite thermoplastic resin composition with flame resistance comprising a basic resin mixture, which comprises a rubber-modified styrene-containing graft copolymer, a thermoplastic polyamide resin and a styrene-containing copolymer, a compatibilizer, a melamine based flame retardant and an organic layered silicate. The nanocomposite thermoplastic resin composition of the present invention offers superior flame resistance without comprising a halogen based flame retardant.
Abstract:
The present invention relates to a styrenic thermoplastic resin composition, and more particularly to a styrenic thermoplastic resin composition comprising a non-halogen flame-retardant having superior flame-retarding properties and impact strength. The present invention provides a flame-retarding styrenic thermoplastic resin composition comprising a) 100 weight parts of a base resin comprising i) 10 to 50 weight parts of a rubber-modified styrenic-containing graft copolymer, ii) 5 to 20 weight parts of phenol novolac resin, and iii) 20 to 70 weight parts of a styrene-containing copolymer; and b) 5 to 20 weight parts of an aromatic phosphate. In addition, the a) base resin may further comprise iv) 10 to 40 weight parts of a thermoplastic polyurethane resin.
Abstract:
The present invention relates to an acrylic rubber-modified copolymer and the styrenic thermoplastics composition using the same. More particularly, the present invention relates to the styrenic thermoplastics composition having superior appearance and thermoformability, which is obtained by adding 0.5-20 parts by weight of an acrylic rubber-modified copolymer having a rubber particle size ranging from 800 to 6, 000 Åto 100 parts by weight of a resin of 10-50 parts by weight of a graft copolymer comprising rubber-modified styrene and 30-70 parts by weight of a copolymer comprising styrene.
Abstract:
The present invention relates to a thermoplastic resin composition and a preparation method of the same, more precisely, a thermoplastic resin composition containing acrylate-styrene-acrylonitrile (ASA) graft copolymer resin, aromatic polycarbonate resin, aromatic vinyl compound and vinyl cyan compound copolymer resin and styrene-acrylonitrile graft maleic anhydride (SAN-g-MAN) to improve exterior physical properties such as scratch resistance, surface gloss, colorability, weather resistance, etc, and a preparation method of the same.
Abstract:
A rubber-modified flame resistant styrene resin composition, which has superior heat stability and weather resistance to prevent discoloration and deterioration due to heat or light and is processed under various molding condition, is provided. The rubber-modified flame resistant styrene resin composition includes a rubber-modified styrene resin, flame retardant comprising compounds selected from a group consisting of tetrabromobisphenol-A-bis(2,3-dibromopropylether), hexabromocyclododecane and a mixture thereof, and brominated epoxy oligomer, and calcium stearate as a lubricant.