摘要:
A nickel-based braze composition is described, containing nickel, palladium, and restricted amounts of boron and silicon. The composition can also contain tantalum, titanium, and zirconium, as well as aluminum, chromium, and cobalt. A method for joining two metal components, using the braze composition, is also described. The braze composition can also be used to fill cracks or other cavities in a component, e.g., a gas turbine part formed from a nickel-based superalloy. Articles of manufacture which contain the braze composition are also described.
摘要:
A flow regulating article is provided. The flow regulating article, in an exemplary embodiment, includes a patterned structure. The patterned structure includes a shape memory alloy capable of changing shape at predetermined temperatures.
摘要:
A composition and process for a nickel-base alloy that exhibits a desirable balance of high-temperature strength and weldability, as well as other properties suitable for high temperature applications. These properties are achieved with an alloy in which the combined level of titanium, aluminum, niobium, and tantalum is carefully controlled. The alloy consists of, by weight, 10 to less than 20% chromium, 15 to 20% cobalt, less than 1.0% molybdenum, 2.5 to 5% tungsten, 1.1 to 1.5% niobium, less than 0.5% tantalum, 3.0 to 3.9% titanium, 2.5 to 3.4% aluminum, 0.07 to 0.15% carbon, less than 0.06% zirconium, less than 0.03% boron, the balance nickel and impurities.
摘要:
An abradable coating composition for use on shrouds in gas turbine engines or other hot gas path metal components exposed to high temperatures containing an initial porous coating phase created by adding an amount of inorganic microspheres, preferably alumina-ceramic microballoons, to a base metal alloy containing high Al, Cr or Ti such as β-NiAl or, alternatively, MCrAlY that serves to increase the brittle nature of the metal matrix, thereby increasing the abradability and oxidation resistance of the coating at elevated temperatures. Coatings having a total open and closed porosity of between 20% and 55% by volume due to the presence of ceramic microballoons ranging in size from about 10 microns to about 200 microns have been found to exhibit excellent abradability for applications involving turbine shroud coatings. An abradable coating thickness in the range of between 40 and 60 ml provides improved performance for turbine shrouds exposed to gas temperatures between 1380° F. and 1800° F. Abradable coatings in accordance with the invention can be used for new metal components or to repair existing equipment. The coatings can be applied to the metal shroud using thermal spray, processes that integrate sintering and brazing, or direct write techniques.
摘要:
Disclosed herein too is a method for manufacturing an article comprising casting an alloy comprising about 1.5 to about 4.5 weight percent aluminum; about 1.5 to about 4.5 weight percent titanium; up to about 3 weight percent niobium; about 14 to about 28 weight percent chromium; about 10 to 23 weight percent cobalt; about 1 to about 3 weight percent of tungsten, rhenium, ruthenium, molybdenum, or a combination thereof; about 0.02 to about 0.15 weight percent of carbon; about 0.001 to about 0.025 weight percent of boron; up to 0.2 weight percent of zirconium, hafnium, or a combination thereof; into a mold.
摘要:
A nickel-based braze composition is described, containing nickel, palladium, and restricted amounts of boron and silicon. The composition can also contain tantalum, titanium, and zirconium, as well as aluminum, chromium, and cobalt. A method for joining two metal components, using the braze composition, is also described. The braze composition can also be used to fill cracks or other cavities in a component, e.g., a gas turbine part formed from a nickel-based superalloy. Articles of manufacture which contain the braze composition are also described.
摘要:
An alloy for use in high temperature applications is presented. The alloy comprises, in atom percent, at least about 50% rhodium (Rh); at least about 5% of a metal selected from the group consisting of platinum (Pt), palladium (Pd), and combinations thereof; from about 5% to about 24% ruthenium (Ru); and from about 1% to about 40% chromium (Cr); wherein the alloy comprises less than about 50% by volume of an A3-structured phase, and wherein the quantity defined by the expression ([Cr]+2[Ru]) is in the range from about 25% to about 50%, where [Ru] and [Cr] are the atom percentages of ruthenium and chromium in the alloy, respectively. Articles comprising the alloy and methods employing the alloy for repairing articles are also presented.
摘要:
The present invention provides a method and system for authenticating a network equipment (NE). When the NE is authenticated, the integrity checking result recorded in the trust environment (TE) of the network equipment is added for joint judgment to determine finally whether to initiate the authentication request or to respond with the authentication access. Only when both of the received access authentication request and the integrity checking result recorded in the TE of the network equipment are correct, the NE responds with the authentication success. And only when the integrity checking result recorded in the TE of the NE is correct, the NE actively initiates a valid access authentication request. Thus only when the integrity of the NE is correct, authentication for the NE is passed, therefore the secure authentication for the NE is ensured, and the possibility that the illegal device or tampered device passes the authentication is eliminated.
摘要:
A computer implemented method, apparatus, and computer program product for booting a computer using a boot list. A determination is made as to whether a boot list is present in a non-volatile memory of the computer. The boot list is a set of paths, in which each path in the boot list is a path of a storage device. If the boot list is not present, a search is performed for the boot list in a reserved area of each storage device in a set of storage devices. When the boot list is found in the reserved area of a storage device in the set of storage devices, the boot list is copied from the reserved area of the storage device in the set of storage devices to form a copied boot list. The copied boot list is stored in the non-volatile memory to form a stored boot list. The computer is booted using the stored boot list in the non-volatile memory.
摘要:
An embodiment of the present invention provides a space-time block code (STBC) transmission method for 4 transmit antennas, comprising adding two 2×2 orthogonal pre-coding before a two Alamouti transmission for a 4 transmit antennas scheme.