摘要:
The present invention is a composition suitable for use as an antioxidant for polyolefin resins, said composition having a structure corresponding to the formula: wherein R1, R2, R3, R4, R5 and R6 are selected from a hydrogen or an alkyl group having 1 to 24 carbon atoms, or a branched alkyl group having 1 to 24 carbon atoms, or a cyclic alkyl group with 1 to 24 carbon atoms; wherein said composition has a peak decomposition temperature of less than 280° C. and a total decomposition energy which is endothermic or if exothermic, releases no more energy; than 40 kJoules/mole.
摘要:
An ethylene-based polymer composition has been discovered and is characterized by a Comonomer Distribution Constant greater than about 45. The new ethylene-based polymer compositions are useful for making many articles, especially including films. Formulations made into films comprising the new polymers are also disclosed, especially blends with synthetic polymer like LDPE where the % LDPE is less than 50% in which the MD shrink tension is greater than 15 cN, puncture is greater than 75 ft-lb/in3, and haze is less than 20%. The polymers are made using a metal complex of a polyvalent aryloxyether.
摘要:
The present invention is a method for producing a film particularly well suited for shrink film applications, said method comprising the steps of selecting a target polyethylene resin and then increasing the melt strength of the polyethylene resin by reacting the polyethylene resin with an alkoxy amine derivative, and then forming a film from the reacted target polyethylene.
摘要:
An ethylene-based polymer composition has been discovered and is characterized by a Comonomer Distribution Constant greater than about 45. The new ethylene-based polymer compositions and blends thereof with one or more polymers, such as LDPE, are useful for making many articles, especially including films.
摘要:
The instant invention provides an ethylene/alpha-olefin interpolymer suitable for use in shrinkage film applications, and articles made therefrom. The ethylene/alpha-olefin interpolymer according to the present invention has a CDBI of less than 60%, and comprises at least two fractions in crossfractionation of the ethylene/alpha-olefin interpolymer, eluting from 85° C. to 90° C. and from 90° C. to 95° C., comprising a weight fraction ratio of >0.68 and a molecular weight homogeneity index of greater than 0.65; wherein the weight fraction ratio is the ratio of the weight of polymer in each fraction divided by the weight of polymer eluting between 95° C. and 100° C. and the molecular weight homogeneity index is the ratio of the weight average molecular weight of the polymer in the fraction divided by the weight average molecular weight of the polymer eluting between 95° C. and 100° C., and wherein the ethylene/alpha-olefin interpolymer has a density in the range of 0.920 to 0.940 g/cm3.
摘要:
A polymer comprises units derived from ethylene and poly(alkoxide) the polymer having at least 0.15 units of amyl groups per 1000 carbon atoms as determined by 13C Nuclear Magnetic Resonance (NMR).
摘要:
A polymer comprises units derived from ethylene and polyalkylene, the polymer having at least 0.15 units of amyl groups per 1000 carbon atoms as determined by 13C Nuclear Magnetic Resonance (NMR).
摘要:
The instant invention provides an ethylene/alpha-olefin interpolymer suitable for use in shrinkage film applications, and articles made therefrom. The ethylene/alpha-olefin interpolymer according to the present invention has a CDBI of less than 60%, and comprises at least two fractions in crossfractionation of the ethylene/alpha-olefin interpolymer, eluting from 85° C. to 90° C. and from 90° C. to 95° C., comprising a weight fraction ratio of >0.68 and a molecular weight homogeneity index of greater than 0.65; wherein the weight fraction ratio is the ratio of the weight of polymer in each fraction divided by the weight of polymer eluting between 95° C. and 100° C. and the molecular weight homogeneity index is the ratio of the weight average molecular weight of the polymer in the fraction divided by the weight average molecular weight of the polymer eluting between 95° C. and 100° C., and wherein the ethylene/alpha-olefin interpolymer has a density in the range of 0.920 to 0.940 g/cm3.
摘要:
The instant invention provides a polyethylene blend composition suitable for blown film, method of producing the same, and films made therefrom. The polyethylene blend composition suitable for blown film according to the present invention comprises the melt blending product of: (a) less than or equal to 4 percent by weight of a low density polyethylene (LDPE) having a density in the range of from 0.915 to 0.935 g/cm3, and a melt index (I2) in the range of from greater than 0.8 to less than or equal to 5 g/10 minutes, and a molecular weight distribution (Mw/Mn) in the range of from 6 to 10; (b) 90 percent or greater by weight of a heterogenous linear low density polyethylene (hLLDPE) having a density in the range of from 0.917 to 0.950 g/cm3, and a melt index (I2) in the range of from 0.1 to less than or equal to 5 g/10 minutes; (c) optionally a hydrotalcite based neutralizing agent; (d) optionally one or more nucleating agents; and (e) optionally one or more antioxidants. When the polyethylene blend-composition is formed into a film via blown film process, the output rate is improved at least 6 percent relative to a similar linear low density polyethylene.
摘要:
The invention provides a polymer comprising units derived from ethylene and siloxane, polymer having at least 0.15 units of amyl groups per 1000 carbon atoms as determined by 13C Nuclear Magnetic Resonance (NMR).