Abstract:
The present invention is directed to a polypropylene composition (C) comprising a heterophasic propylene copolymer and an inorganic filler, the use of said polypropylene composition (C) for the production of a foamed article and a foamed article obtained from said polypropylene composition (C).
Abstract:
The present invention relates to a polypropylene based composition comprising:(A) from 40.0 to 85.0 wt % of a heterophasic propylene copolymer having a content of xylene cold soluble (XCS) fraction in the range of 15 wt % to 35 wt %, based on the total weight of the heterophasic propylene copolymer;(B) from 5.0 to 15.0 wt % of a terpolymer of propylene with ethylene and 1-butene comonomer units having a melting temperature Tm as measured in differential scanning calorimetry (DSC) of less than 140° C.; (C) from 5.0 to 25.0 wt % of an ethylene copolymer with alpha-olefin comonomer units having from 4 to 12 carbon atoms with a density of from 850 kg/m3 to 900 kg/m3; and(D) from 5.0 to 25.0 wt % of an inorganic filler, wherein the amounts of components (A), (B), (C), and (D) are all based on the total weight amount of the polypropylene based composition, said polypropylene based composition having a melt flow rate (MFR2) as measured at 230° C. and 2.16 kg load in accordance with ISO 1133 in the range of 2.0 g/10 min to 20 g/10 min, an article comprising said polypropylene based composition and the use of said terpolymer (B) for reducing the paint adhesion failure of an article comprising said polypropylene based composition.
Abstract:
A heterophasic propylene copolymer (HECO) comprising a polypropylene matrix having a melt flow rate MFR2 (230° C.) in the range of 45 to 75 g/10 min for the preparation of molde articles with low CLTE.
Abstract:
The present invention is directed to a polypropylene composition, said polypropylene composition comprising two different polypropylene fractions (PP1) and (PP2), wherein the first polypropylene (PP1) has a weight molecular weight Mw in the range of above 45 kg/mol to below 65 kg/mol and a melting temperature of at least 140° C.
Abstract:
The present invention relates to novel polypropylene compositions suitable for automotive applications, having a good balance of mechanical properties and especially low gloss. The inventive compositions are characterized by at least two heterophasic propylene copolymers (HECOs), where at least one of the HECOs is characterized by a rather high molecular weight rubber, an ethylene-a-olefin elastomer (EOE) having a rather low melt flow rate MFR2 (190° C.) and a specific ratio between the MFR of the ethylene-a-olefin elastomer (EOE) and of at least one of the heterophasic propylene copolymers (HECOs).
Abstract:
The present invention is directed to a heterophasic propylene copolymer (HECO), a polyolefin composition (PO) comprising the heterophasic propylene copolymer (HECO), an automotive article comprising the heterophasic propylene copolymer (HECO) and/or the polyolefin composition (PO) and a process for the preparation of the polyolefin composition (PO) as well as the use of the heterophasic propylene copolymer (HECO) for improving the mechanical properties of a polyolefin composition (PO).
Abstract:
This invention relates to a thermoplastic polyolefin composition having a melt flow rate MFR2 (230° C.) between 20 and 100 g/10 min, to the use of such thermoplastic polyolefin composition for the production of injection molded articles, e.g. automotive parts and to injection molded articles prepared by using such thermoplastic polyolefin composition.
Abstract:
Composition comprising a heterophasic propylene copolymer and two different slip agents, namely—a fatty acid amid derivative of formula (I) wherein R1 is a C5 to C25 alkyl residue or C5 to C25 alkenyl residue, R2 is a long-chain organic residue containing at least 6 carbon atoms, and—an unsaturated fatty acid amide.
Abstract:
The present invention relates to a polyolefin composition comprising a heterophasic propylene copolymer having a MFR2 of at least 5 g/10 min and a polyethylene (PE) having a density of at least 935 kg/m3 and a melt flow rate MFR5 (190° C.) of less than 1.5 g/10 min.5
Abstract translation:本发明涉及一种聚烯烃组合物,其包含MFR 2为至少5g / 10min的多相丙烯共聚物和密度为至少935kg / m 3的聚乙烯(PE)和熔体流动速率MFR 5(190℃) 。)小于1.5 g / 10 min
Abstract:
The present invention is directed to a polypropylene composition (C) comprising a heterophasic propylene copolymer (HECO), comprising a matrix being a propylene polymer (PP1), an elastomeric propylene copolymer (EPR) being dispersed in said matrix and a nucleating agent (NU). The polypropylene composition (C) further comprises polymeric fibers (PE). The present invention is also directed to a foamed article comprising the polypropylene composition (C) and the use of polymeric fibers (PE) as an impact modifier for a heterophasic propylene copolymer (HECO).