HIGH SILICA CONTENT SUBSTRATE SUCH AS FOR USE IN THIN-FILM BATTERY
    35.
    发明申请
    HIGH SILICA CONTENT SUBSTRATE SUCH AS FOR USE IN THIN-FILM BATTERY 有权
    高二氧化硅含量基板,如用于薄膜电池

    公开(公告)号:US20160301095A1

    公开(公告)日:2016-10-13

    申请号:US14684627

    申请日:2015-04-13

    Abstract: A high silica content substrate, such as for a thin-film battery, is provided. The substrate has a high silica content, such as over 90% by weight silica, and is thin, for example less than 500 μm. The substrate may include a surface with a topography or profile that facilitates bonding with a coating layer, such as a coating of an electrochemical battery material. The high silica content substrate may be flexible, have high temperature resistance, high strength and/or be non-reactive. The substrate may be suitable for use in the high temperature environments used in many chemical deposition or formation processes, such as electrochemical battery material formation processes.

    Abstract translation: 提供高二氧化硅含量的基底,例如薄膜电池。 基板具有高的二氧化硅含量,例如超过90重量%的二氧化硅,并且薄,例如小于500μm。 衬底可以包括具有促进与涂层(例如电化学电池材料的涂层)的粘合的形貌或轮廓的表面。 高二氧化硅含量的基材可以是柔性的,具有耐高温性,高强度和/或非反应性。 衬底可适用于许多化学沉积或形成工艺中使用的高温环境,例如电化学电池材料形成工艺。

    Locally-sintered porous soot parts and methods of forming
    36.
    发明授权
    Locally-sintered porous soot parts and methods of forming 有权
    局部烧结多孔烟灰部件及成型方法

    公开(公告)号:US09452946B2

    公开(公告)日:2016-09-27

    申请号:US14057329

    申请日:2013-10-18

    Abstract: A porous soot sheet is formed using a roll-to-roll glass soot deposition and sintering process. The soot sheet formation involves depositing glass soot particles on a deposition surface to form a supported soot layer, removing the soot layer from the deposition surface to form a soot sheet, and heating a portion of the soot sheet to locally-sinter the glass soot particles and form a porous soot part having a sintered peripheral edge.

    Abstract translation: 使用辊对辊玻璃烟灰沉积和烧结工艺形成多孔烟炱片。 烟叶片形成包括在沉积表面上沉积玻璃烟灰颗粒以形成支撑的烟灰层,从沉积表面除去烟灰层以形成烟炱片,并且加热烟炱纸的一部分以将玻璃烟灰颗粒局部烧结 并形成具有烧结周边边缘的多孔烟灰部分。

    Laser sintering system and method for forming high purity, low roughness silica glass
    37.
    发明授权
    Laser sintering system and method for forming high purity, low roughness silica glass 有权
    激光烧结体系及形成高纯度,低糙度的二氧化硅玻璃的方法

    公开(公告)号:US09422187B1

    公开(公告)日:2016-08-23

    申请号:US14862771

    申请日:2015-09-23

    Abstract: A system and method for making a thin sintered silica sheet is provided. The method includes providing a soot deposition surface and forming a glass soot sheet by delivering a stream of glass soot particles from a soot generating device to the soot deposition surface. The method includes providing a sintering laser positioned to direct a laser beam onto the soot sheet and forming a sintered glass sheet from the glass soot sheet by delivering a laser beam from the sintering laser onto the glass soot sheet. The sintered glass sheet formed by the laser sintering system or method is thin, has low surfaces roughness and/or low contaminant levels.

    Abstract translation: 提供一种用于制造薄的烧结二氧化硅片的系统和方法。 该方法包括提供烟灰沉积表面并通过将烟灰发生装置的玻璃烟灰颗粒流输送到烟灰沉积表面来形成玻璃烟灰片。 该方法包括提供烧结激光器,其定位成将激光束引导到烟灰片上,并通过将来自烧结激光器的激光束输送到玻璃烟炱片上,从玻璃烟炱片形成烧结玻璃片。 通过激光烧结体系或方法形成的烧结玻璃板薄,表面粗糙度低和/或污染物含量低。