YIELD OPTIMIZATION OF POLYCARBONATE POLYOLS
    32.
    发明申请
    YIELD OPTIMIZATION OF POLYCARBONATE POLYOLS 有权
    聚碳酸酯多元醇的YIELD优化

    公开(公告)号:US20150025217A1

    公开(公告)日:2015-01-22

    申请号:US14379576

    申请日:2013-03-13

    CPC classification number: C08G64/305 C08G64/0208

    Abstract: Embodiments of the invention provide for methods of producing a polycarbonate polyol. The method includes charging a vessel with butanediol, charging the vessel with a polymerization catalyst, and adding to the vessel dimethyl carbonate at a rate of at least 2.0 g of DMC per minute per kg of BDO to produce polycarbonate polyol at a polycarbonate polyol yield of at least 80% of a theoretical yield.

    Abstract translation: 本发明的实施方案提供了生产聚碳酸酯多元醇的方法。 该方法包括用丁二醇装入容器,用聚合催化剂装入容器,并以每千克BDO每分钟至少2.0克DMC的速率向容器中加入容器中,以聚碳酸酯多元醇的产率制备聚碳酸酯多元醇 至少80%的理论产量。

    ELASTOMERS FOR PAPER MILL EQUIPMENT
    33.
    发明申请
    ELASTOMERS FOR PAPER MILL EQUIPMENT 有权
    纸机设备用弹性体

    公开(公告)号:US20140352904A1

    公开(公告)日:2014-12-04

    申请号:US14374056

    申请日:2013-02-27

    Abstract: Embodiments of the invention provide for paper mill equipment that can better withstand the conditions of a paper Mill. Embodiments encompass paper mill equipment that incorporate a polyurethane layer having a hysteresis value of less than 70% and a permanent set of less than 30%. The polyurethane layer includes a polyurethane produced by curing a mixed composition. The mixed composition includes at least a urethane prepolymer (A) and at least a curing agent (B) having an active hydrogen group (H). The urethane prepolymer (A) has at least one terminal isocyanate group and is obtained by reacting at least a polyisocyanate compound (a) with at least a polycarbonate diol compound (b) having a number average molecular weight of at least 1500 g/mol. The curing agent (B) includes at least an amine compound. The elastomer compositions are also useful to coat the acid pickling roller in the steel industry.

    Abstract translation: 本发明的实施例提供了能够更好地承受造纸厂的条件的造纸设备。 实施例包括结合具有小于70%的滞后值和小于30%的永久变形的聚氨酯层的造纸设备。 聚氨酯层包括通过固化混合组合物制备的聚氨酯。 混合组合物至少包含氨基甲酸酯预聚物(A)和至少具有活性氢基(H)的固化剂(B)。 氨基甲酸酯预聚物(A)具有至少一个末端异氰酸酯基团,并且通过使至少多异氰酸酯化合物(a)与数均分子量为至少1500g / mol的至少一种聚碳酸酯二醇化合物(b)反应而获得。 固化剂(B)至少包含胺化合物。 弹性体组合物也可用于涂覆钢铁工业中的酸洗辊。