Zinc plating method
    31.
    发明授权
    Zinc plating method 失效
    镀锌方法

    公开(公告)号:US4030987A

    公开(公告)日:1977-06-21

    申请号:US663695

    申请日:1976-03-04

    IPC分类号: C25D3/22 C25D3/24

    CPC分类号: C25D3/24 C25D3/22

    摘要: An article is zinc plated by electrodeposition in an alkaline zinc plating bath of ZnO and NaOH to which has been added, together with a small quantity of an aromatic aldehyde, a polyamine sulfone represented by the formula ##STR1## WHERE: EACH OF R.sub.1 and R.sub.2 is hydrogen, an allyl group, a straight-chain or branched-chain alkyl group having 1 to 16 carbon atoms, an aralkyl group, or a hydroxyalkyl group of the general formula HO--CH.sub.2).sub.m, where m is an integer of 1 to 6;X.sup.- is a halogen ion, HSO.sub.4.sup.-, HSO.sub.3.sup.-, HCOO.sup.-, or CH.sub.3 COO.sup.-; andn is an integer such that the number average molecular weight becomes 2,000 to 350,000.a and b are natural numbers having a relation such that a:b = 100; (10 to 100).

    摘要翻译: 通过在已经加入的ZnO和NaOH的碱性锌电镀浴中电沉积制品,以及少量的芳族醛,由式[IMAGE> WHERE]表示的聚胺砜:

    Positive electrode active material, method for manufacturing positive electrode active material and nonaqueous electrolyte battery
    33.
    发明授权
    Positive electrode active material, method for manufacturing positive electrode active material and nonaqueous electrolyte battery 失效
    正极活性物质,正极活性物质和非水电解质电池的制造方法

    公开(公告)号:US08771876B2

    公开(公告)日:2014-07-08

    申请号:US12761172

    申请日:2010-04-15

    IPC分类号: H01M4/58 H01M4/00

    摘要: A positive electrode active material includes a lithium complex oxide particle, and a coating layer formed on at least a part of the surface of the lithium complex oxide particle. The lithium complex oxide particle is a lithium complex oxide particle composed mainly of nickel. The coating layer contains an oxo acid and/or an oxo acid compound, an acidity of the surface of the lithium complex oxide particle composed mainly of nickel is increased by the coating layer. The acidity is determined based on a pH of a supernatant of water in a state where after 1.0 part by weight of the lithium complex oxide particle composed mainly of nickel and having a coating layer formed thereon is dispersed in 50 parts by weight of water. The lithium complex oxide particle sediments, and the pH is less than 8.0.

    摘要翻译: 正极活性物质包括锂复合氧化物颗粒和形成在锂复合氧化物颗粒的表面的至少一部分上的涂层。 锂复合氧化物颗粒是主要由镍组成的锂复合氧化物颗粒。 涂层含有含氧酸和/或含氧酸化合物,主要由镍组成的锂复合氧化物颗粒的表面的酸度由涂层增加。 在1.0重量份以镍为主成分并且其上形成有涂层的锂复合氧化物颗粒分散在50重量份水中的状态下,基于水的上清液的pH确定酸度。 锂复合氧化物颗粒沉积,pH值小于8.0。

    Electronic watermark embedding apparatus for selectively embedding electronic watermark information in different frequency components of image data and electronic watermark embedding method
    34.
    发明授权
    Electronic watermark embedding apparatus for selectively embedding electronic watermark information in different frequency components of image data and electronic watermark embedding method 失效
    电子水印嵌入装置,用于将图像数据和电子水印嵌入方法的不同频率分量中的电子水印信息选择性地嵌入

    公开(公告)号:US08238600B2

    公开(公告)日:2012-08-07

    申请号:US12233096

    申请日:2008-09-18

    IPC分类号: G06K9/00

    摘要: An electronic watermark embedding apparatus and an electronic watermark embedding method can severally deal with both of the resistance property of an electronic watermark and the prevention of image quality deterioration. Electronic watermark information of a high importance level is embedded in a component having a strong resistance property, and electronic watermark information of a low importance level is embedded in a component exerting little influence on an image quality. As a result, the electronic watermark information to be embedded in the component having a strong resistance property is limited to that of a high importance level. Moreover, the image quality deterioration can be suppressed in comparison with the case of embedding all pieces of information, and the electronic watermark information of low importance level is embedded in the component having a weak resistance property but exerting little influence on an image quality.

    摘要翻译: 电子水印嵌入装置和电子水印嵌入方法可以分别处理电子水印的电阻特性和防止图像质量劣化。 将具有高重要度的电子水印信息嵌入到具有强电阻特性的分量中,并且将低重要度级别的电子水印信息嵌入到对图像质量几乎没有影响的分量中。 结果,要嵌入具有较强电阻特性的部件中的电子水印信息被限制在高重要程度的电子水印信息。 此外,与嵌入所有信息的情况相比,可以抑制图像质量劣化,并且将低重要度级别的电子水印信息嵌入具有弱电阻性能但对图像质量影响不大的部件中。

    Image processing apparatus and method
    35.
    发明授权
    Image processing apparatus and method 有权
    图像处理装置及方法

    公开(公告)号:US08164793B2

    公开(公告)日:2012-04-24

    申请号:US12511773

    申请日:2009-07-29

    CPC分类号: G06K15/107

    摘要: In a multipass printing that performs a plurality of printing scans over a unit area of a print medium by using a leading head and a follower head, the multivalued image data for the leading head is distributed according to the print volume information for up to the preceding printing scan. Then, the multivalued image data for the leading head is subjected to the grayscale level reduction operation to generate binary data. Based on the binary data, the print volume information is updated, after which the multivalued image data for the follower head is distributed according to the print volume information. This causes a plurality of printing scans or a plurality of print heads, that print the same unit area, to have a correlation among them, with the result that dots on a plurality of planes when overlapped have an excellent scattering characteristic.

    摘要翻译: 在通过使用前导头和跟随头在打印介质的单位区域上执行多次打印扫描的多页打印中,用于前导头的多值图像数据根据打印体积信息被分配到最前面 打印扫描。 然后,对前导头的多值图像数据进行灰度级降低操作,以生成二进制数据。 基于二进制数据,更新打印体积信息,然后根据打印量信息分配随机头的多值图像数据。 这导致打印相同单位区域的多个打印扫描或多个打印头在它们之间具有相关性,结果是当重叠时多个平面上的点具有优异的散射特性。

    Battery
    36.
    发明授权
    Battery 有权
    电池

    公开(公告)号:US07906237B2

    公开(公告)日:2011-03-15

    申请号:US10866214

    申请日:2004-06-10

    IPC分类号: H01M4/58 H01M6/04

    摘要: A battery is provided which has a high capacity and can improve battery characteristics, such as cycle characteristics. The battery includes a spirally wound electrode body, wherein a cathode and an anode are wound with a separator in between. The anode includes, for example, simple substances, alloys, compounds of metal elements or metalloid elements capable of forming an alloy with Li, the like and combinations thereof. An electrolytic solution wherein an electrolyte salt is dissolved in a solvent is impregnated in the separator. For the electrolyte salt, a light metallic salt having B—O bond or P—O bond, such as difluoro[oxalato-O,O′]lithium borate and tetra fluoro[oxalato-O,O′]lithium phosphate, can be used. By forming a stable coating, decomposition reaction of the solvent can be inhibited, and reaction between the anode and the solvent can be prevented.

    摘要翻译: 提供具有高容量并且可以改善诸如循环特性的电池特性的电池。 电池包括螺旋卷绕的电极体,其中阴极和阳极在其间缠绕有隔膜。 阳极包括例如能够与Li形成合金的简单物质,合金,金属元素的化合物或类金属元素及其组合。 将电解质盐溶解在溶剂中的电解液浸渍在隔膜中。 对于电解质盐,可以使用具有B-O键或P-O键的轻金属盐,例如二氟[草酸-O,O']硼酸锂和四氟[草酸-O,O']磷酸锂 。 通过形成稳定的涂层,能够抑制溶剂的分解反应,能够防止阳极与溶剂的反应。

    POSITIVE ELECTRODE ACTIVE MATERIAL, METHOD FOR MANUFACTURING POSITIVE ELECTRODE ACTIVE MATERIAL AND NONAQUEOUS ELECTROLYTE BATTERY
    38.
    发明申请
    POSITIVE ELECTRODE ACTIVE MATERIAL, METHOD FOR MANUFACTURING POSITIVE ELECTRODE ACTIVE MATERIAL AND NONAQUEOUS ELECTROLYTE BATTERY 失效
    正极电极活性材料,制造电极活性材料和非电解电解质电池的方法

    公开(公告)号:US20100273057A1

    公开(公告)日:2010-10-28

    申请号:US12761172

    申请日:2010-04-15

    IPC分类号: H01M4/58 H01M4/00

    摘要: A positive electrode active material includes a lithium complex oxide particle, and a coating layer formed on at least a part of the surface of the lithium complex oxide particle. The lithium complex oxide particle is a lithium complex oxide particle composed mainly of nickel. The coating layer contains an oxo acid and/or an oxo acid compound, an acidity of the surface of the lithium complex oxide particle composed mainly of nickel is increased by the coating layer. The acidity is determined based on a pH of a supernatant of water in a state where after 1.0 part by weight of the lithium complex oxide particle composed mainly of nickel and having a coating layer formed thereon is dispersed in 50 parts by weight of water. The lithium complex oxide particle sediments, and the pH is less than 8.0.