WHITE POLYIMIDE FILM AND MANUFACTURE THEREOF
    32.
    发明申请
    WHITE POLYIMIDE FILM AND MANUFACTURE THEREOF 有权
    白色聚酰亚胺薄膜及其制造方法

    公开(公告)号:US20120095147A1

    公开(公告)日:2012-04-19

    申请号:US12906951

    申请日:2010-10-18

    CPC classification number: C08G73/1039 C08J5/18 C08J2379/08 C08L79/08

    Abstract: A white polyimide film comprises a polyimide base polymer and a coloration filler homogeneously distributed in the white polyimide film by reacting a diamine component with a dianhydride component and a coloration filter. The diamine component can include 2,2′-bis(trifluoromethyl)benzidine, and the dianhydride component can include 3,3′,4,4′-biphenyltetracarboxylic dianhydride and 2,2-bis[4-(3,4-dicarboxyphenoxy)phenyl]propane dianhydride. The coloration filler can include TiO2, Al2O3, CaCO3, CaSO4, SiO2, BN, AlN and clay. The white polyimide film has a coefficient of thermal expansion (CTE) less than about 60 ppm/° C. in a temperature range between about 100° C. and about 200° C. , an elongation rate between about 5% and about 60%, and a b*-value between about 0 and about 15. In some embodiments, a method of manufacturing the white polyimide film is also described.

    Abstract translation: 白色聚酰亚胺膜包括通过使二胺组分与二酸酐组分和着色过滤器反应而均匀分布在白色聚酰亚胺膜中的聚酰亚胺基聚合物和着色填料。 二胺组分可包括2,2'-双(三氟甲基)联苯胺,二酐组分可包括3,3',4,4'-联苯四羧酸二酐和2,2-双[4-(3,4-二羧基苯氧基) 苯基]丙烷二酐。 着色填料可以包括TiO2,Al2O3,CaCO3,CaSO4,SiO2,BN,AlN和粘土。 白色聚酰亚胺膜在约100℃至约200℃的温度范围内具有小于约60ppm /℃的热膨胀系数(CTE),约5%至约60%的伸长率 ,并且ab *值在约0和约15之间。在一些实施例中,还描述了制造白色聚酰亚胺膜的方法。

Patent Agency Ranking