摘要:
Readily processable moulding materials with improved impact strength of polyamides and graft products which have a particular chemical and physical structure.
摘要:
The invention relates to high-impact polyether sulfone molding compositions containing aromatic polyether sulfones, diene graft polymers and, optionally, other thermoplastic resins, at most half the aromatic polyether sulfone being replaceable by other thermoplastic resins.
摘要:
Thermoplastic molding composition comprisingA. 5 to 99% by weight (based on A+B) of a polycarbonate based on substituted dihydroxydiphenyl cycloalkanesB. 1 to 95% by weight (based on A+B) of a graft polymer prepared by a special process of5 to 90 parts by weight of a mixture ofB.1.1. 50 to 95 parts by weight styrene, .alpha.-methyl styrene, C.sub.1-4 alkyl- or halogen-nucleus-substituted styrenes, C.sub.1-8 alkyl methacrylates, C.sub.1-8 alkyl acrylates or mixtures thereof andB.1.2. 5 to 50 parts by weight acrylonitrile, methacrylonitrile, C.sub.1-8 alkyl methacrylates, C.sub.1-8 alkyl acrylates, maleic anhydride, C.sub.1-4 alkyl-N-maleic imides, phenyl-N-maleic imides or mixtures thereof onB.2. 10 to 95 parts by weight of a diene rubber having an average particle diameter d50 of from 0.09 to 1 .mu.m and a gel content of more than 50% by weight and optionally at least one other thermoplastic resin which replaces up to 75% by weight of the polycarbonate A.
摘要:
The invention relates to thermoplastic particulate graft polymers of a rubber (AB), consisting of a core (A) of rubber-like polymer of olefinically unsaturated monomers having softening temperatures (glass temperatures) below 0.degree. C. and a shell (B) of organopolysiloxane, and a polymer (C) of at least one ethylenically unsaturated monomer grafted into the rubber (AB) and to their use, optionally in admixture with brittle thermoplastic vinyl resins, as thermoplastic molding compositions.
摘要:
Graft Polymers of a cross-linked copolymer of compounds of formula (I) or (II) ##STR1## and another vinyl compound as graft basis, and a polymerized vinyl group-containing phosphonic acid derivative as graft.
摘要:
The invention relates to thermoplastic molding compositions showing improved properties, more especially improved dimensional stability and notched impact strength, particularly at low temperatures, in the form of a mixture of at least 35% by weight of a copolyamide containing polydiorganosiloxane carbonamide units and/or of a mixture of partly crystalline polyamides and (co)polyamides containing polydiorganosiloxane carbonamide units and from 1 to 65% by weight of graft products of vinyl polymers on rubbers.The invention also relates to the dimensionally stable molding compositions tough at low temperatures characterized above which additionally contain amorphous siloxane-free polyamides added in quantities of up to 64% by weight.
摘要:
The invention relates to thermoplastic polyamide moulding compositions with improved toughness at low temperatures consisting of at least 60% by weight of polyamide and from 3 to 35% by weight of graft rubbers from the group comprising diene rubbers and acrylate rubbers, which are produced in that a mixture of the two components is produced in the presence of from 0.01 to 5% by weight of a radical forming agent and the moulding compositions are then heated below the polyamide melting point as far as possible in the absence of oxygen.
摘要:
Polymer powders and thermoplastic moulding materials with improved properties are obtained if graft polymers and/or resins in particle form are used and small amounts of rubber-like polymers are polymerized or graft-polymerized onto their particle surfaces.
摘要:
The invention relates to a process for the recovery of thermoplastic polymers from aqueous dispersions by spray-drying after treatment with carboxylic acid of formula I ##STR1## wherein X is a single bond, --CH.sub.2 -- or --C.sub.2 H.sub.4 --, andR is --H, --OH or ##STR2##
摘要翻译:本发明涉及一种通过喷雾干燥从水分散体中回收热塑性聚合物的方法,该方法是用式I的羧酸(I)(其中X是单键,-CH 2 - 或-C 2 H 4 - )和R 是-H,-OH或
摘要:
Molding compounds of(A) 5 to 95% by weight of a graft product of a mixture of 50 to 100 parts by weight styrene, .alpha.-methyl styrene, vinyl toluene, methyl methacrylate or mixtures thereof and 0 to 50 parts by weight acrylonitrile on a particulate silicone rubber with a mean particle diameter (d.sub.50) of from 0.10 to 0.50 .mu.m having a total rubber content of from 30 to 90% by weight and(B) 95 to 5% by weight of a graft product of a mixture of 50 to 100 parts by weight styrene, .alpha.-methyl styrene, vinyl toluene, methyl methacrylate or mixtures thereof and 0 to 50 parts by weight acrylonitrile on a particulate acrylate rubber with a mean particle diameter (d.sub.50) of from 0.05 to 1.00 .mu.m having a total rubber content of 30 to 80% by weight.