摘要:
Compositions suitable for film comprise at least one ethylene/α-olefin interpolymer, wherein the ethylene/α-olefin interpolymer may have, for example, a Mw/Mn from about 1.7 to about 3.5, at least one melting point, Tm, in degrees Celsius, and a density, d, in grams/cubic centimeter, wherein the numerical values of Tm and d correspond to the relationship: Tm>−2002.9+4538.5(d)−2422.2(d)2.
摘要:
The present invention relates to a polymer produced by polymerizing a vinyl aromatic monomer in the presence of a small amount of furfuryl (alkyl)acrylate.
摘要:
Multimodal polyethylene compositions are provided. Extrusion compositions including the multimodal polyethylene are provided. The extrusion composition further include a high pressure low density polyethylene and optionally other additives and/or polyethylenes. Extruded articles made from the polyethylene extrusion compositions are also provided.
摘要:
The invention provides an ethylene-based polymer formed from at least the following: ethylene and a “monomeric chain transfer agent (monomeric CTA),” comprising a “copolymerization end” and a “chain transfer end.”
摘要:
Multimodal polyethylene compositions are provided. Extrusion compositions including the multimodal polyethylene are provided. The extrusion composition further include a high pressure low density polyethylene and optionally other additives and/or polyethylenes. Extruded articles made from the polyethylene extrusion compositions are also provided.
摘要:
The present invention is a method for increasing the melt strength of a polyethylene resin comprising reacting the polyethylene resin with a free radical generator with a decomposition energy in between −50 kJoule/mole and −250 kJoules/mole and a peak decomposition temperature of less than 280 degree C. The resulting resin has increased melt strength with higher ratio of elongational viscosities at 0.1 to 100 rad/s when compared to substantially similar polyethylene resins which have not been reacted with a free radical generator such as an alkoxy amine derivative.
摘要:
The present invention relates to particular ethylene-based polymer compositions suitable for use in binder fiber applications. The materials are characterized in having a peak recrystallization temperature in the range of from 85° C. to 110 C, and a Comonomer Distribution Constant (“CDC”) of 55 or greater. The materials are also characterized by having a tan delta value at 0.1 rad/sec from about 15 to 50, and a complex viscosity at 0.1 rad/second of 1400 Pa·sec or less.
摘要:
Compositions having good impact performance can be made from a thermoplastic (e.g., a polyolefin such as polypropylene or HDPE) and an ethylene multi-block copolymer. The compositions are easily molded and often have particular utility in making, for example, automotive facia, parts and other household articles.
摘要:
Compositions having good impact performance can be made from a thermoplastic (e.g., a polyolefin such as polypropylene or HDPE) and an ethylene multi-block copolymer. The compositions are easily molded and often have particular utility in making, for example, automotive facia, parts and other household articles.
摘要:
The present invention is related to a bimodal rubber characterized in that the bimodal rubber is a composition of linear, and branched rubber molecules, and has a broad, yet monomodal Mw distribution and rubber modified polymers produced therefrom.