摘要:
Methods and compositions are provided that relate to cement compositions comprising sub-micron calcium carbonate and latex. An embodiment includes a cement composition comprising: cement, water, sub-micron calcium carbonate having a particle size in a range of from greater than 100 nanometers to about 1 micron, and latex.
摘要:
Compositions and methods are directed to a cement composition for use in a subterranean formation. In an embodiment the cement composition comprises: (A) cement; (B) water; and (C) a polymer, wherein the polymer: (i) consists essentially of a monomer or monomers selected from the group consisting of acrylic acid, esters of acrylic acid, maleic acid, methacrylic acid, esters of methacrylic acid, itaconic acid, fumeric acid, citraconic acid, mesoconic acid, and any alkali metal, alkaline earth metal, or ammonium salt of any of the foregoing, and any combination of any of the foregoing.
摘要:
A cement composition or method of using the cement composition in a subterranean formation, the composition having: (A) cement; (B) water; and (C) a polymer, wherein the polymer: (i) comprises a monomer or monomers selected from the group consisting of epoxysuccinic acid, a substituted epoxysuccinic acid, and an alkali metal salt, alkaline earth metal salt, or ammonium salt of any of the foregoing, and any combination of any of the foregoing; (ii) has the following characteristics: (a) is water soluble; and (b) is biodegradable; and (iii) is capable of providing: (a) a thickening time of at least 2 hours for a test composition at a temperature of 190° F. and a pressure of 5,160 psi; and (b) an initial setting time of less than 24 hours for the test composition at a temperature of 217° F. and a pressure of 3,000 psi.
摘要:
Compositions and methods according to the invention are directed to a cement composition for use in a subterranean formation. The cement composition comprises: (A) cement; (B) water; and (C) a polymer, wherein the polymer: (i) comprises a monomer or monomers selected from the group consisting of epoxysuccinic acid, a substituted epoxysuccinic acid, and an alkali metal salt, alkaline earth metal salt, or ammonium salt of any of the foregoing, and any combination of any of the foregoing; (ii) has the following characteristics: (a) is water soluble; and (b) is biodegradable; and (iii) is capable of providing: (a) a thickening time of at least 2 hours for a test composition at a temperature of 190° F. and a pressure of 5,160 psi; and (b) an initial setting time of less than 24 hours for the test composition at a temperature of 217° F. and a pressure of 3,000 psi, wherein the test composition consists of 860 grams of Class-H Portland cement, 325 grams of deionized water, and 0.4% by weight of the cement of the polymer. The method comprises the steps of: (A) introducing the cement composition into the subterranean formation; and (B) allowing the cement composition to set after introduction into the subterranean formation.
摘要:
Methods and compositions are provided that may comprise cement, a nano-particle, latex, and water. An embodiment of the present invention includes a method of cementing in a subterranean formation. The method may include introducing a cement composition into the subterranean formation, wherein the cement composition comprises cement, a nano-particle, latex, and water. The method further may include allowing the cement composition to set in the subterranean formation. Another embodiment of the present invention include a cement composition. The cement composition may comprise cement, a nano-particle, latex, and water.
摘要:
Compositions and methods are directed to a cement composition for use in a subterranean formation. In an embodiment the cement composition comprises: (A) cement; (B) water; and (C) a polymer, wherein the polymer: (i) consists essentially of a monomer or monomers selected from the group consisting of acrylic acid, esters of acrylic acid, maleic acid, methacrylic acid, esters of methacrylic acid, itaconic acid, fumeric acid, citraconic acid, mesoconic acid, and any alkali metal, alkaline earth metal, or ammonium salt of any of the foregoing, and any combination of any of the foregoing; (ii) has the following characteristics: (a) is water soluble; and (b) is biodegradable; and (iii) is capable of providing: (a) a thickening time of at least 2 hours for a test composition maintained under a temperature condition of 190° F. and a pressure of 5,160 psi; and (b) an initial setting time of less than 24 hours for the test composition maintained under a temperature condition of 217° F. and a pressure of 3,000 psi, wherein the test composition consists of 860 grams of Class-H Portland cement, 325 grams of deionized water, and 0.4% by weight of the cement of the polymer. In another embodiment the method comprises the steps of: (A) introducing the cement composition into the subterranean formation; and (B) allowing the cement composition to set after introduction into the subterranean formation.
摘要:
Compositions and methods are directed to a cement composition for use in a subterranean formation. In an embodiment the cement composition comprises: (A) cement; (B) water; and (C) a polymer, wherein the polymer: (i) consists essentially of a monomer or monomers selected from the group consisting of acrylic acid, esters of acrylic acid, maleic acid, methacrylic acid, esters of methacrylic acid, itaconic acid, fumeric acid, citraconic acid, mesoconic acid, and any alkali metal, alkaline earth metal, or ammonium salt of any of the foregoing, and any combination of any of the foregoing.
摘要:
A well treatment composition comprises: an aqueous liquid; a fluid loss additive, wherein the fluid loss additive comprises a high molecular weight, water-swellable polymer; and an amphiphilic dispersant, wherein the well treatment composition has an activity of at least 10%. A method of cementing in a subterranean formation comprises: introducing a cement composition into the subterranean formation, the cement composition comprising: (i) cement; (ii) water; and (iii) the well treatment composition; and allowing the cement composition to set.
摘要:
Compositions and methods according to the invention are directed to a cement composition for use in a subterranean formation. The cement composition comprises: (A) cement; (B) water; and (C) a polymer, wherein the polymer: (i) comprises a monomer or monomers selected from the group consisting of epoxysuccinic acid, a substituted epoxysuccinic acid, and an alkali metal salt, alkaline earth metal salt, or ammonium salt of any of the foregoing, and any combination of any of the foregoing; (ii) has the following characteristics: (a) is water soluble; and (b) is biodegradable; and (iii) is capable of providing: (a) a thickening time of at least 2 hours for a test composition at a temperature of 190° F. and a pressure of 5,160 psi; and (b) an initial setting time of less than 24 hours for the test composition at a temperature of 217° F. and a pressure of 3,000 psi, wherein the test composition consists of 860 grams of Class-H Portland cement, 325 grams of deionized water, and 0.4% by weight of the cement of the polymer. The method comprises the steps of: (A) introducing the cement composition into the subterranean formation; and (B) allowing the cement composition to set after introduction into the subterranean formation.
摘要:
Methods and compositions are provided that relate to cement compositions and methods comprising sub-micron calcium carbonate and latex. An embodiment includes a method of cementing in a subterranean formation. The method may comprise introducing a cement composition into the subterranean formation, wherein the cement composition comprises cement, water, sub-micron calcium carbonate, and latex. The method further may comprise allowing the cement composition to set in the subterranean formation. Another embodiment includes a cement composition that may comprise cement, water, a sub-micron calcium carbonate, and latex.