Method of sulfonation of block polymers
    1.
    发明授权
    Method of sulfonation of block polymers 有权
    嵌段聚合物的磺化方法

    公开(公告)号:US08835562B2

    公开(公告)日:2014-09-16

    申请号:US12498778

    申请日:2009-07-07

    IPC分类号: C08F8/36 C08F297/04 C08C19/20

    摘要: Improved methods for preparing sulfonated block polymers with acyl sulfates in non-halogenated aliphatic solvents are provided. The methods include the sulfonation of a precursor block polymer with an acyl sulfate in a reaction mixture further comprising at least one non-halogenated aliphatic solvent to form a sulfonated block polymer, wherein the initial concentration of the precursor block polymer is in the range of from about 0.1 wt % to a concentration that is below the limiting concentration of the precursor block polymer based on the total weight of the reaction mixture. A sulfonation degree of greater than about 1.0 milliequivalent sulfonic acid per gram sulfonated block polymer can be achieved substantially free of polymer precipitation and free of disabling gelation.

    摘要翻译: 提供了在非卤代脂族溶剂中制备具有酰基硫酸盐的磺化嵌段聚合物的改进方法。 所述方法包括在还含有至少一种非卤代脂族溶剂的反应混合物中使用酰基硫酸酯磺化前体嵌段聚合物以形成磺化嵌段聚合物,其中前体嵌段聚合物的初始浓度范围为 约0.1重量%至低于前体嵌段聚合物的极限浓度的浓度,基于反应混合物的总重量。 可以实现大于约1.0毫当量磺酸/克磺化嵌段聚合物的磺化度,基本上不含聚合物沉淀并且没有失效的凝胶化。

    Process for preparing membranes and membrane structures from a sulfonated block copolymer fluid composition
    2.
    发明授权
    Process for preparing membranes and membrane structures from a sulfonated block copolymer fluid composition 有权
    从磺化嵌段共聚物流体组合物制备膜和膜结构的方法

    公开(公告)号:US08377515B2

    公开(公告)日:2013-02-19

    申请号:US13186295

    申请日:2011-07-19

    IPC分类号: C08L53/00

    摘要: The present invention relates to an improved method for making sulfonated block copolymers and to methods for making membranes from such block copolymers. In particular, the present invention relates to an improved method for making sulfonated block copolymers having at least two polymer end blocks that are resistant to sulfonation and at least one polymer interior block that is susceptible to sulfonation where the sulfonation agent is C2 to C8 acyl sulfate. In the improved process the residual carboxylic acid formed from the C2 to C8 acyl sulfate is converted to C1 to C4 alkyl esters by contacting the residual carboxylic acid with at least a 0.9:1 molar ratio of a C1 to C4 alcohol to residual carboxylic acid, resulting in an improved sulfonated block copolymer solution. The present invention further relates to the use of such sulfonated block copolymer solutions to prepare various membranes and other articles.

    摘要翻译: 本发明涉及制备磺化嵌段共聚物的改进方法和由这种嵌段共聚物制备膜的方法。 特别地,本发明涉及制备磺化嵌段共聚物的改进方法,所述磺化嵌段共聚物具有至少两个耐磺化的聚合物端嵌段和至少一个易于磺化的聚合物内部嵌段,其中磺化剂是C2至C8酰基硫酸酯 。 在改进的方法中,由C 2至C 8酰基硫酸形成的残余羧酸通过使残余羧酸与至少0.9:1摩尔比的C1至C4醇与残余羧酸接触而转化为C 1至C 4烷基酯, 得到改进的磺化嵌段共聚物溶液。 本发明还涉及这种磺化嵌段共聚物溶液用于制备各种膜和其它制品的用途。

    Sulfonated block copolymer fluid composition for preparing membranes and membrane structures
    3.
    发明授权
    Sulfonated block copolymer fluid composition for preparing membranes and membrane structures 有权
    用于制备膜和膜结构的磺化嵌段共聚物流体组合物

    公开(公告)号:US08377514B2

    公开(公告)日:2013-02-19

    申请号:US13149589

    申请日:2011-05-31

    IPC分类号: C08L53/00

    摘要: The present invention relates to an improved method for making sulfonated block copolymers and to methods for making membranes from such block copolymers. In particular, the present invention relates to an improved method for making sulfonated block copolymers having at least two polymer end blocks that are resistant to sulfonation and at least one polymer interior block that is susceptible to sulfonation where the sulfonation agent is C2 to C8 acyl sulfate. In the improved process the residual carboxylic acid formed from the C2 to C8 acyl sulfate is converted to C1 to C4 alkyl esters by contacting the residual carboxylic acid with at least a 0.9:1 molar ratio of a C1 to C4 alcohol to residual carboxylic acid, resulting in an improved sulfonated block copolymer solution. The present invention further relates to the use of such sulfonated block copolymer solutions to prepare various membranes and other articles.

    摘要翻译: 本发明涉及制备磺化嵌段共聚物的改进方法和由这种嵌段共聚物制备膜的方法。 特别地,本发明涉及制备磺化嵌段共聚物的改进方法,所述磺化嵌段共聚物具有至少两个耐磺化的聚合物端嵌段和至少一个易于磺化的聚合物内部嵌段,其中磺化剂是C2至C8酰基硫酸酯 。 在改进的方法中,由C 2至C 8酰基硫酸形成的残余羧酸通过使残余羧酸与至少0.9:1摩尔比的C1至C4醇与残余羧酸接触而转化为C 1至C 4烷基酯, 得到改进的磺化嵌段共聚物溶液。 本发明还涉及这种磺化嵌段共聚物溶液用于制备各种膜和其它制品的用途。

    Method of Sulfonation of Block Polymers
    6.
    发明申请
    Method of Sulfonation of Block Polymers 有权
    块状聚合物的磺化方法

    公开(公告)号:US20100048817A1

    公开(公告)日:2010-02-25

    申请号:US12498778

    申请日:2009-07-07

    IPC分类号: C08G81/00

    摘要: Improved methods for preparing sulfonated block polymers with acyl sulfates in non-halogenated aliphatic solvents are provided. The methods include the sulfonation of a precursor block polymer with an acyl sulfate in a reaction mixture further comprising at least one non-halogenated aliphatic solvent to form a sulfonated block polymer, wherein the initial concentration of the precursor block polymer is in the range of from about 0.1 wt % to a concentration that is below the limiting concentration of the precursor block polymer based on the total weight of the reaction mixture. A sulfonation degree of greater than about 1.0 milliequivalent sulfonic acid per gram sulfonated block polymer can be achieved substantially free of polymer precipitation and free of disabling gelation.

    摘要翻译: 提供了在非卤代脂族溶剂中制备具有酰基硫酸盐的磺化嵌段聚合物的改进方法。 所述方法包括在还含有至少一种非卤代脂族溶剂的反应混合物中使用酰基硫酸酯磺化前体嵌段聚合物以形成磺化嵌段聚合物,其中前体嵌段聚合物的初始浓度范围为 约0.1重量%至低于前体嵌段聚合物的极限浓度的浓度,基于反应混合物的总重量。 可以实现大于约1.0毫当量磺酸/克磺化嵌段聚合物的磺化度,基本上不含聚合物沉淀并且没有失效的凝胶化。