Cathodic dissolution of cobaltic hydroxide
    2.
    发明授权
    Cathodic dissolution of cobaltic hydroxide 失效
    氢氧化钴的阴极溶解

    公开(公告)号:US4175014A

    公开(公告)日:1979-11-20

    申请号:US883378

    申请日:1978-03-06

    IPC分类号: C25B1/00 C25C1/08

    CPC分类号: C25B1/00 C22B23/0461

    摘要: A method is provided for the recovery of cobalt from nickel solutions, wherein cobalt is separated from said solution as a precipitate containing cobaltic hydroxide precipitate and also containing nickel, the method comprising dissolving the precipitate for the subsequent recovery of cobalt therefrom by reducing trivalent metal in said precipitate to the divalent state. This is achieved by forming an aqueous slurry of said precipitate acidified with sulfuric acid to a pH ranging from about 0.1 to 2, subjecting the precipitate of said aqueous slurry to electrolytic reduction at the cathode of an electrolytic cell having an insoluble anode, said precipitate being isolated from said anode during said electrolytic reduction and continuing the electrolytic reduction of said precipitate from the trivalent to the divalent state and effect the dissolution thereof.

    摘要翻译: 提供了一种用于从镍溶液中回收钴的方法,其中钴作为含有氢氧化钴沉淀物并且还含有镍的沉淀物从所述溶液中分离,所述方法包括将沉淀物溶解以随后从其中回收钴,通过还原三价金属 所述沉淀为二价态。 这是通过将用硫酸酸化的所述沉淀物的水性浆料形成至约0.1至2的pH,使所述含水浆料的沉淀物在具有不溶性阳极的电解池的阴极处进行电解还原来实现的,所述沉淀物为 在所述电解还原期间与所述阳极分离,并且将所述沉淀物的电解还原为三价至二价状态,并使其溶解。

    Selective extraction of molybdenum and vanadium from spent catalysts by
oxidative leaching with sodium aluminate and caustic
    3.
    发明授权
    Selective extraction of molybdenum and vanadium from spent catalysts by oxidative leaching with sodium aluminate and caustic 失效
    通过氧化浸出铝酸钠和苛性碱从废催化剂中选择性提取钼和钒

    公开(公告)号:US4666685A

    公开(公告)日:1987-05-19

    申请号:US861689

    申请日:1986-05-09

    摘要: Spent hydrodesulfurization catalysts containing alumina, at least one metal from the group consisting of molybdenum, tungsten and vanadium and at least one metal from the group consisting of nickel and cobalt, sulfur, and, usually, residual oil are oxygen pressure leached at a temperature of at least about 400.degree. F. with a base from the group consisting of sodium hydroxide and sodium aluminte in at least stoichimetric amount to yield a solution having a pH between about 7 and 9 containing dissolved molybdenum, vanadium and any tungsten which may be recovered and a readily filterable residue containing aluminum, nickel and cobalt which may be worked up to recover the valuable constituents, with overall processing being accomplished in an environmentally acceptable manner.

    摘要翻译: 含有氧化铝的废加氢脱硫催化剂,由钼,钨和钒组成的组中的至少一种金属和至少一种由镍和钴,硫,以及通常为残油组成的组中的金属,在 至少约400°F,其中碱为氢氧化钠和铝铝,至少为硫酸钡,以产生pH为约7至9的溶液,其中含有溶解的钼,钒和可回收的任何钨, 一种易于过滤的含有铝,镍和钴的残余物,其可被处理以回收有价值的成分,其中整体加工以环境可接受的方式完成。

    Reclaiming of aluminum-chromium waste materials from etching operations
    5.
    发明授权
    Reclaiming of aluminum-chromium waste materials from etching operations 失效
    从蚀刻操作回收铝铬废料

    公开(公告)号:US4954168A

    公开(公告)日:1990-09-04

    申请号:US352301

    申请日:1989-05-15

    摘要: A method is provided for treating sludge containing substantial amounts of chromium, aluminum and iron and residuals of other elements. The method comprises forming a slurry of the sludge in water at a temperature ranging from ambient to 150.degree. F. with the specific gravity of the slurry ranging from about 1.05 to 1.25, and adding a mineral acid to the slurry to provide a pH ranging from about 0.1-3 to dissolve selectively the aluminum and the chromium and leave a solids residue containing gangue material comprising an oxidized iron compound, calcium sulfate, calcium fluoride, calcium silicate among other solids. The pH of the solution is controlled at range of about 2 to 3.5 to precipitate undesirable elements, including iron, without substantially adversely affecting the dissolved chromium and aluminum. The chromium/aluminum-containing solution is separated from the solids therein to provide a substantially purified solution of chromium/-aluminum, and the pH of the solution raised to a range of about 12 to 13.8 to precipitate chromium as chromium hydroxide and provide a pregnant aluminate solution. The chromium hydroxide-containing solution is then subjected to solid/liquid separation to extract chromium hydroxide therefrom and providea pregnant aluminate solution which is thereafter treated to recover alumina therefrom.

    摘要翻译: 提供了一种处理含有大量铬,铝和铁以及其它元素残留物的污泥的方法。 该方法包括在室温至150°F的温度范围内形成污泥的浆液,浆料的比重范围为约1.05至1.25,向矿浆中加入无机酸以提供pH范围从 约0.1-3以选择性地溶解铝和铬,并留下含有氧化铁化合物,硫酸钙,氟化钙,硅酸钙等含固体残留物的含ue石材料。 将溶液的pH控制在约2至3.5的范围内以沉淀包括铁在内的不期望的元素,而不会对溶解的铬和铝基本上有不利影响。 将含铬/铝的溶液与其中的固体分离以提供基本纯化的铬/铝溶液,并且溶液的pH升高至约12至13.8的范围以使铬沉淀为氢氧化铬并提供怀孕 铝酸盐溶液。 然后将含氢氧化铬的溶液进行固/液分离以从其中提取氢氧化铬,并提供一种怀孕的铝酸盐溶液,然后将其处理以从其中回收氧化铝。

    Cyclic process for recovering metal values and alumina from spent
catalysts
    6.
    发明授权
    Cyclic process for recovering metal values and alumina from spent catalysts 失效
    从废催化剂中回收金属值和氧化铝的循环方法

    公开(公告)号:US4670229A

    公开(公告)日:1987-06-02

    申请号:US861690

    申请日:1986-05-09

    摘要: Metal values and alumina are recovered from spent, usually oily, catalysts by oxygen pressure leaching with sodium hydroxide and/or sodium aluminate to dissolve molybdenum, vanadium and/or tungsten and provide a solid, filterable residue containing alumina and cobalt and/or nickel, the residue is digested with sodium hydroxide to give a sodium aluminate solution and a residue enriched in nickel and/or cobalt, alumina is recovered from the sodium aluminate solution as a solid and the remaining supernatant solution is recycled to the oxygen pressure leaching step wherein the alumina content of the aluminate solution is precipitated and a bleed for metals in the aluminate solution is provided.

    摘要翻译: 通过用氢氧化钠和/或铝酸钠进行氧压浸出来从废的,通常是油性的催化剂中回收金属值和氧化铝以溶解钼,钒和/或钨,并提供含有氧化铝和钴和/或镍的固体,可过滤的残余物, 残余物用氢氧化钠消化,得到铝酸钠溶液,富含镍和/或钴的残余物,作为固体从铝酸钠溶液中回收氧化铝,将剩余的上清液再循环至氧气压力浸出步骤,其中 铝酸盐溶液的氧化铝含量被沉淀,并且提供铝酸盐溶液中的金属渗出。

    Removal of hexavalent selenium from nickel, cobalt or copper sulfate
solution
    7.
    发明授权
    Removal of hexavalent selenium from nickel, cobalt or copper sulfate solution 失效
    从镍,钴或硫酸铜溶液中去除六价硒

    公开(公告)号:US4544541A

    公开(公告)日:1985-10-01

    申请号:US620670

    申请日:1984-06-14

    IPC分类号: C01B19/00 C22B15/00

    摘要: A process is provided for removing hexavalent selenium from an acidic sulfate solution containing at least one metal ion from the group consisting of nickel, cobalt and copper at ambient pressure and at a temperature not exceeding the boiling point of the solution. The solution is treated with an agent from the group consisting of a compound which will produce nascent hydrogen in the solution and finely divided metal from the group consisting of nickel, cobalt and copper resulting from in situ precipitation of the metal in the acid sulfate solution. Thus, following treatment with the compound, the hexavalent selenium is reduced to a form separable from the solution by solid-liquid separation.

    摘要翻译: 提供一种用于在环境压力和温度不超过溶液沸点的温度下从含有镍,钴和铜的至少一种金属离子的酸性硫酸盐溶液中除去六价硒的方法。 该溶液用来自在溶液中产生新生氢的化合物的试剂和由金属在酸性硫酸盐溶液中原位沉淀产生的由镍,钴和铜组成的组中的细碎金属处理。 因此,在用化合物处理后,通过固液分离将六价硒还原成与溶液分离的形式。

    Production of nonferrous metals with low selenium contents
    8.
    发明授权
    Production of nonferrous metals with low selenium contents 失效
    硒含量低的有色金属生产

    公开(公告)号:US4214900A

    公开(公告)日:1980-07-29

    申请号:US064689

    申请日:1979-08-08

    摘要: Selenium is precipitated from solutions or slurries containing nonferrous metals, particularly nickel by contacting the solution or slurries with a semimetallic chromous precipitant of the nonferrous metal, particularly nickel, which has a nonferrous metal to chromium ratio between about 10:1 and about 200:1 and which has a metallic content between about 50% and about 90%. The semimetallic chromous precipitant of the nonferrous metal is prepared by hydrogen reducing a solution of the nonferrous metal or slurries containing chromous salts in amount to provide the aforementioned nickel to chromium ratios.

    摘要翻译: 通过使溶液或浆液与有色金属,特别是镍的半金属铬沉淀剂接触,使含有有色金属,特别是镍的溶液或浆料中的硒沉淀,其中有色金属与铬之比约为10:1至200:1 并且其金属含量在约50%至约90%之间。 有色金属的半金属铬沉淀剂通过将含有铬盐的有色金属或浆料的溶液氢还原,以提供上述镍与铬的比例来制备。

    Purification of nickel and cobalt metal powders by a caustic wash
    9.
    发明授权
    Purification of nickel and cobalt metal powders by a caustic wash 失效
    通过苛性碱清洗镍和钴金属粉末

    公开(公告)号:US4149875A

    公开(公告)日:1979-04-17

    申请号:US883379

    申请日:1978-03-06

    摘要: A method is provided for decreasing the silicon content of relatively pure nickel and/or cobalt powder, wherein silicon is present as an impurity substantially in the oxidic state. The method comprises mixing the metal powder in an aqueous solution of an alkali metal hydroxide, e.g. sodium hydroxide, with the temperature of the solution ranging from ambient to below boiling and maintaining the powder in contact with the solution until the silicon content of the powder has been reduced to the desired level.