摘要:
Provided is a method for producing a silver fine powder covered with an organic substance, which comprises a step of mixing (i) a dispersion of silver particles covered with a protective material X1 that comprises an organic compound having an unsaturated bond and having a molecular weight of from 150 to 1000 in a liquid organic medium A, (ii) a protective material X2 that comprises an organic compound of which the number of the carbon atoms constituting the carbon skeleton is smaller than that of the organic compound to constitute the protective material X1, and (iii) a liquid organic medium B of which the ability to dissolve the protective material X1 therein is higher than that of the liquid organic medium A, thereby promoting the dissolution of the protective material X1 in the liquid organic medium B and the adhesion of the protective material X2 to the surface of the silver particles. Accordingly, the invention provides an industrial, large-scale mass-production system for a silver fine powder covered with a protective material having a low molecular weight, of which the sintering temperature can be greatly lowered.
摘要:
Used is a sample holder for MALDI mass spectrometry, which has a CuO secondary particle as a laser-beam-absorbing matrix and in which the secondary particle comprises an aggregate of CuO primary particles having an average particle diameter of 100 nm or smaller and has an uneven surface arising from the shape formed by the primary particles constituting the outermost surface of the secondary particle. As the CuO secondary particle, usable is one derived from a CuO powder produced by baking basic copper carbonate in air at 200 to 300° C., and the basic copper carbonate is produced in a process of mixing an aqueous ammonium hydrogencarbonate solution and an aqueous copper nitrate solution. The CuO secondary particle has an average particle diameter of, for example, from 0.3 to 10 μm.
摘要:
A silver particle dispersion liquid comprising a silver particle powder having an average particle diameter (DTEM) of 50 nm or less, the surface of the particle being covered with an organic protective material, dispersed in a non-polar or small polar liquid organic medium having a boiling point of 60 to 300° C., wherein the organic protective material is an amine compound having one or more unsaturated bonds in one molecule. The silver particle dispersion liquid can be produced by reducing a silver compound in a liquid including one or more alcohol or polyol acting as a reducing agent, wherein the reduction reaction is conducted in the presence of an amine compound having a molecular weight of 100 to 1,000 and having one or more unsaturated bonds in one molecule.
摘要:
Used is a sample holder for MALDI mass spectrometry, which has a CuO secondary particle as a laser-beam-absorbing matrix and in which the secondary particle comprises an aggregate of CuO primary particles having an average particle diameter of 100 nm or smaller and has an uneven surface arising from the shape formed by the primary particles constituting the outermost surface of the secondary particle. As the CuO secondary particle, usable is one derived from a CuO powder produced by baking basic copper carbonate in air at 200 to 300° C., and the basic copper carbonate is produced in a process of mixing an aqueous ammonium hydrogencarbonate solution and an aqueous copper nitrate solution. The CuO secondary particle has an average particle diameter of, for example, from 0.3 to 10 μm.
摘要:
A magnetic material is provided that has an iron oxide phase whose principal phase is a crystal of a structure which has the same space group as ε-Fe2O3 crystal and in which Al is substituted for a portion of the Fe sites of the ε-Fe2O3 crystal. The molar ratio of Al to Fe in the iron oxide phase, when expressed as Al:Fe=x:(2−x), satisfies 0≦x≦1. The value of x is preferably in the range of 0.3 to 0.7. The average particle diameter of the powder determined from a TEM image is preferably 5 to 200 nm, more preferably 10 to 100 nm. The magnetic material has very high practical value because it enables the extremely high coercive force Hc of the ε-Fe2O3 crystal to be regulated to a level enabling utilization in magnetic recording medium and various other applications. The magnetic powder can be produced by a method combining the reverse micelle method and the sol-gel method.
摘要翻译:提供一种磁性材料,其具有氧化铁相,其主相是具有与ε-Fe 2 O 3结晶相同的空间基团的结构的晶体,并且在 该Al取代了ε-Fe 2 O 3结晶的一部分Fe位点。 当以Al:Fe = x:(2-x)表示时,氧化铁相中的Al与Fe的摩尔比满足0
摘要:
Assemblages of particles of a magnetic alloy that are suited to magnetic recording are represented by the formula [TXM1-X] containing T and M in a composition ratio where X in the formula is in the range from 0.3 or greater to 0.7 or less, where T is one or two members of the group consisting of Fe and Co and M is one or two members of the group consisting of Pt and Pd, and metallic elements other than T and M that constitute no more than 30 at. % (including 0 at. %) of (T+M) as a percentage of atoms, and the remainder consists of impurities that are unavoidable from a production standpoint, wherein: the face-centered tetragonal fraction is 10-100%, the average grain size as measured by TEM observation (DTEM) is in the range from 5-30 nm, the x-ray crystal grain size derived by x-ray diffraction (DX) is no less than 4 nm, the particles of are dispersed from each other at a distance, and the dispersion on the composition of the individual particles is kept within a stipulated range.
摘要翻译:适用于磁记录的磁性合金颗粒的组合由含有T和M的式[T XSI M 1-X N]表示,其组成比为X 在式中,在0.3以上且0.7以下的范围内,其中,T是由Fe和Co组成的组中的一个或两个成员,M是由Pt和Pd组成的组中的一个或两个成员,以及金属元素 除T和M外,不超过30个。 (T + M)的%(包括0原子%),其余部分由从生产角度不可避免的杂质组成,其中:面心四方分数为10-100%,平均 通过TEM观察(D TEM)测量的晶粒尺寸在5-30nm的范围内,通过x射线衍射得到的x射线晶粒尺寸(D×X SUB >)不小于4nm,颗粒彼此分开一段距离,单个颗粒的组成分散保持在规定范围内。
摘要:
A magnetic powder composed primarily of Fe that has been surface-treated with a silane coupling agent, which magnetic powder is characterized in that it contains Co such that Co/Fe expressed in atomic percent is 20-50 at. %, Al such that Al/Fe expressed in atomic percent is 5-30 at. %, and one or more rare earth elements R (including Y) such that R/Fe expressed in atomic percent is 4-20 at. %, and has average particle diameter of smaller than 80 nm, TAP density of 0.7 g/cm3 or greater, ignition point of 165 ° C. or higher, and oxygen content of 26 wt % or less.
摘要:
[OBJECT] A composition of a metal nanoparticle is provided in which reproducibility in a method of producing a metal film with excellent low-temperature sinterable properties is improved. An article using the metal nanoparticle composition is also provided.[SOLVING MEANS] A composition of a metal nanoparticle that has a secondary aggregation diameter (median diameter) of 2.0 μm or less as determined by disk centrifugal-type particle size measurement is used.
摘要:
Provided is a method for producing a silver particle powder excellent in the dispersibility in a liquid organic medium having a low polarity, which comprises reducing a silver compound in an alcohol having a boiling point of from 80° C. to 200° C. or in a polyol having a boiling point of from 150 to 300° C., at a temperature of from 80° C. to 200° C. under reflux while maintaining the stream having a Reynolds number of not more than 3.70×104. The stream having a Reynolds number of not more than 3.70×104 can be maintained by stirring with a stirring power of not more than 5.68×108 W. According to the method, a silver particle powder having good low-temperature sinterability and good dispersibility and suitable for use for microwiring formation can be obtained at a high yield.
摘要:
A cleaning agent for a silver-containing composition is provided which can readily remove silver adhered to an object to be cleaned with excellent operability and low environmental loads. This cleaning agent for the silver-containing composition includes an iron nitrate aqueous solution and used to remove silver derived from a composition containing silver nanoparticles having an average diameter of 1 nm to 100 nm adhered to the object to be cleaned.