摘要:
The present invention concerns heterophasic propylene copolymers, comprising a propylene homopolymer (PPH) and an ethylene-propylene rubber (EPR), having a very broad molecular weight distribution, a well-defined total ethylene content and a specific intrinsic viscosities of the ethylene-propylene rubber (EPR). The invention further concerns the process to produce such heterophasic propylene copolymers. The heterophasic propylene copolymers of the present invention are particularly suited for pails, pallets, IBCs and crates. In particular, the heterophasic propylene copolymers of the present invention are characterized by an improved resistance to creep.
摘要:
The present invention concerns heterophasic propylene copolymers, comprising a propylene homopolymer (PPH) and an ethylene-propylene rubber (EPR), having a very broad molecular weight distribution, a well-defined total ethylene content and a specific intrinsic viscosities of the ethylene-propylene rubber (EPR). The invention further concerns the process to produce such heterophasic propylene copolymers. The heterophasic propylene copolymers of the present invention are particularly suited for pails, pallets, IBCs and crates. In particular, the heterophasic propylene copolymers of the present invention are characterized by an improved resistance to creep.
摘要:
This invention discloses bottles and pre-forms prepared by injection-stretch-blow-molding (ISBM) from a composition comprising polypropylene and an inorganic non-sorbitol nucleating agent.
摘要:
Degraded polypropylene (co)polymer modified with a linear dialkylperoxide in order to retain its impact strength and a process for its preparation.
摘要:
This invention relates to the use of a linear dialkyl peroxide having an hexyne or an hexene backbone, for producing a controlled rheology polypropylene heterophasic copolymer of melt index MI2 larger than 15 g/10 min, having simultaneously a very high impact resistance and a high flexural modulus.
摘要:
This invention discloses bottles and pre-forms prepared by injection-stretch-blow-moulding (ISBM) from a composition comprising polypropylene and an inorganic non-sorbitol nucleating agent.
摘要:
Degraded polypropylene (co)polymer modified with a linear dialkylperoxide in order to retain its impact strength and a process for its preparation.