Current collector for SOFC fuel cells
    3.
    发明授权
    Current collector for SOFC fuel cells 有权
    SOFC燃料电池集电器

    公开(公告)号:US06737186B2

    公开(公告)日:2004-05-18

    申请号:US10159860

    申请日:2002-05-31

    IPC分类号: H01M810

    摘要: The ferritic iron alloy is particularly suitable as a material for current collectors used in SOFC solid electrolyte high-temperature fuel cells. The material has a high chromium content upwards of 22% by weight, and a molybdenum content of 1 to 10% by weight. Additionally, there is provided 0.01 to 1.5% by weight of yttrium, rare earth metals, and/or their oxides. The alloy in particular has a high resistance to corrosion under the standard cell atmospheres in the temperature range from 700° to 900° C.

    摘要翻译: 铁素体铁合金特别适用于在SOFC固体电解质高温燃料电池中使用的集电器材料。 该材料的铬含量高达22重量%,钼含量为1〜10重量%。 此外,提供0.01至1.5重量%的钇,稀土金属和/或其氧化物。 在700〜900℃的温度范围内,该合金特别是在标准电池气氛下具有很高的耐腐蚀性。

    Seal compositions, methods, and structures for planar solid oxide fuel cells
    5.
    发明授权
    Seal compositions, methods, and structures for planar solid oxide fuel cells 有权
    平面固体氧化物燃料电池的密封组合物,方法和结构

    公开(公告)号:US08691470B2

    公开(公告)日:2014-04-08

    申请号:US12292078

    申请日:2008-11-12

    IPC分类号: C03C8/00 H01M2/08 H01M2/14

    摘要: A seal composition includes a first alkaline earth metal oxide, a second alkaline earth metal oxide which is different from the first alkaline earth metal oxide, aluminum oxide, and silica in an amount such that molar percent of silica in the composition is at least five molar percent greater than two times a combined molar percent of the first alkaline earth metal oxide and the second alkaline earth metal oxide. The composition is substantially free of boron oxide and phosphorus oxide. The seal composition forms a glass ceramic seal which includes silica containing glass cores located in a crystalline matrix comprising barium aluminosilicate, and calcium aluminosilicate crystals located in the glass cores.

    摘要翻译: 密封组合物包括第一碱土金属氧化物,与第一碱土金属氧化物不同的第二碱土金属氧化物,氧化铝和二氧化硅,其量使得组合物中二氧化硅的摩尔百分比为至少五摩尔 百分比大于第一碱土金属氧化物和第二碱土金属氧化物的组合摩尔百分数的两倍。 该组合物基本上不含氧化硼和氧化磷。 密封组合物形成玻璃陶瓷密封件,其包括位于包括硅铝酸钡的晶体基质中的含二氧化硅的玻璃核心和位于玻璃核心中的硅铝酸钙晶体。

    Crack free SOFC electrolyte
    6.
    发明授权
    Crack free SOFC electrolyte 有权
    无裂纹SOFC电解液

    公开(公告)号:US08663869B2

    公开(公告)日:2014-03-04

    申请号:US12659742

    申请日:2010-03-19

    IPC分类号: H01M8/02 H01M8/10 H01M2/14

    摘要: A solid oxide fuel cell (SOFC) stack includes a plurality of SOFCs, and a plurality of interconnects, each interconnect containing a conductive perovskite layer on an air side of the interconnect. The stack in internally manifolded for fuel and the conductive perovskite layer on each interconnect is not exposed in the fuel inlet riser. The SOFC electrolyte has a smaller roughness in regions adjacent to the fuel inlet and fuel outlet openings in the electrolyte than under the cathode or anode electrodes.

    摘要翻译: 固体氧化物燃料电池(SOFC)堆叠包括多个SOFC和多个互连,每个互连在互连的空气侧包含导电的钙钛矿层。 在内部歧管的用于燃料的叠层和每个互连上的导电钙钛矿层不会暴露在燃料入口立管中。 在阴极或阳极电极下,SOFC电解质在邻近燃料入口和电解液燃料出口的区域具有较小的粗糙度。

    Crack free SOFC electrolyte
    7.
    发明申请
    Crack free SOFC electrolyte 有权
    无裂纹SOFC电解液

    公开(公告)号:US20100239937A1

    公开(公告)日:2010-09-23

    申请号:US12659742

    申请日:2010-03-19

    IPC分类号: H01M8/24 H01M8/00

    摘要: A solid oxide fuel cell (SOFC) stack includes a plurality of SOFCs, and a plurality of interconnects, each interconnect containing a conductive perovskite layer on an air side of the interconnect. The stack in internally manifolded for fuel and the conductive perovskite layer on each interconnect is not exposed in the fuel inlet riser. The SOFC electrolyte has a smaller roughness in regions adjacent to the fuel inlet and fuel outlet openings in the electrolyte than under the cathode or anode electrodes.

    摘要翻译: 固体氧化物燃料电池(SOFC)堆叠包括多个SOFC和多个互连,每个互连在互连的空气侧包含导电的钙钛矿层。 在内部歧管的用于燃料的叠层和每个互连上的导电钙钛矿层不会暴露在燃料入口立管中。 在阴极或阳极电极下,SOFC电解质在邻近燃料入口和电解液燃料出口的区域具有较小的粗糙度。

    Powder-metallurgic method for producing highly dense shaped parts
    9.
    发明授权
    Powder-metallurgic method for producing highly dense shaped parts 有权
    粉末冶金法生产高密度成型零件

    公开(公告)号:US07390456B2

    公开(公告)日:2008-06-24

    申请号:US10238938

    申请日:2002-09-10

    IPC分类号: B22F3/12

    摘要: Highly dense shaped parts are produced with a powder metallurgic process. The parts are formed of an alloy that, besides of at least 20 weight % chromium, consists of iron and one or several additional alloy portions that in sum do not amount to more than 10 weight %. The part is produced by pressing and sintering to near final shape a ready-to-press powder where the additional alloy portions are introduced in form of a master-alloy powder. The master-alloy may contain the following variations: the additional alloy portions and the iron portions; or the additional alloy portions, the iron parts, and the chromium portions; or additional alloy portions and the chromium portions.

    摘要翻译: 用粉末冶金工艺生产高度致密的零件。 这些部件由合金形成,除了至少20重量%的铬以外,由铁和一个或多个另外的合金部分组成,其总和不超过10重量%。 该部件通过将接近最终形状的压制和烧结制成即用型粉末,其中附加的合金部分以母合金粉末的形式引入。 母合金可以包含以下变型:附加合金部分和铁部分; 或附加的合金部分,铁部分和铬部分; 或附加的合金部分和铬部分。

    Seal compositions, methods, and structures for planar solid oxide fuel cells
    10.
    发明申请
    Seal compositions, methods, and structures for planar solid oxide fuel cells 有权
    平面固体氧化物燃料电池的密封组合物,方法和结构

    公开(公告)号:US20100119917A1

    公开(公告)日:2010-05-13

    申请号:US12292078

    申请日:2008-11-12

    IPC分类号: C03C8/00 B28B1/00 H01M2/08

    摘要: A seal composition includes a first alkaline earth metal oxide, a second alkaline earth metal oxide which is different from the first alkaline earth metal oxide, aluminum oxide, and silica in an amount such that molar percent of silica in the composition is at least five molar percent greater than two times a combined molar percent of the first alkaline earth metal oxide and the second alkaline earth metal oxide. The composition is substantially free of boron oxide and phosphorus oxide. The seal composition forms a glass ceramic seal which includes silica containing glass cores located in a crystalline matrix comprising barium aluminosilicate, and calcium aluminosilicate crystals located in the glass cores.

    摘要翻译: 密封组合物包括第一碱土金属氧化物,与第一碱土金属氧化物不同的第二碱土金属氧化物,氧化铝和二氧化硅,其量使得组合物中二氧化硅的摩尔百分比为至少五摩尔 百分比大于第一碱土金属氧化物和第二碱土金属氧化物的组合摩尔百分数的两倍。 该组合物基本上不含氧化硼和氧化磷。 密封组合物形成玻璃陶瓷密封件,其包括位于包括硅铝酸钡的晶体基质中的含二氧化硅的玻璃核心和位于玻璃核心中的硅铝酸钙晶体。