Process for preparing metallic cadmium powder
    2.
    发明授权
    Process for preparing metallic cadmium powder 失效
    制备金属镉粉的工艺

    公开(公告)号:US5505761A

    公开(公告)日:1996-04-09

    申请号:US185849

    申请日:1994-01-25

    IPC分类号: B22F9/12 H01M4/38 H01M4/44

    CPC分类号: H01M4/38 B22F9/12

    摘要: A process for preparing a metallic cadmium powder for use in a nickel-cadmium by heat melting metallic cadmium in an evaporator, introducing an inert gas into the evaporator to discharge cadmium vapor along with the inert gas into a cooler, and collecting the resulting metallic cadmium powder, wherein the process condition is regulated such that at least one of the following conditions (1) and (2) can be satisfied:(1) the amount of the inert gas flow introduced into the evaporator is at least 30 Nl/g of cadmium vapor while the direction of introducing the inert gas into the evaporator is set against the surface of the molten cadmium; and(2) the temperature of the molten cadmium in the evaporator and the amount of the inert gas flow introduced into the evaporator are set such that the following formulae can be satisfied:log y.gtoreq.8.8.times.10.sup.-3 x-5.3 (600.ltoreq.x.ltoreq.900), andlog y.gtoreq.1.8.times.10.sup.-3 x-0.96 (330.ltoreq.x.ltoreq.600),wherein x is the temperature (.degree.C.) of the molten cadmium, and y is the flow rate (cm/sec) of the inert gas over the surface of said molten cadmium.

    摘要翻译: PCT No.PCT / JP92 / 01447 Sec。 371日期:1994年1月25日 102(e)日期1994年1月25日PCT提交1992年11月6日PCT公布。 公开号WO93 / 24262 日本1993年12月9日。一种用于通过在蒸发器中热熔融金属镉制备用于镍镉的金属镉粉末的方法,将惰性气体引入蒸发器以将镉蒸汽与惰性气体一起排放到冷却器 并收集所得到的金属镉粉末,其中调节工艺条件使得可以满足以下条件(1)和(2)中的至少一个:(1)引入蒸发器的惰性气体流量为 至少30Nl / g的镉蒸汽,同时将惰性气体引入蒸发器的方向设置在熔融镉的表面上; 和(2)蒸发器中的熔融镉的温度和引入蒸发器的惰性气体流量的量被设定为使得可满足以下公式:log y> / = 8.8×10-3×5.3(600 < / = x <900),log y> = 1.8×10-3×0.96(330≤x≤600),其中x是熔融镉的温度(℃),y 是所述熔融镉表面上的惰性气体的流量(cm / sec)。