摘要:
There is described (pref. non-adhesive) coating compositions (which may be either water or solvent borne) that comprise an autoxidisable vinyl polymer, the autoxidisable polymer having a vinyl polymer backbone 25% to 75% by wt of the autoxidisable polymer; fatty acid residue 25% to 75% by wt of the autoxidisable polymer; Tg from −60° C. to +20° C., Mw from 3500 to 50000 g/mol; and polydispersity from 2 to 10; the autoxidisable polymer obtained by a process of: (A) polymerising ethylenically unsaturated vinyl monomers comprising: at least one epoxy functional vinyl monomer 15% to 100% by wt total monomers in (A); 0 to 85% of at least one other ethylenically unsaturated vinyl monomer, (preferably other than styrenic monomers) by wt total monomers in (A); (B) reacting the epoxy functional polymer from (A) with fatty acids having an average iodine value from 30 to 250 g I2/100 g fatty acid; where composition has: a) a opt. co-solvent content ≦40% by wt of the composition; b) a solids content either ≧30% (aqueous) ≧60% (solvent based) by wt of the composition, the composition as a coating film having a telegraphing value of less than 10 gloss units (difference between an initial smooth gloss minus an initial rough gloss of the film).
摘要:
A water dilutable UV-curable polyurethane containing alkylene oxide groups, the polyurethane being obtained from components comprising at least: (i) 1 to 25 wt. % of at least one polyisocyanate; (ii) 0 to 80 wt. % of at least one hydroxyl functional compound containing alkylene oxide groups; (iii) 10 to 90 wt. % of at least one hydroxyl functional compound containing at least one polymerisable unsaturated (meth)acryloyl functional group per molecule; and (iv) 0 to 50 wt. % of at least one isocyanate-reactive compound not comprised by (ii) or (iii); wherein the sum of (i) to (iv) is 100%.
摘要:
An aqueous coating composition with an improved open time comprising (a) a crosslinkable water-dispersible oligomer(s); (b) a dispersed polymer(s), (c) a pigment(s) with an oil absorption number ≦25 g oil/100 g pigment and optionally (d) a Newtonian-like thickener(s) and (e) a thixotropic thickener(s) wherein the weight ratio of (a):(b) is in the range of from 10:90 to 60:40; wherein (d)+(e)=0.1 to 10 wt % and wherein said composition when drying to form a coating has a tack-free time of ≦24 hours.
摘要:
An aqueous composition comprising a polyurethane dispersion with a sediment content ≦5%, wherein the polyurethane has an acid value in the range of from 25 to 65 mgKOH/g and comprises (i) 36 to 60 wt % of at least one aromatic polyisocyanate and where the polyurethane is prepared in the presence of (a) ≦5 wt % of 1-methyl-2-pyrrolidinone by weight of the polyurethane and (b) at least one reactive diluent.
摘要:
An aqueous coating composition, which when in the form of a film exhibits an MVTR of ≦500 g/m2/24 h comprising 20 to 80 wt % of a polyurethane A with an acid value of 8 to 40 mg KOH/g and a hard segment content ≧40 wt %, a ring structure content ≧48 wt % and 80 to 20 wt % of a vinyl polymer B with a Tg≧20° C.
摘要:
An aqueous crosslinkable coating composition comprising i) an autoxidizably crosslinkable polymer, ii) a not autoxidizably crosslinkable vinyl polymer bearing carbonyl groups and iii) carbonyl-reactive groups to crosslink the vinyl polymer.
摘要:
A water dilutable UV-curable polyurethane containing alkylene oxide groups, the polyurethane being obtained from components comprising at least: (i) 1 to 25 wt. % of at least one polyisocyanate; (ii) 0 to 80 wt. % of at least one hydroxyl functional compound containing alkylene oxide groups; (iii) 10 to 90 wt. % of at least one hydroxyl functional compound containing at least one polymerizable unsaturated (meth)acryloyl functional group per molecule; and (iv) 0 to 50 wt. % of at least one isocyanate-reactive compound not comprised by (ii) or (iii); wherein the sum of (i) to (iv) is 100%.
摘要:
An aqueous coating composition, which when in the form of a film exhibits an MVTR of ≦500 g/m2/24 h comprising 20 to 80 wt % of a polyurethane A with an acid value of 8 to 40 mg KOH/g and a hard segment content ≧40 wt %, a ring structure content ≧48 wt % and 80 to 20 wt % of a vinyl polymer B with a Tg≧20° C.
摘要:
An aqueous solution coating composition comprising an autoxidisable polyvinyl polymer having ≧20% of fatty acid residue by weight of polymer; Tg from −60 to +15° C.; acid value of 15 to 75 mg KOH/g, Mw from 2500 to 100000 g/mol; polydispersity ≦30, said composition having ≦25% co-solvent by weight of solids, ≧30% solids by weight of composition; said composition when in the form of a coating having a telegraphing value defined as the difference in gloss at a 20° angle of between a film cast on rough PVC and a film cast on smooth PVC of 10 gloss units.
摘要:
An aqueous composition comprising a polyurethane dispersion with a sediment content ≦5%, wherein the polyurethane has an acid value in the range of from 25 to 65 mgKOH/g and comprises (i) 36 to 60 wt % of at least one aromatic polyisocyanate and where the polyurethane is prepared in the presence of (a) ≦5 wt % of 1-methyl-2-pyrrolidinone by weight of the polyurethane and (b) at least one reactive diluent.