Abstract:
Provided for herein is a process to produce an essentially homogeneous single liquid phase hydrocarbon-rubber cement from a polymer slurry comprising a hydrocarbon-rubber, a diluent, and unreacted monomer(s), the process comprising: (a) contacting the polymer slurry with a hydrocarbon solvent; and (b) removing the diluent in amounts not sufficiently more than is necessary to produce the essentially homogeneous single liquid phase hydrocarbon-rubber cement wherein the mass fraction of monomer(s) in the hydrocarbon-rubber cement, based on the total amount of hydrocarbon-rubber present in the hydrocarbon-rubber cement, is less than the mass fraction of monomer(s) in the hydrocarbon-rubber slurry, based on the total amount of hydrocarbon-rubber present in the hydrocarbon-rubber slurry, wherein the diluent comprises a hydrofluorocarbon.
Abstract:
The invention is directed to essentially saturated hydrocarbon polymer composition comprising essentially saturated hydrocarbon polymers having A) a backbone chain, B) a plurality of essentially hydrocarbyl sidechains connected to A), said sidechains each having a number-average molecular weight of from 2500 Daltons to 125,000 Daltons and a MWD by SEC of 1.0-3.5; and having A) a Newtonian limiting viscosity (&eegr;0) at 190° C. at least 50% greater than that of a linear olefinic polymer of the same chemical composition and weight average molecular weight, preferably at least twice as great as that of said linear polymer, B) a ratio of the rubbery plateau modulus at 190° C. to that of a linear polymer of the same chemical composition less than 0.5, preferably
Abstract:
Methods for producing elastomers or elastomeric compositions are provided. One or more C4 to C7 isoolefins and one or more comonomers can be polymerized in the presence of a diluent comprising one or more hydrofluorocarbons to provide a slurry comprising polymer product, unreacted monomer and the diluent. The slurry can be extruded to separate at least a portion of the diluent from the polymer product. The separated diluent can be recycled for polymerizing the one or more C4 to C7 isoolefins.
Abstract:
Provided for herein is a process for separating a hydrocarbon-rubber from a hydrofluorocarbon diluent comprising contacting a polymer slurry comprising the hydrocarbon-rubber dispersed within the hydrofluorocarbon diluent with a hydrocarbon solvent capable of dissolving the hydrocarbon-rubber, to produce a first liquid phase and a second liquid phase, and separating the first liquid phase from the second liquid phase.
Abstract:
Provided for herein is a process to produce an essentially homogeneous single liquid phase hydrocarbon-rubber cement from a polymer slurry comprising a hydrocarbon-rubber, a diluent, and unreacted monomer(s), the process comprising: (a) contacting the polymer slurry with a hydrocarbon solvent; and (b) removing the diluent in amounts not sufficiently more than is necessary to produce the essentially homogeneous single liquid phase hydrocarbon-rubber cement wherein the mass fraction of monomer(s) in the hydrocarbon-rubber cement, based on the total amount of hydrocarbon-rubber present in the hydrocarbon-rubber cement, is less than the mass fraction of monomer(s) in the hydrocarbon-rubber slurry, based on the total amount of hydrocarbon-rubber present in the hydrocarbon-rubber slurry, wherein the diluent comprises a hydrofluorocarbon.
Abstract:
Methods for producing elastomers or elastomeric compositions are provided. One or more C4 to C7 isoolefins and one or more comonomers can be polymerized in the presence of a diluent comprising one or more hydrofluorocarbons to provide a slurry comprising polymer product, unreacted monomer and the diluent. The slurry can be extruded to separate at least a portion of the diluent from the polymer product. The separated diluent can be recycled for polymerizing the one or more C4 to C7 isoolefins.
Abstract:
The invention is directed to essentially saturated hydrocarbon polymer composition comprising essentially saturated hydrocarbon polymers having A) a backbone chain, B) a plurality of essentially hydrocarbyl sidechains connected to A), said sidechains each having a number-average molecular weight of from 2500 Daltons to 125,000 Daltons and a MWD by SEC of 1.0-3.5; and having A) a Newtonian limiting viscosity (&eegr;0) at 190° C. at least 50% greater than that of a linear olefinic polymer of the same chemical composition and weight average molecular weight, preferably at least twice as great as that of said linear polymer, B) a ratio of the rubbery plateau modulus at 190° C. to that of a linear polymer of the same chemical composition less than 0.5, preferably
Abstract:
Provided for herein is a process for separating a hydrocarbon-rubber from a hydrofluorocarbon diluent comprising contacting a polymer slurry comprising the hydrocarbon-rubber dispersed within the hydrofluorocarbon diluent with a hydrocarbon solvent capable of dissolving the hydrocarbon-rubber, to produce a first liquid phase and a second liquid phase, and separating the first liquid phase from the second liquid phase.
Abstract:
The invention is directed to essentially saturated hydrocarbon polymer composition comprising essentially saturated hydrocarbon polymers having A) a backbone chain; B) a plurality of essentially hydrocarbyl sidechains connected to A), said sidechains each having a number-average molecular weight of from 2500 Daltons to 125,000 Daltons and a MWD by SEC of 1.0-3.5; and having A) a Newtonian limiting viscosity (&eegr;0) at 190° C. at least 50% greater than that of a linear olefinic polymer of the same chemical composition and weight average molecular weight, preferably at least twice as great as that of said linear polymer, B) a ratio of the rubbery plateau modulus at 190° C. to that of a linear polymer of the same chemical composition less than 0.5, preferably