摘要:
A method of preparing a composite optical retarder is provided. A first and a second liquid crystal coating materials are respectively disposed on opposite surfaces of a photoalignment film to respectively form a first and a second optical retarders. The composite optical retarder having the photoalignment film sandwiched by the first and the second optical retarders is thus obtained.
摘要:
The present invention pertains to a transparent conductive film including a conductive layer having different thicknesses so as to increase the optical transmittance while maintaining the conductivity of the transparent conductive film. The present invention also pertains to a process for the preparation of the above-mentioned transparent conductive film.
摘要:
The present invention pertains to a transparent conductive film including a conductive layer having different thicknesses so as to increase the optical transmittance while maintaining the conductivity of the transparent conductive film. The present invention also pertains to a process for the preparation of the above-mentioned transparent conductive film.
摘要:
A method for making a retardation film includes: (a) forming a photo-alignment layer on a substrate; (b) exposing the photo-alignment layer such that first and second regions of the alignment surface are oriented in a first alignment direction; (c) disposing a patterned mask over the photo-alignment layer such that the first regions of the alignment surface are shielded; (d) exposing the second regions such that the second regions are oriented in a second alignment direction, and the first regions remain oriented in the first alignment direction; (e) coating liquid crystal molecules over the alignment surface; and (f) curing the liquid crystal molecules.
摘要:
A method for making a polarizer-and-compensator assembly includes: (a) forming an alignment film on a releasable substrate; (b) forming a liquid crystal film on the alignment film so as to form a compensator layer on the releasable substrate; and (c) transferring the compensator layer from the releasable substrate to a polarizer plate by removing the releasable substrate from the compensator layer and attaching the alignment film to the polarizer plate.
摘要:
A method for forming a microstructure includes: (a) forming a photocurable layer on a substrate, the photocurable layer including at least one photocurable compound that has a photocurable functional group equivalent weight ranging from 70 to 700 g/mol; (b) covering partially the photocurable layer using a patterned mask; (c) exposing the photocurable layer through the patterned mask using a first light source so that the photocurable layer is cured at first regions which are exposed; (d) removing the patterned mask; and (e) illuminating the photocurable layer using a second light source to cure second regions of the photocurable layer which have not been cured. The first and second regions have different surface heights and provide a surface roughness for the microstructure.
摘要:
A method for making a retarder includes: (a) forming a photocurable layer on a substrate, the photocurable layer including at least one photocurable prepolymer that has a plurality of reactive functional groups and a functional group equivalent weight ranging from 70 to 700 g/mol; (b) covering partially the photocurable layer using a patterned mask; (c) exposing the photocurable layer through the patterned mask; (d) removing the patterned mask; (e) exposing the photocurable layer to cure second regions of the photocurable layer so as to form a microstructure; (f) forming an alignment layer on the microstructure; (g) forming a liquid crystal layer on the alignment layer; and (h) curing the liquid crystal layer.
摘要:
A method of preparing a composite optical retarder is provided. A first and a second liquid crystal coating materials are respectively disposed on opposite surfaces of a photoalignment film to respectively form a first and a second optical retarders. The composite optical retarder having the photoalignment film sandwiched by the first and the second optical retarders is thus obtained.
摘要:
A method for forming a microstructure includes: (a) forming a photocurable layer on a substrate, the photocurable layer including at least one photocurable compound that has a photocurable functional group equivalent weight ranging from 70 to 700 g/mol; (b) covering partially the photocurable layer using a patterned mask; (c) exposing the photocurable layer through the patterned mask using a first light source so that the photocurable layer is cured at first regions which are exposed; (d) removing the patterned mask; and (e) illuminating the photocurable layer using a second light source to cure second regions of the photocurable layer which have not been cured. The first and second regions have different surface heights and provide a surface roughness for the microstructure.
摘要:
A method for making a retarder includes: (a) forming a photocurable layer on a substrate, the photocurable layer including at least one photocurable prepolymer that has a plurality of reactive functional groups and a functional group equivalent weight ranging from 70 to 700 g/mol; (b) covering partially the photocurable layer using a patterned mask; (c) exposing the photocurable layer through the patterned mask; (d) removing the patterned mask; (e) exposing the photocurable layer to cure second regions of the photocurable layer so as to form a microstructure; (f) forming an alignment layer on the microstructure; (g) forming a liquid crystal layer on the alignment layer; and (h) curing the liquid crystal layer.