A plasma display and a driving device therefor. In a sustain discharge driving circuit that includes a power recovery circuit and a sustain voltage supply circuit, a transformer is used. The transformer includes a primary coil and a secondary coil that are coupled with each other. The primary coil of the transformer is connected in parallel to a panel capacitor serving as a capacitive load so as to increase a change of a voltage that is applied to an inductor, such that a voltage rising period and a voltage falling period are reduced. With the reduction of the turn-on time of a switch, the power consumption of the switch is reduced. Further, as the inductor initially stores current, the occurrence of hard switching is reduced when a sustain discharge voltage is applied and elements of the circuit are protected.
摘要:
Disclosed herein are a multilayer ceramic capacitor, a dielectric composition capable of sintering at a lower temperature and having a small variation in dielectric constant, a multilayer ceramic capacitor using the same, and a method thereof. The dielectric composition includes BaTiO3, MgCO3, Y2O3, Cr2O3, Mn2V2O7, and xBaO-yZrO2-zSiO2 acting as a sintering agent (where 0.1≦x≦0.3, 0.1≦y≦0.3 and 0.4≦z≦0.8, x+y+z=1), wherein when representing the composition with the formula aBaTiO3-bMgCO3-cY2O3-dCr2O3-e(Mn2V2O7)-f(xBaO-yZrO2-zSiO2), the ratio of the components satisfies the conditions of a=100, 0.1≦b≦3.0, 0.3≦c≦2.0, 0.05≦d≦0.2, 0.01≦e≦1.5, 0.5≦f≦3.0 based on the molar ratio. When manufacturing a multilayer ceramic capacitor of a higher capacitance, which is formed to have the thin layer structure of 4 μm or less, short circuits between internal electrodes and the deterioration in capacitance due to massing of the electrodes into ball at the ends may be remarkably reduced.
摘要翻译:本文公开了一种多层陶瓷电容器,能够在较低温度下烧结并且介电常数变化小的电介质组合物,使用其的多层陶瓷电容器及其方法。 电介质组成包括作为烧结剂的BaTiO3,MgCO3,Y2O3,Cr2O3,Mn2V2O7和xBaO-yZrO2-zSiO2(其中0.1≤x≤0.3,0.1≤y≤0.3且0.4≤z≤0.8) ,x + y + z = 1),其中当用式aBaTiO3-bMgCO3-cY2O3-dCr2O3-e(Mn2V2O7)-f(xBaO-yZrO2-zSiO2)代表组合物时,组分的比例满足a = 100,0.1 <= b <= 3.0,0.3 <= c <= 2.0,0.05 <= d <= 0.2,0.01 <= e <= 1.5,0.5 <= f <3.0。 当制造具有4μm或更小的薄层结构的较高电容的多层陶瓷电容器时,内部电极之间的短路以及由于电极在端部组装成球而导致的电容劣化可能显着地 减少
摘要:
A dielectric ceramic composition of high dielectric constant and low dielectric loss, which can be co-fired with Ag electrodes, is provided for use in various parts of electric and electronic appliances. Based on a base composition with a high dielectric constant, the composition comprises glass frit and optionally CuO, as represented by the following formula: a wt. % {x CaO-y1 Sm2O3-y2 Nd2O3-w Li2O-z TiO2}+b wt. % (ZnO—B2O3—SiO2 based or Li2O—B2O3—SiO2 based glass frit)+c wt. % CuO wherein, 13.0 mol %≦x≦20.0 mol %; 10.0 mol %≦y1+y2≦17.0 mol %; 6.0 mol %≦w≦11.0 mol %; 60.0 mol %≦z≦67.0 mol % with the proviso that x+y1+y2+w+z=100; 85.0 wt. %≦a≦97.0 wt. %; 3.0 wt. %≦b≦15.0 wt. %; and c≦7.0 wt. %.
摘要翻译:提供了可与Ag电极共烧的高介电常数和低介电损耗的介电陶瓷组合物,用于电气和电子设备的各种部件。 基于具有高介电常数的基础组合物,组合物包含玻璃料和任选的CuO,如下式所示:其中,13.0mol%<= x <= 20.0mol%; 10.0mol%<= Y1 + y2 <= 17.0mol%; 6.0摩尔%<= w <= 11.0摩尔%; 60.0mol%<= z <= 67.0mol%,条件是x + y1 + y2 + w + z = 100; 85.0重量% %<= a <= 97.0wt。 %; 3.0重量% %<= b <= 15.0wt。 %; 和c <= 7.0 WT。 %
摘要:
A dielectric ceramic composition of high dielectric constant and low dielectric loss, which can be co-fired with Ag electrodes, is provided for use in various parts of electric and electronic appliances. The composition is represented by the following chemical formula: a wt. % {x BaO—y1Nd2O3—y2Sm2O3—w Bi2O3—z TiO2}+ b wt. % (ZnO—B2O3—SiO2—PbO based glass frit)+ c wt. % CuO wherein, 10.0 mol %≦x≦20.0 mol %; 7.0 mol %≦y1+y2≦20.0 mol %; 0.5 mol %≦w≦5.0 mol %; 60.0 mol %≦z≦80.0 mol %, with the proviso that x+y1+y2+w+z=100; 80.0 wt. %≦a≦98.0 wt. %; 1.0 wt. %≦b≦10.0 wt. %; 1.0 wt. %≦c≦10.0 wt. %.
摘要翻译:提供了可与Ag电极共烧的高介电常数和低介电损耗的介电陶瓷组合物,用于电气和电子设备的各种部件。 该组合物由以下化学式表示:其中10.0mol%<= x <= 20.0mol%; 7.0mol%<= Y1 + y2 <= 20.0mol%; 0.5mol%<= w <= 5.0mol%; 60.0mol%<= z <= 80.0mol%,条件是x + y1 + y2 + w + z = 100; 80.0重量% %<= a <= 98.0wt。 %; 1.0重量% %<= b <= 10.0wt。 %; 1.0重量% %<= C&LE; 10.0 WT。 %。
摘要:
A dielectric ceramic composition of high dielectric constant and low dielectric loss, which can be co-fired with Ag electrodes, is provided for use in various parts of electric and electronic appliances. The composition is represented by the following chemical formula: a wt. % {xZrO2−yZnO−wNb2O5−zTiO2}+cwt. % glass frit wherein, 5.0 mol %≦x≦45.0 mol %; 1.5 mol %≦y≦19.0 mol %; 1.5 mol %≦w≦19.0 mol %; 40.0 mol %≦z≦59.0 mol % with the proviso that x+y+w+z=100, 75.0≦a≦97.0, and 3.0≦c≦25.0.
摘要翻译:提供了可与Ag电极共烧的高介电常数和低介电损耗的介电陶瓷组合物,用于电气和电子设备的各种部件。 该组合物由以下化学式表示:其中,5.0mol%<= x <= 45.0mol%; 1.5mol%<= y <= 19.0mol%; 1.5mol%<= w <= 19.0mol%; 40.0mol%<= z <= 59.0mol%,条件是x + y + w + z = 100,75.0 <= a <= 97.0和3.0 <= C&LE; 25.0。
摘要:
The non reducible dielectric ceramic composition comprising a main component of (Ba1-xCax)m(Ti1-yZry)O3, subcomponents of MgO, Re2O3, MO, MnO and V2O5 where Re is one or more elements selected from the group of Y, Dy and Ho and M is one or two elements selected from the group of Ba and Ca, and a sintering aid of SiO2, wherein when the composition is represented by the formula 100(Ba1-xCax)m(Ti1-yZry)O3+bMgO+cRe2O3+dMO+eMnO+fV2O5+gSiO2, the ratio of the components satisfies the conditions of 0.005≦x≦0.15, 0.995≦m≦1.03, 0.0005≦y≦0.005, 0.1≦b≦3.0, 0.1≦c≦3.0, 0.05≦d≦2.0, 0.05≦e≦50.3, 0.0.≦f≦0.1, and 0.2≦g≦3.0 based on the molar ratio.
摘要翻译:不可还原的介电陶瓷组合物包含主要成分为(Ba 1-x Ca 2)m(Ti 1-y) / 3,Y 3 O 3 O 3,MgO,Re 2 O 3 N 3,Mo,MnO和 其中Re是选自Y,Dy和Ho中的一种或多种元素,M是选自Ba和Ca中的一种或两种元素 ,和SiO 2的烧结助剂,其中当组合物由式100表示时(Ba 1-x C x S x N)&lt; SUB (Ti 1-y Z y)O 3 + b M g O + c Re 2 O 3%+ dMO + eMnO + fV 2 O 5 + gSiO 2 2,组分的比例满足条件 为0.005 <= x <=0.15,0.995≤m≤1.03,0.0005≤y≤0.005,0.1≤b≤3.0,0.1≤c≤3.0,0.05≤d≤2.0,0.05 基于摩尔比,<= e <= 50.3,0.0。<= f <= 0.1和0.2 <= g <= 3.0。
摘要:
A low temperature sinterable dielectric ceramic composition and a multilayer ceramic chip capacitor. The dielectric ceramic composition is expressed by the general formula: aBaTiO3-bMgCO3-cY2O3-dCr2O3-eV2O5-f(xZrO2-y(K,Li)2O-zSiO2) (x+y+z=1; 0.05≦x≦0.18, 0.01≦y≦0.08, and 0.7.4≦z≦0.93); in which a, b, c, d, e and f are molar ratios; a=100, 1.0≦b≦2.0, 0.2≦c≦2.0, 0.02≦d≦0.3, 0.02≦e≦0.3, and 0.5≦f
摘要翻译:低温可烧结介电陶瓷组合物和多层陶瓷片式电容器。 介电陶瓷组合物由以下通式表示:aBaTiO3-bMgCO3-cY2O3-dCr2O3-eV2O5-f(xZrO2-y(K,Li)2O-zSiO2)(x + y + z = 1; 0.05 <= x < 0.18,0.01 <= y <= 0.08和0.7.4 <= z <= 0.93); 其中a,b,c,d,e和f是摩尔比; a = 100,1.0 <= b <= 2.0,0.2 <= c <= 2.0,0.02 <= d <= 0.3,0.02 <= e <= 0.3和0.5 <= f <2。 使用介电陶瓷组合物制备多层陶瓷片状电容器。 根据本发明的电介质组合物可以在低温下烧结而不降低介电常数,从而可以制造超薄层电介质。
摘要:
Multilayer ceramic chip capacitors which satisfy X5R (−55 to 85° C., &Dgr;C=±15%) requirements and which are compatible with reducing atmosphere sintering conditions so that base metals such as nickel and nickel alloys may be used for internal electrodes are made in accordance with the invention. The multilayer ceramic chip capacitor comprises alternately staked, dielectric ceramic layers and internal electrode layers wherein dielectric ceramic layers comprise per 100 mol of BaTiO3, BaTiO3; MgCO3: 0.2 to 3.0 mol; at least one selected from Y2O3, Ho2O3, Dy2O3 and Yb2O3: 0.05 to 1.5 mol; Cr2O3: 0.1 to 1.5 mol; BaxCa(1−x)SiO3 (provided that 0≦x≦1): 0.2 to 3.0 mol; and Mn2V2O7: 0.01 to 1.5 mol. The multilayer ceramic chip capacitor of the present invention has a high dielectric constant, satisfies X5R characteristics can be sintered at a low temperature of 1,200 to 1,250° C.
摘要翻译:制成满足X5R(-55〜85℃,ΔC=±15%)要求的多层陶瓷片式电容器,其与还原性气氛烧结条件兼容,使得诸如镍和镍合金的贱金属可用于内部电极 多层陶瓷片状电容器包括交替堆叠的介电陶瓷层和内部电极层,其中介电陶瓷层包含每100mol BaTiO 3,BaTiO 3; MgCO3:0.2〜3.0mol; 选自Y2O3,Ho2O3,Dy2O3和Yb2O3中的至少一种:0.05至1.5mol; Cr 2 O 3:0.1〜1.5摩尔 BaxCa(1-x)SiO 3(条件是0 <= x <= 1):0.2-3.0mol; Mn2V2O7:0.01〜1.5mol。 本发明的多层陶瓷片状电容器具有高介电常数,满足X5R特性,可在1,200〜1250℃的低温烧结。
摘要:
A low temperature sintering microwave dielectric composition which can be sintered at a temperature of below 1250.degree. C. The composition includes a composition of xLiO.sub.1/2 --yCaO--.sub.z SmO.sub.3/2 --wTiO.sub.2 --qBO.sub.3/2 where 13.00.ltoreq.x.ltoreq.16.00, 11.00.ltoreq.y.ltoreq.13.00, 18.00.ltoreq.z.ltoreq.21.00, 45.00.ltoreq.w.ltoreq.51.00 and 0
摘要翻译:可在低于1250℃的温度下烧结的低温烧结微波电介质组合物。该组合物包括xLiO1 / 2-yCaO-zSmO3 / 2-wTiO2-qBO3 / 2的组合物,其中13.00≤x= 16.00,11.00 = y 13.00,18.00 = z = 21.00,45.00 = w = 51.00和0