Carburized and high-frequency hardened part having high strength
    1.
    发明授权
    Carburized and high-frequency hardened part having high strength 有权
    渗碳高频淬火部件具有高强度

    公开(公告)号:US08894778B2

    公开(公告)日:2014-11-25

    申请号:US12078898

    申请日:2008-04-08

    摘要: The present invention relates to a mechanical part, which is obtained by: processing a steel into a shape of a part, the steel having an alloy composition containing, by weight percent, C: 0.10 to 0.30%, Si: 0.50 to 3.00%, Mn: 0.30 to 3.00%, P: 0.030% or less, S: 0.030% or less, Cu: 0.01 to 1.00%, Ni: 0.01 to 3.00%, Cr: 0.20 to 1.00%, Al: 0.20% or less, N: 0.05% or less, and the remainder of Fe and inevitable impurities, and the alloy composition satisfying the following condition: [Si %]+[Ni %]+[Cu %]−[Cr %]>0.50, in which [Si %], [Ni %], [Cu %] and [Cr %] represent the concentration of Si, the concentration of Ni, the concentration of Cu and the concentration of Cr in the alloy composition, respectively; subjecting the steel to a carburizing treatment in a vacuum, followed by gradually cooling the steel; and subsequently subjecting the steel to a high-frequency hardening to thereby harden a surface of the steel.

    摘要翻译: 本发明涉及一种机械部件,其通过以下步骤获得:将钢加工成部件的形状,所述钢具有合金组成,所述合金组合物以重量百分比含有C:0.10至0.30%,Si:0.50至3.00%, Mn:0.30〜3.00%,P:0.030%以下,S:0.030%以下,Cu:0.01〜1.00%,Ni:0.01〜3.00%,Cr:0.20〜1.00%,Al:0.20%以下,N :0.05%以下,余量为Fe和不可避免的杂质,合金组成满足下列条件:[Si%] + [Ni%] + [Cu%] - [Cr%]> 0.50,其中[Si %],[Ni%],[Cu%]和[Cr%]分别表示合金组成中Si的浓度,Ni的浓度,Cu的浓度和Cr的浓度; 在真空中对钢进行渗碳处理,然后逐渐冷却钢; 然后对钢进行高频硬化,使钢的表面硬化。

    Sheave member for belt-type continuously variable transmission and method of manufacturing the same
    2.
    发明授权
    Sheave member for belt-type continuously variable transmission and method of manufacturing the same 有权
    带式无级变速器的滑轮构件及其制造方法

    公开(公告)号:US07988796B2

    公开(公告)日:2011-08-02

    申请号:US11976646

    申请日:2007-10-26

    IPC分类号: C23C8/00 B21K1/42

    摘要: A method of manufacturing a sheave member for a belt-type continuously variable transmission includes a forming step wherein an intermediate product having a sheave surface is formed by forging a steel material; a carburization step wherein the intermediate product is heated in a carburization gas; a gradual cooling step wherein the cooling speed is equal to or less than 20° C./sec, at least until the temperature of the intermediate product has passed through the transformation point; a high-frequency electrical heating step wherein a selected portion(s) of the intermediate product is heated; a water quenching step wherein the selected portion is quenched by contact with water; and a finishing step wherein a grinding process is applied to the intermediate product to attain the final shape. In the cooling step, preferably, the intermediate product is contacted with a cooling gas at a pressure lower than atmospheric pressure.

    摘要翻译: 一种制造带式无级变速器的滑轮构件的方法包括:形成步骤,其中通过锻造钢材形成具有滑轮表面的中间产品; 渗碳步骤,其中所述中间产物在渗碳气中加热; 至少直到中间产品的温度通过相变点为止,其中冷却速度等于或小于20℃/秒的逐渐冷却步骤; 高频电加热步骤,其中加热所述中间产物的选定部分; 水淬步骤,其中所选择的部分通过与水接触来淬火; 以及精加工步骤,其中将研磨工艺施加到中间产品以获得最终形状。 在冷却步骤中,优选地,中间产物在低于大气压的压力下与冷却气体接触。

    Carburized and high-frequency hardened part having high strength
    3.
    发明申请
    Carburized and high-frequency hardened part having high strength 有权
    渗碳高频淬火部件具有高强度

    公开(公告)号:US20080247901A1

    公开(公告)日:2008-10-09

    申请号:US12078898

    申请日:2008-04-08

    IPC分类号: C22C38/42 C23C8/20

    摘要: The present invention relates to a mechanical part, which is obtained by: processing a steel into a shape of a part, the steel having an alloy composition containing, by weight percent, C: 0.10 to 0.30%, Si: 0.50 to 3.00%, Mn: 0.30 to 3.00%, P: 0.030% or less, S: 0.030% or less, Cu: 0.01 to 1.00%, Ni: 0.01 to 3.00%, Cr: 0.20 to 1.00%, Al: 0.20% or less, N: 0.05% or less, and the remainder of Fe and inevitable impurities, and the alloy composition satisfying the following condition: [Si %]+[Ni %]+[Cu %]−[Cr %]>0.50, in which [Si %], [Ni %], [Cu %] and [Cr %] represent the concentration of Si, the concentration of Ni, the concentration of Cu and the concentration of Cr in the alloy composition, respectively; subjecting the steel to a carburizing treatment in a vacuum, followed by gradually cooling the steel; and subsequently subjecting the steel to a high-frequency hardening to thereby harden a surface of the steel.

    摘要翻译: 本发明涉及一种机械部件,其通过以下步骤获得:将钢加工成部件的形状,所述钢具有合金组成,所述合金组合物以重量百分比含有C:0.10至0.30%,Si:0.50至3.00%, Mn:0.30〜3.00%,P:0.030%以下,S:0.030%以下,Cu:0.01〜1.00%,Ni:0.01〜3.00%,Cr:0.20〜1.00%,Al:0.20%以下,N :0.05%以下,余量为Fe和不可避免的杂质,合金组成满足下列条件:&lt;&lt;直线公式描述=“在线公式”end =“lead”?> [Si%] + [Ni%] + [Cu%] - [Cr%]> 0.50,<?在线公式描述=“In-line formula”end =“tail”?>其中[Si%],[Ni% ],[Cu%]和[Cr%]分别表示合金组成中Si的浓度,Ni的浓度,Cu的浓度和Cr的浓度; 在真空中对钢进行渗碳处理,然后逐渐冷却钢; 然后对钢进行高频硬化,使钢的表面硬化。

    Sheave member for belt-type continuously variable transmission and method of manufacturing the same
    4.
    发明申请
    Sheave member for belt-type continuously variable transmission and method of manufacturing the same 有权
    带式无级变速器的滑轮构件及其制造方法

    公开(公告)号:US20080099107A1

    公开(公告)日:2008-05-01

    申请号:US11976646

    申请日:2007-10-26

    摘要: A method of manufacturing a sheave member for a belt-type continuously variable transmission includes a forming step wherein an intermediate product having a sheave surface is formed by forging a steel material; a carburization step wherein the intermediate product is heated in a carburization gas; a gradual cooling step wherein the cooling speed is equal to or less than 20° C./sec, at least until the temperature of the intermediate product has passed through the transformation point; a high-frequency electrical heating step wherein a selected portion(s) of the intermediate product is heated; a water quenching step wherein the selected portion is quenched by contact with water; and a finishing step wherein a grinding process is applied to the intermediate product to attain the final shape. In the cooling step, preferably, the intermediate product is contacted with a cooling gas at a pressure lower than atmospheric pressure.

    摘要翻译: 一种制造带式无级变速器的滑轮构件的方法包括:形成步骤,其中通过锻造钢材形成具有滑轮表面的中间产品; 渗碳步骤,其中所述中间产物在渗碳气中加热; 至少直到中间产品的温度通过相变点为止,其中冷却速度等于或小于20℃/秒的逐渐冷却步骤; 高频电加热步骤,其中加热所述中间产物的选定部分; 水淬步骤,其中所选择的部分通过与水接触来淬火; 以及精加工步骤,其中将研磨工艺施加到中间产品以获得最终形状。 在冷却步骤中,优选地,中间产物在低于大气压的压力下与冷却气体接触。