Production method of machine parts and the machine parts thus produced
    1.
    发明授权
    Production method of machine parts and the machine parts thus produced 失效
    机器零件的生产方法和由此生产的机器零件

    公开(公告)号:US4808486A

    公开(公告)日:1989-02-28

    申请号:US70059

    申请日:1987-07-06

    IPC分类号: B22D19/06 B22D19/16 B32B15/01

    摘要: A machine part such as a cylinder or a feeding screw of an injection molding machine and the like is produced such that a separating metallic plate is inserted in a mold adapted to mold the cylinder or the feeding screw, thereby providing two molding cavities on both sides of the separating plate, and melted metals adapted to form a main portion and a corrosion and wear resistant portion of the cylinder or feeding screw are poured into the two cavities. In this manner the two kinds of metals poured into the two cavities are metallurgically fused together with the separating plate interposed therebetween.

    摘要翻译: 制造诸如注射成型机等的气缸或进料螺杆的机器部件,使得分离金属板插入适于模制圆筒或进料螺杆的模具中,从而在两侧设置两个模腔 并且适于形成主要部分的熔融金属和圆筒或进料螺杆的耐腐蚀和耐磨部分被注入到两个空腔中。 以这种方式,两种注入两个空腔的金属与其间插入的分隔板冶金地熔合在一起。

    Metallic scales and method of manufacturing the same
    2.
    发明授权
    Metallic scales and method of manufacturing the same 失效
    金属鳞片及其制造方法

    公开(公告)号:US4510371A

    公开(公告)日:1985-04-09

    申请号:US359530

    申请日:1982-03-18

    IPC分类号: B23K15/00 B23K26/00

    摘要: A surface of a linear magnetic bar is subjected to such high density energy as a fine beam of laser rays, electrons, ions, plasma or an electric current to change permeability of portions subjected to the high density energy so as to form graduations spaced uniformly. A magnetic sensor is used to detect variation in the permeability, thus measuring movement, speed or acceleration of the scale relative to the magnetic sensor. The scale may be formed on a movable portion of a machine, for example a piston rod of a die casting machine or an injection molding machine.

    摘要翻译: 线性磁棒的表面经受诸如激光,电子,离子,等离子体或电流的精细光束的高密度能量,以改变经受高密度能量的部分的透过率,以形成均匀间隔的刻度。 磁传感器用于检测磁导率的变化,从而测量刻度尺相对磁传感器的运动,速度或加速度。 刻度可以形成在机器的可移动部分上,例如压铸机的活塞杆或注射成型机。

    Method for manufacturing stainless steel die cast products having low
melting point
    3.
    发明授权
    Method for manufacturing stainless steel die cast products having low melting point 失效
    低熔点不锈钢压铸产品的制造方法

    公开(公告)号:US4178983A

    公开(公告)日:1979-12-18

    申请号:US945886

    申请日:1978-09-26

    CPC分类号: B22D17/00 B22D17/08

    摘要: In a method for manufacturing a stainless steel die cast product having low melting point, an alloy consisting of 0.01-0.1% by weight of carbon, 1.0-3.0% by weight of silicon, not more than 12% by weight (but excluding 3-7% by weight) of manganese, 8-25% by weight of nickel, 16-20% by weight of chromium, 1.5-2.5% by weight of copper, 0.2-0.7% by weight of boron, 0.5-2.0% by weight of molybdenum and the balance of iron is die-casted in a metal mold made of a tungsten alloy or a molybdenum alloy and maintained at a temperature of the metal mold of 250.degree.-450.degree. C. under conditions of a casting temperature higher than the liquid phase temperature of the molten alloy by 100.degree.-150.degree. C., an injection pressure of 200-500 kg/cm.sup.2, and an injection plunger speed of 0.2-1.0 m/sec.

    摘要翻译: 在制造具有低熔点的不锈钢压铸产品的方法中,由0.01-0.1重量%的碳,1.0-3.0重量%的硅,不超过12重量%(但不包括3- 7重量%)的锰,8-25重量%的镍,16-20重量%的铬,1.5-2.5重量%的铜,0.2-0.7重量%的硼,0.5-2.0重量% 的钼,其余的铁被压铸在由钨合金或钼合金制成的金属模具中,并且在铸造温度高于该温度的条件下保持在金属模具的温度为250-450℃ 熔融合金的液相温度为100-150℃,注射压力为200-500kg / cm2,注射柱塞速度为0.2-1.0m / sec。

    Method of forming wear-resistant layer
    4.
    发明授权
    Method of forming wear-resistant layer 失效
    耐磨层成型方法

    公开(公告)号:US4750667A

    公开(公告)日:1988-06-14

    申请号:US14351

    申请日:1987-02-13

    CPC分类号: B22F5/00 B22F3/26 B22F7/08

    摘要: A method whereby a base member having a surface on which a wear-resistant layer is formed and a mold member are disposed in opposing relation so as to form a gap between the surface of the base member and the surface of the mold member opposing the surface of the base member. Sintered hard substance grains of a hard substance powder such as material selected from carbides, nitrides and borides of metals belonging to groups IV, V and VI of the periodic table are filled in the afore-mentioned gap along the wear-resistant layer forming surface of the base member. A metal of self-melting alloy is then permeated into a filling-up layer of the sintered hard substance grains. The mold member is thereafter removed and the exposed surface is polished to obtain a fine wear-resistant layer on the base member.