POLYPROPYLENE BASED FILM
    3.
    发明公开

    公开(公告)号:US20230257567A1

    公开(公告)日:2023-08-17

    申请号:US18020680

    申请日:2021-08-25

    申请人: Borealis AG

    IPC分类号: C08L23/14

    CPC分类号: C08L23/14

    摘要: The present invention relates to a film, preferably an unoriented film, comprising a polypropylene composition comprising a random copolymer of propylene monomer units and ethylene comonomer units, wherein the random copolymer has a content of ethylene comonomer units of from 0.5 to 4.0 wt %, based on the total weight amount of monomer units in the random copolymer, the polypropylene composition has a melt flow rate MFR2 of from 0.5 to 20.0 g/10 min, determined according to ISO 1133 at a temperature of 230° C. and a load of 2.16 kg, and the film has a tensile modulus in machine direction TM-MD in the range of from 450 to 850 MPa, when measured according to ISO 527-3 on a 50 μm monolayer cast film, a process for producing such a film and the use of such a polypropylene composition for the production of a film with an improved balance of properties of tensile modulus and protrusion impact.

    MULTILAYER FILM WITH IMPROVED PROPERTIES

    公开(公告)号:US20230001674A1

    公开(公告)日:2023-01-05

    申请号:US17781069

    申请日:2020-12-01

    申请人: BOREALIS AG

    摘要: The present invention relates to a multilayer film comprising at least two outer layers (A) and (C) and at least one core layer (B), at least one of the outer layers (A) and/or (C) comprises component a1), whereas the other outer layer comprises component a1) or a2), whereby component a1) is a terpolymer of propylene, ethylene and one C4 to C10 α-olefin; whereby said terpolymer a1) has an ethylene content in the range of 0.1 to 8.0 wt.-% based on the total weight of the terpolymer a1); a C4 to C10 α-olefin content in the range of 0.1 to 16.0 wt.-% based on the total weight of the terpolymer a1); and a melt flow rate MFR2 measured according to ISO 1133 (230° C., 2.16 kg load) in the range of 0.5 to 12.0 g/10 min; component a2) is a polypropylene having a melting temperature of at least 150° C.; and layer (B) comprises a heterophasic propylene copolymer b), said heterophasic propylene copolymer b) comprises a matrix being a random propylene copolymer b1) and an elastomeric propylene copolymer b2) dispersed in said matrix; whereby the heterophasic propylene copolymer b) has a melt flow rate MFR2 measured according to ISO 1133 (230° C., 2.16 kg load) in the range of 0.3 to 20.0 g/10 min; a xylene cold soluble content (XCS) determined according ISO 16152 (25° C.) in the range of 16.0 to 50.0 wt.-%; and a comonomer content in the range of 11.5 to 21.0 mol-%. In addition, the present invention relates to the use of the multilayer film according to the present invention for soft packaging applications, preferably pouches for food packaging, for medical applications or for pharmaceutical applications.