公开(公告)号:US20220384181A1
公开(公告)日:2022-12-01
申请号:US17681607
申请日:2022-02-25
摘要: A method is disclosed of manufacturing a semiconductor structure comprising an (001) oriented zincblende structure group III-nitride layer, such as GaN. The layer is formed on a 3C-SiC layer on a silicon substrate. A nucleation layer is formed, recrystallized and then the zincblende structure group III-nitride layer is formed by MOVPE at temperature T3 in the range 750-1000 ° C., to a thickness of at least 0.5μ. There is also disclosed a corresponding semiconductor structure comprising a zincblende structure group III-nitride layer which, when characterized by XRD, shows that the substantial majority, or all, of the layer is formed of zincblende structure group III-nitride in preference to wurtzite structure group III-nitride.
-
公开(公告)号:US11817315B2
公开(公告)日:2023-11-14
申请号:US17681607
申请日:2022-02-25
CPC分类号: H01L21/0254 , H01L21/0262 , H01L21/02381 , H01L21/02447 , H01L21/02458 , H01L29/04 , H01L29/2003 , H01L33/007 , H01L33/32
摘要: A method is disclosed of manufacturing a semiconductor structure comprising an (001) oriented zincblende structure group III-nitride layer, such as GaN. The layer is formed on a 3C-SiC layer on a silicon substrate. A nucleation layer is formed, recrystallized and then the zincblende structure group III-nitride layer is formed by MOVPE at temperature T3 in the range 750-1000° C., to a thickness of at least 0.5μ. There is also disclosed a corresponding semiconductor structure comprising a zincblende structure group III-nitride layer which, when characterized by XRD, shows that the substantial majority, or all, of the layer is formed of zincblende structure group III-nitride in preference to wurtzite structure group III-nitride.
-
公开(公告)号:US11302530B2
公开(公告)日:2022-04-12
申请号:US16496388
申请日:2018-03-29
摘要: A method is disclosed of manufacturing a semiconductor structure comprising an (001) oriented zincblende structure group III-nitride layer, such as GaN. The layer is formed on a 3C—SiC layer on a silicon substrate. A nucleation layer is formed, recrystallized and then the zincblende structure group III-nitride layer is formed by MOVPE at temperature T3 in the range 750-1000° C., to a thickness of at least 0.5 μm. There is also disclosed a corresponding semiconductor structure comprising a zincblende structure group III-nitride layer which, when characterized by XRD, shows that the substantial majority, or all, of the layer is formed of zincblende structure group III-nitride in preference to wurtzite structure group III-nitride.
-
-