摘要:
A halogen-free self-extinguishing thermoplastic composition comprising as the flame retardant, one or more phosphorus-containing compounds or elemental phosphorous, a polyphenylene ether, a styrene-acrylonitrile copolymer, a phenol/aldehyde resin, a terpolymer of styrene, acrylonitrile and a hydroxy-containing ester of acrylic or methacrylic acid on which a polyphenylene ether is grafted, and optionally, a diene elastomer having grafted thereon styrene and acrylonitrile monomers.
摘要:
A halogen-free flameproofed thermoplastic molding material consists of a halogen-free thermoplastic resin (A) and one or more further halogen-free components.The thermoplastic resin (A) is present in an amount of from 30 to 90% by weight, based on the molding material. The latter contains, as further components, from 1 to 50% by weight of a phenol/aldehyde resin (B), from 1 to 50% by weight of a nitrogen-containing organic compound (C) and from 3 to 50% by weight of a phosphorus-containing organic compound (D), the percentages in each case being based on the molding material.The molding material is used for the production of flameproofed moldings.
摘要:
A flameproofed thermoplastic molding material consists ofA. a thermoplastic resin containing a vinylaromatic monomerand furthermore containsB. from 0 to 100 parts by weight of an elastomer having a glass transition temperature Tg 0.degree. C., as an impact modifier,C. from 2 to 50 parts by weight of a halogen-containing organic compound (flameproofing agent),D. from 0.5 to 20 parts by weight of a compound containing a metal or non-metal (synergistic agent) andE. from 5 to 50 parts by weight of a novolak (phenol/aldehyde resin).The novolak is obtained from an aldehyde of the formula (I)R.sup.1 --CHO (I)where R.sup.1 is H, C.sub.1 -C.sub.10 -alkyl, cycloalkyl, C.sub.6 -C.sub.12 -aryl or .omega.-aryl-C.sub.1 -C.sub.3 -alkyl, and a mixture of phenols, and this mixture contains two or more monosubstituted phenols and the substituents can be alkyl of 1 to 8 carbon atoms or CN.The molding material is used for the production of flameproofed moldings.
摘要:
Thermoplastic molding materials contain a blend of a polyphenylene ether with a copolymer which consists of monovinyl-aromatic monomers, alkyl methacrylates where alkyl is of not more than 8 carbon atoms and, if required, an elastomer component having a glass transition temperature of .ltoreq.0.degree. C.
摘要:
The invention relates to thermoplastic molding materials based on impact resistant polystyrene and polyphenylene ethers. The molding materials of this invention contain a flexible component having a glass temperature below -70.degree. C. and a flexible component having a glass temperature in the range of 0.degree. to -70.degree. C.
摘要:
High molecular weight polyphenylene ethers are prepared from monohydric phenols by an oxidative coupling reaction with oxygen in the presence of a catalyst complex obtained from a copper salt and an organic amine by a method wherein the metal component of the catalyst is separated off, after the polymerization, by the addition of a polymeric polycarboxylic acid which is essentially composed of unsaturated monofunctional or difunctional carboxylic acids and/or their anhydrides.Advantageously, the polymeric polycarboxylic acids used are homopolymers or copolymers of (a) from 50 to 100% by weight of one or more unsaturated monofunctional acids of 3 to 10 carbon atoms and/or one or more difunctional acids or their anhydrides of 4 to 6 carbon atoms and from 0 to 50% by weight of one or more monomers which do not possess an acid function and can be copolymerized with (a).
摘要:
High molecular weight polyphenylene ethers are prepared from monohydric phenols by an oxidative coupling reaction with oxygen in the presence of a solvent and of a catalyst complex consisting of a copper salt and an organic amine of the general formula ##STR1## where R.sup.1 is C.sub.2 -C.sub.20 -alkylidene, preferably C.sub.2 -C.sub.12 -alkylidene, or alkenylidene, R.sup.2 is H or C.sub.1 -C.sub.12 -alkyl, preferably C.sub.1 -C.sub.4 -alkyl, or C.sub.5 -C.sub.8 -cycloalkyl, each of which is unsubstituted or substituted by functional groups, and n is an integer from 1 to 4, preferably 1 or 2. Preferred functional groups are --OR.sup.3, --NHR.sup.3 or --SR.sup.3, in which R.sup.3 is H C.sub.1 -C.sub.12 -alkyl or C.sub.5 -C.sub.8 -cycloalkyl, and the most suitable amines are 3-tert.-butoxypropylamine, 4-tert.-butoxybutylamine, 3-tert.-butoxy-2-methylpropylamine, 3-tert.-butoxy-2,3-dimethylpropylamine, 3-tert.-butoxy-2-methyloctylamine and N-methyl-N-(4-tert.-butoxybutyl)-amine. The polyphenylene ethers can be processed to moldings by a thermoplastic method.
摘要:
The catalyst is removed in the preparation of high molecular weight polyphenylene ethers from monohydric phenols, which are alkyl-substituted at the two ortho-positions but not at the para-position and may or may not be alkyl-substituted at the meta-position, by an oxidative coupling reaction with oxygen at from 15.degree. to 50.degree. C. in the presence of a catalyst complex obtained from a copper salt and an organic amine, in the presence of from 1 to 20 parts by weight of a solvent per part by weight of the monomeric phenol, and in the presence or absence of an activator, and removal of the metal component of the catalyst from the polyphenylene ether solution with a complex-forming or chelate-forming compound in aqueous solution, in the presence or absence of reducing and stabilizing substances and assistants for accelerating the interphase reactions and for phase separation, by a method in which the continuous removal of the copper catalyst is carried out in one or more mixer-settler stages at a phase volume ratio of the organic phase to the aqueous phase of from 1:0.1 to 1:1.0, preferably from 1:0.4 to 1:0.6.
摘要:
A thermoplastic molding material consists of from 10 to 90 parts by weight of a polycarbonate A and from 90 to 10 parts by weight of a graft copolymer B having a mean particle size of from 200 to 700 nm (d.sub.50 value of the integral mass distribution). The graft polymer B is formed from an elastomer (rubber) (b.sub.1), which accounts for from 10 to 80% by weight, and a grafted shell (b.sub.2), which accounts for from 90 to 20% by weight, the percentages in each case being based on (B).The elastomer (b.sub.1) is composed of from 50 to 99.9% by weight of an alkyl acrylate, where alkyl is of 1 to 8 carbon atoms, and from 0.1 to 5% by weight of a copolymerizable polyfunctional crosslinking monomer.The grafted shell (b.sub.2) is produced in three stages and contains, as graft monomers,(b.sub.2 a.sub.1) from 5 to 40% by weight of a monoethylenically unsaturated aromatic hydrocarbon of not more than 12 carbon atoms, in the first stage,(b.sub.2 a.sub.2) from 15 to 50% by weight of a mixture of a monoethylenically unsaturated aromatic hydrocarbon of not more than 12 carbon atoms and a copolymerizable ethylenically unsaturated monomer, in a weight ratio of from 90:10 to 60:40, in the second stage, and(b.sub.2 a.sub.3) from 10 to 85% by weight of an alkyl (meth)acrylate in the third stage, the percentages in each case being based on (b.sub.2).
摘要:
The use of tricyclodecenyl alcohol in place of other crosslinking agents for crosslinking the soft component of impact-resistant polystyrene based on a polystyrene-grafted poly(alkyl acrylate) improves the flow of mixtures of the said polystyrene with polyphenylene ethers.