Abstract:
Provided is a joining structure capable of simplifying the manufacturing process and having high corrosion resistance. A joining structure has a welded part for connecting joined members made of a metal that forms a passive film. An outermost surface portion of the welded part has a pitting potential. The welded part may include a welded part main body formed inside and a surface-modified layer formed in contact with the welded part main body, and the surface-modified layer may include the outermost surface portion having a pitting potential.
Abstract:
A method of manufacturing a joint body of a ceramic body and a metal body includes a step of joining them together by passing a current to an abutment surface between them. The joining step includes a step of heating up the abutment surface to a temperature T1 within a temperature range between (Tr-220)° C. and (Tr-50)° C. in a period longer than 10 seconds, Tr being a recrystallization temperature of the metal body, a step of heating the abutment surface for a period longer than 5 seconds at a temperature T2 within a temperature range between Tm×0.3° C. and Tm×0.45° C., Tm being a melting point of the metal body, and a step of heating the abutment surface for a period longer than 3 seconds at a heating temperature higher than Tm×0.48° C. and lower than Tm×0.6° C.