Abstract:
A porous ceramic composition having improved thermal stability is comprised of ceramic grains bonded together by grain boundary phase comprised of silica, yttrium and oxygen wherein the amount of alkali metals, alkaline earth metals and other transition metals not including rare earth metals is at most 2% by weight of the grain boundary phase.
Abstract:
A porous ceramic composition having improved thermal stability is comprised of ceramic grains bonded together by a grain boundary phase comprised of silica, rare earth element that is Eu, Gd, Nd or mixture thereof and oxygen and optionally yttrium, wherein the grain boundary phase has a amount of an alkali, an alkaline earth metal and a transition metal other than yttrium that is at most 2% by weight of the grain boundary phase.
Abstract:
A process for manufacturing silver nanowires is provided, wherein the recovered silver nanowires have a high aspect ratio; and, wherein the total glycol concentration is
Abstract:
A process for manufacturing silver nanowires is provided, wherein the recovered silver nanowires have a high aspect ratio; and, wherein the total glycol concentration is
Abstract:
Porous aluminum-containing ceramic bodies are treated to form acicular mullite crystals onto the surfaces of their pores. The crystals are formed by contacting the body with a fluorine-containing gas or a source of both fluorine and silicon atoms to form fluorotopaz at the surface of the pores, and then decomposing the fluorotopaz to form acicular mullite crystals. This process allows the surface area of the ceramic body to be increased significantly while retaining the geometry (size, shape, general pore structure) of the starting body. The higher surface area makes the body more efficient as a particulate filter and also allows for easier introduction of catalytic materials.
Abstract:
An anhydrous mixed powder or mixed granule is provided including 1 to 10 wt % of oxidized maltodextrin; 10 to 60 wt % of an amino acid based builder; 1 to 87.7 wt % of an additional builder selected from the group consisting of carbonate builders, citrate builders, silicate builders, amino acid derived builders and mixtures thereof; a bleach activator; a surfactant; 0.1 to 7 wt % of a phosphonate; enzyme; 0 to 75 wt % of a filler; and
Abstract:
A porous ceramic composition having improved thermal stability is comprised of ceramic grains bonded together by grain boundary phase comprised of silica, yttrium and oxygen wherein the amount of alkali metals, alkaline earth metals and other transition metals not including rare earth metals is at most 2% by weight of the grain boundary phase.