Abstract:
An ethylenic polymer comprising amyl groups from about 0.1 to about 2.0 units per 1000 carbon atoms as determined by Nuclear Magnetic Resonance and both a peak melting temperature, Tm, in ° C., and a heat of fusion, Hf, in J/g, as determined by DSC Crystallinity, where the numerical values of Tm and Hf correspond to the relationship Tm≧(0.2143*Hf)+79.643. An ethylenic polymer comprising at least one preparative TREF fraction that elutes at 95° C. or greater using a Preparative Temperature Rising Elution Fractionation method, where at least one preparative TREF fraction that elutes at 95° C. or greater has a gpcBR value greater than 0.05 and less than 5 as determined by gpcBR Branching Index by 3D-GPC, and where at least 5% of the ethylenic polymer elutes at a temperature of 95° C. or greater based upon the total weight of the ethylenic polymer.
Abstract:
An ethylene-based polymer, which is a low density polyethylene (LDPE), obtained by free radical polymerization of ethylene, and wherein the LDPE has a GPC parameter “LSP” less than 1.60.An ethylene-based polymer that comprises the following features: a) at least 0.1 amyl groups per 1000 total carbon atoms; b) a melt index of 0.01 to 0.3; c) a z-average molecular weight of Mz (conv.) of greater than 350,000 g/mol and less than 425,000 g/mol; d) a gpcBR value from 1.50 to 2.05, and e) a MWD(conv) [Mw(conv)/Mn(conv)] from 6 to 9. An ethylene-based polymer that comprises the following features: a) at least 0.1 amyl groups per 1000 total carbon atoms; b) a melt viscosity ratio (V0.1/V100), at 190° C., greater than, or equal to, 58; c) a melt viscosity at 0.1 rad/s, 190° C., greater than, or equal to, 40,000 Pa·s, and d) a gpcBR value from 1.50 to 2.25.
Abstract:
An ethylenic polymer comprising amyl groups from about 0.1 to about 2.0 units per 1000 carbon atoms as determined by Nuclear Magnetic Resonance and both a peak melting temperature, Tm, in ° C., and a heat of fusion, Hf, in J/g, as determined by DSC Crystallinity, where the numerical values of Tm and Hf correspond to the relationship Tm≧(0.2143*Hf)+79.643. An ethylenic polymer comprising at least one preparative TREF fraction that elutes at 95° C. or greater using a Preparative Temperature Rising Elution Fractionation method, where at least one preparative TREF fraction that elutes at 95° C. or greater has a gpcBR value greater than 0.05 and less than 5 as determined by gpcBR Branching Index by 3D-GPC, and where at least 5% of the ethylenic polymer elutes at a temperature of 95° C. or greater based upon the total weight of the ethylenic polymer.
Abstract:
An ethylene-based polymer, which is a low density polyethylene (LDPE), obtained by free radical polymerization of ethylene, and wherein the LDPE has a GPC parameter “LSP” less than 1.60.An ethylene-based polymer that comprises the following features: a) at least 0.1 amyl groups per 1000 total carbon atoms; b) a melt index of 0.01 to 0.3; c) a z-average molecular weight of Mz (conv.) of greater than 350,000 g/mol and less than 425,000 g/mol; d) a gpcBR value from 1.50 to 2.05, and e) a MWD(conv) [Mw(conv)/Mn(conv)] from 6 to 9. An ethylene-based polymer that comprises the following features: a) at least 0.1 amyl groups per 1000 total carbon atoms; b) a melt viscosity ratio (V0.1/V100), at 190° C., greater than, or equal to, 58; c) a melt viscosity at 0.1 rad/s, 190° C., greater than, or equal to, 40,000 Pa·s, and d) a gpcBR value from 1.50 to 2.25.
Abstract:
An ethylenic polymer comprising amyl groups from about 0.1 to about 2.0 units per 1000 carbon atoms as determined by Nuclear Magnetic Resonance and both a peak melting temperature, Tm, in ° C., and a heat of fusion, Hf, in J/g, as determined by DSC Crystallinity, where the numerical values of Tm and Hf correspond to the relationship Tm≧(0.2143*Hf)+79.643. An ethylenic polymer comprising at least one preparative TREF fraction that elutes at 95° C. or greater using a Preparative Temperature Rising Elution Fractionation method, where at least one preparative TREF fraction that elutes at 95° C. or greater has a gpcBR value greater than 0.05 and less than 5 as determined by gpcBR Branching Index by 3D-GPC, and where at least 5% of the ethylenic polymer elutes at a temperature of 95° C. or greater based upon the total weight of the ethylenic polymer.
Abstract:
Disclosed is an ethylene-based polymer with a density from about 0.90 to about 0.94 in grams per cubic centimeter, with a molecular weight distribution (Mw/Mn) from about 2 to about 30, a melt index (I2) from about 0.1 to about 50 grams per 10 minutes, and further comprising sulfur from about 5 to about 4000 parts per million. The amount of sulfur is also determined based upon the total weight of the ethylene-based polymer. Also disclosed is process for making an ethylene-based polymer which includes the steps of splitting a process fluid for delivery into a tubular reactor; feeding an upstream process feed stream into a first reaction zone and at least one downstream process feed stream into at least one other reaction zone, where the process fluid has an average velocity of at least 10 meters per second; and initiating a free-radical polymerization reaction.
Abstract:
An ethylenic polymer comprising amyl groups from about 0.1 to about 2.0 units per 1000 carbon atoms as determined by Nuclear Magnetic Resonance and both a peak melting temperature, Tm, in ° C., and a heat of fusion, Hf, in J/g, as determined by DSC Crystallinity, where the numerical values of Tm and Hf correspond to the relationship Tm≧(0.2143*Hf)+79.643. An ethylenic polymer comprising at least one preparative TREF fraction that elutes at 95° C. or greater using a Preparative Temperature Rising Elution Fractionation method, where at least one preparative TREF fraction that elutes at 95° C. or greater has a gpcBR value greater than 0.05 and less than 5 as determined by gpcBR Branching Index by 3D-GPC, and where at least 5% of the ethylenic polymer elutes at a temperature of 95° C. or greater based upon the total weight of the ethylenic polymer.
Abstract:
An ethylene-based polymer, which is a low density polyethylene (LDPE), obtained by free radical polymerization of ethylene, and wherein the LDPE has a GPC parameter “LSP” less than 1.60.An ethylene-based polymer that comprises the following features: a) at least 0.1 amyl groups per 1000 total carbon atoms; b) a melt index of 0.01 to 0.3; c) a z-average molecular weight of Mz (conv.) of greater than 350,000 g/mol and less than 425,000 g/mol; d) a gpcBR value from 1.50 to 2.05, and e) a MWD(conv) [Mw(conv)/Mn(conv)] from 6 to 9. An ethylene-based polymer that comprises the following features: a) at least 0.1 amyl groups per 1000 total carbon atoms; b) a melt viscosity ratio (V0.1/V100), at 190° C., greater than, or equal to, 58; c) a melt viscosity at 0.1 rad/s, 190° C., greater than, or equal to, 40,000 Pa·s, and d) a gpcBR value from 1.50 to 2.25.
Abstract:
The invention provides a composition comprising a low density polyethylene (LDPE) obtained by free radical polymerization of ethylene, and wherein the LDPE has a GPC-Viscometer parameter “DPP” less than 1.3. The invention also provides a composition comprising an ethylene-based polymer that comprises the following features: a) at least 0.1 amyl groups per 1000 total carbon atoms; b) a melt index from 0.5 to 0.9 c) a MWD(conv) [(Mw(conv)/Mn(conv))] from 9 to 13. The invention also provides a composition comprising an ethylene-based polymer that comprises the following features: a) at least 0.1 amyl groups per 1000 total carbon atoms; b) a MWD(conv) from 9 to 13; c) a gpcBR value from 2.0 to 5.0; and d) a melt strength (MS) greater than 20 cN.
Abstract:
Disclosed is an ethylene-based polymer with a density from about 0.90 to about 0.94 in grams per cubic centimeter, with a molecular weight distribution (Mw/Mn) from about 2 to about 30, a melt index (I2) from about 0.1 to about 50 grams per 10 minutes, and further comprising sulfur from about 5 to about 4000 parts per million. The amount of sulfur is also determined based upon the total weight of the ethylene-based polymer. Also disclosed is process for making an ethylene-based polymer which includes the steps of splitting a process fluid for delivery into a tubular reactor; feeding an upstream process feed stream into a first reaction zone and at least one downstream process feed stream into at least one other reaction zone, where the process fluid has an average velocity of at least 10 meters per second; and initiating a free-radical polymerization reaction.