CELLULOSE ACYLATE FILM AND METHOD FOR PRODUCING THE SAME
    1.
    发明申请
    CELLULOSE ACYLATE FILM AND METHOD FOR PRODUCING THE SAME 审中-公开
    纤维素乙酸酯薄膜及其制造方法

    公开(公告)号:US20150015833A1

    公开(公告)日:2015-01-15

    申请号:US14499880

    申请日:2014-09-29

    Abstract: A cellulose acylate film that contains at least one kind of cellulose acylate that has a substitution degree of an acyl group that contains an aromatic group of from 0.1 to 2.0, or a substitution degree of an acyl group having from 2 to 4 carbon atoms of from 2.0 to 2.6, and has an in-plane retardation at a wavelength of 550 nm Re(550) of from 80 to 350 nm, and the number of bright spots caused from irregular retardation regions having a major axis diameter of from 0.01 to 0.05 mm of 500 or less per 1 cm2 causes less light leakage irrespective of Re of 80 nm or more, so as to enhance the display capability of IPS type and FFS type liquid crystal display devices.

    Abstract translation: 一种纤维素酰化物膜,其含有至少一种酰化物的酰化物的取代度为含有0.1〜2.0的芳香族基团的酰基或具有2〜4个碳原子的酰基的取代度, 2.0〜2.6,并且在550nm的Re(550)为550〜350nm的波长的面内相位差,以及由长轴径为0.01〜0.05mm的不规则延迟区域引起的亮点数 500或更小的每1cm 2会导致较少的漏光,而不考虑80nm以上的Re,从而提高IPS型和FFS型液晶显示装置的显示能力。

    LOUVER FILM, PLANAR LIGHT SOURCE DEVICE, AND LIQUID CRYSTAL DISPLAY DEVICE

    公开(公告)号:US20200292878A1

    公开(公告)日:2020-09-17

    申请号:US16885749

    申请日:2020-05-28

    Abstract: A louver film, a planar light source device, and a liquid crystal display device enables further improvement of directivity for visibility while light use efficiency is maintained and also enable improvement of viewing angle contrast and halo. The louver film includes a plurality of lenses which are arranged at a constant pitch on an emission side of a light source; a first support disposed on a side closer to the light source than the lenses and has a thickness greater than or equal to the pitch of the lenses and a refractive index of 1.5 or greater; and a light reflecting layer disposed on a side closer to the light source than the first support and has a reflectivity of 90% or greater and openings on optical axes of the plurality of lenses, and the opening ratio of each opening is in a range of 30% to 70%.

    OPTICAL FILM, MULTILAYER FILM, AND MANUFACTURING METHOD THEREOF
    7.
    发明申请
    OPTICAL FILM, MULTILAYER FILM, AND MANUFACTURING METHOD THEREOF 审中-公开
    光膜,多层膜及其制造方法

    公开(公告)号:US20130163082A1

    公开(公告)日:2013-06-27

    申请号:US13707072

    申请日:2012-12-06

    CPC classification number: G02B5/305 G02B5/3016 G02B5/3083 G02F1/133528

    Abstract: An optical film that does not cause display unevenness, includes a retardation layer A (A layer) satisfying the following relational expression, nz>nx≧ny here, nx represents an in-plane refractive index in a direction of an in-plane slow axis, ny represents an in-plane refractive index in a direction orthogonal to the direction of an in-plane slow axis, and nz represents a refractive index in a thickness direction; and a retardation layer B (B layer) of which in-plane retardation Re and thickness direction retardation Rth satisfy the following relational expressions: 0 nm≦Re≦20 nm and 50 nm≦Rth≦300 nm, wherein the total film thickness is 5 μm to 40 μm.

    Abstract translation: 不产生显示不均匀的光学膜包括满足以下关系式的延迟层A(A层),nz> nx> = ny,nx表示平面内缓慢方向的面内折射率 ny表示在与面内慢轴方向正交的方向上的面内折射率,nz表示厚度方向的折射率; 以及面内延迟量Re和厚度方向延迟Rth满足以下关系式的延迟层B(B层):0nm @ Re @ 20nm和50nm @ Rth @ 300nm,其中总膜厚度为5 妈妈到40个妈妈

    OPTICAL FILM, MULTILAYER FILM, AND MANUFACTURING METHOD THEREOF
    10.
    发明申请
    OPTICAL FILM, MULTILAYER FILM, AND MANUFACTURING METHOD THEREOF 审中-公开
    光膜,多层膜及其制造方法

    公开(公告)号:US20160025911A1

    公开(公告)日:2016-01-28

    申请号:US14878741

    申请日:2015-10-08

    CPC classification number: G02B5/305 G02B5/3016 G02B5/3083 G02F1/133528

    Abstract: A manufacturing method of a multilayer film having: an optical film including: a retardation layer A satisfying the relational expression, nz>nx≧ny, here, nx represents an in-plane refractive index in a direction of an in-plane slow axis, ny represents an in-plane refractive index in a direction orthogonal to the direction of an in-plane slow axis, and nz represents a refractive index in a thickness direction; a retardation layer B of which in-plane retardation Re and thickness direction retardation Rth satisfy the relational expressions, 0 nm≦Re≦20 nm, 50 nm≦Rth≦300 nm, wherein the total film thickness is 5 μm to 40 μm; and a laminate layer C on the surface of the A layer, the manufacturing method including: manufacturing a multilayer structure including the A layer and the C layer by a solution co-casting method; and forming the B layer on the surface of the A layer of the multilayer structure by coating.

    Abstract translation: 一种多层膜的制造方法,具有:光学膜,包括:满足关系式的延迟层A,nz>nx≥ny,这里,nx表示面内慢轴方向的面内折射率, ny表示与正面内的慢轴的方向正交的方向的面内折射率,nz表示厚度方向的折射率。 面内相位差Re和厚度方向延迟Rth满足关系式的延迟层B为0nm< nlE; Re≦̸ 20nm,50nm≦̸ Rth≦̸ 300nm,其中,总膜厚为5μm〜40μm; 和A层表面上的层压层C,其制造方法包括:通过溶液共铸法制造包括A层和C层的多层结构; 并通过涂布在多层结构的A层的表面上形成B层。