Titanium dioxide finishing process
    2.
    发明授权
    Titanium dioxide finishing process 有权
    二氧化钛整理工艺

    公开(公告)号:US07247200B2

    公开(公告)日:2007-07-24

    申请号:US11263702

    申请日:2005-11-01

    IPC分类号: C09C1/36 C09C3/04 C01G23/047

    摘要: This disclosure relates to process for producing titanium dioxide (TiO2) pigments, comprising the following steps: a) oxidizing a mixture of titanium tetrahalide and a rutile forming agent, such as aluminum halide, present in the vapor phase and in the presence of a nucleant to form a gaseous suspension comprising titanium dioxide particles; b) passing the gaseous suspension to a cooling conduit; c) introducing scouring material into the cooling conduit; wherein the particles of the scouring material have a diameter in the range of about 0.25 mm to about 12.7 mm; d) separating the vapor phase to form a powder comprising the titanium dioxide particles and the scouring material; and e) simultaneously subjecting the powder to substantially uniform heating at a temperature of about 300° C. to about 600° C. and reducing the size of the titanium dioxide particles and the particles of the scouring material in the powder to a mean particle size of about 50 nm to about 1000 nm, whereby the titanium dioxide pigment has a chloride content of less than about 500 ppm. The so treated powder may have a residual free chlorine content of less than about 1 ppm.

    摘要翻译: 本公开涉及生产二氧化钛(TiO 2)颜料的方法,包括以下步骤:a)氧化四卤化钛和存在于蒸气中的金红石形成剂如卤化铝的混合物 并在成核剂存在下形成包含二氧化钛颗粒的气态悬浮液; b)将气态悬浮液通过冷却管道; c)将精练材料引入冷却管道; 其中所述精练材料的颗粒的直径在约0.25mm至约12.7mm的范围内; d)分离气相以形成包含二氧化钛颗粒和洗涤材料的粉末; 和e)在约300℃至约600℃的温度下同时对粉末进行基本上均匀的加热,并将粉末中二氧化钛颗粒和擦洗材料的颗粒的尺寸减小到平均粒度 为约50nm至约1000nm,由此二氧化钛颜料的氯化物含量小于约500ppm。 如此处理的粉末可具有小于约1ppm的残余游离氯含量。

    Injector mixer apparatus
    4.
    发明授权
    Injector mixer apparatus 失效
    注射器混合装置

    公开(公告)号:US4430001A

    公开(公告)日:1984-02-07

    申请号:US306593

    申请日:1981-09-28

    申请人: George A. Schurr

    发明人: George A. Schurr

    IPC分类号: B01F5/04 B01F5/20 B01F13/02

    摘要: An apparatus and process for uniformly mixing a relatively small amount of material with a relatively large amount of another material in particulate form by introducing the smaller amount of material via a pipe within another concentric pipe through which a high pressure gas is introduced which thereby provides a zone of turbulence into which a particulate material in larger amounts is introduced, the mixture of gas and materials being transported through a treatment chamber to produce a uniform mixture.

    摘要翻译: 通过经由另一同心管中的管引入较少量的材料,将相对少量的材料与相对大量的另一种材料均匀混合的装置和方法,通过该管道引入高压气体,从而提供 引入更大量的颗粒材料的湍流区域,气体和材料的混合物通过处理室输送以产生均匀的混合物。