Process for production of steel strip
    2.
    发明授权
    Process for production of steel strip 失效
    钢带生产工艺

    公开(公告)号:US5339887A

    公开(公告)日:1994-08-23

    申请号:US947708

    申请日:1992-09-18

    摘要: A continuously cast steel strip which consists of a solidified casting shell and a liquid core is reduced in thickness in a roll deformation and is then rolled. In order to avoid undesired fluctuations in thickness, to improve the structure and to simplify the roll deformation unit, a steel strip billet of 40-80 mm thickness is cast, roll deformed to 15-40 mm thickness having a 2-15 mm residual liquid core in a maximum of three steps. The roll deformed billet is then guided to complete solidification.

    摘要翻译: 由固化的铸造壳体和液芯组成的连续铸钢带的厚度在轧制变形中减小,然后轧制。 为了避免厚度的不希望的波动,为了改善结构和简化辊变形单元,铸造厚度为40-80mm的钢带坯,轧制变形到15-40mm厚度,具有2-15mm的残留液体 核心最多三步。 然后引导轧辊变形钢坯完全凝固。

    Continuous casting plant for casting thin slabs
    3.
    发明授权
    Continuous casting plant for casting thin slabs 失效
    铸造薄板坯连铸机

    公开(公告)号:US5613548A

    公开(公告)日:1997-03-25

    申请号:US517881

    申请日:1995-08-22

    CPC分类号: B22D11/115

    摘要: A continuous casting plant for casting thin slabs includes an electromagnetic decelerating unit for the molten steel which flows into the mold through a submerged casting pipe. The electromagnetic decelerating unit is composed of a coil with a ferromagnetic core arranged on each of the long sides of the mold and a yoke surrounding the mold. The cores on the long sides of the mold each are composed of a principal core and a partial core on the side of the cast strand, wherein different partial cores can be used as desired for adapting the magnetic field to changing casting conditions.

    摘要翻译: 用于铸造薄板坯的连续铸造设备包括用于通过浸没铸造管流入模具的钢水的电磁减速单元。 电磁减速单元由布置在模具的每个长边上的具有铁磁芯的线圈和围绕模具的轭构成。 模具长边上的芯体由铸芯侧面的主芯和部分芯组成,其中根据需要可以使用不同的部分芯以使磁场适应变化的铸造条件。

    Method for sequence casting of steel strip
    4.
    发明授权
    Method for sequence casting of steel strip 失效
    钢带顺序铸造方法

    公开(公告)号:US4969506A

    公开(公告)日:1990-11-13

    申请号:US297846

    申请日:1989-01-17

    CPC分类号: B22D11/086

    摘要: A method for the sequential casting of steel strip in steel strip casting equipment wherein under normal operating conditions a steel melt is fed through a pouring tube having discharge ports into the pouring area of a cooled ingot mold at a location below the surface of the melt in the mold and is thereafter removed from the mold in the form of steel strip by the combined operation of mold oscillation means and strip discharge means. After the feed of melt is interrupted, anchoring rods are partially longitudinally immersed into the melt laterally of the pouring area of the mold, and the surface of the melt in the mold is lowered to a level below the pouring area. After a desired interval, the melt feed is continued, and the level of the surface of the melt in the mold is allowed to rise above the discharge ports of the pouring tube. Thereafter, casting flux is applied to the surface of the melt, and the operation of the mold oscillation means and the strip discharge means is resumed. The method also includes the steps of restarting the feed of melt through the pouring tube after a desired interval; allowing the level of the melt in the cavity of the mold to rise above the discharge opening of the pouring tube; thereafter applying a layer of casting flux to the surface of the melt in the mold; and restarting the strip discharge means and the mold oscillation means such that the original level of melt in the cavity in the mold is reestablished and maintained.

    摘要翻译: 一种用于在钢带铸造设备中顺序铸造钢带的方法,其中在正常操作条件下,将钢熔体通过具有排出口的倾倒管进入熔融物表面下方的冷却铸模的浇注区域, 模具,然后通过模具振动装置和带材排出装置的组合操作从钢带形式将其从模具中取出。 在熔体进料被中断之后,锚定杆部分纵向地浸入到模具的浇注区域侧面的熔体中,并且模具中的熔体表面被降低到低于浇注区域的水平。 在期望的间隔之后,继续进行熔体供给,并且允许模具中的熔体的表面的水平高于浇注管的排出口。 此后,将熔剂施加到熔体的表面,并恢复模具振动装置和带材排出装置的操作。 该方法还包括以下步骤:在所需间隔之后重新启动熔体通过浇注管的进料; 允许模具的空腔中的熔体的水平高于浇注管的排出口; 然后将铸造助焊剂层施加到模具中的熔体表面; 并且重新开始带材排出装置和模具振动装置,使得模具中空腔中的原始熔体水平重新建立和维持。

    Method and apparatus for continuously casting metal
    5.
    发明授权
    Method and apparatus for continuously casting metal 失效
    用于连续铸造金属的方法和装置

    公开(公告)号:US4787438A

    公开(公告)日:1988-11-29

    申请号:US14654

    申请日:1987-02-13

    IPC分类号: B22D11/08 B22D11/20 B22D11/18

    CPC分类号: B22D11/202

    摘要: Apparatus and processes for use therewith are provided for the start-up of the continuous casting of strip metal, preferably steel, in which liquid metal is poured into a flared type continuous casting strip-shaped mold equipped with detector means for monitoring the instantaneous surface level of the liquid metal bath formed in the flared zone of the mold, and sensor means for sensing the presence of liquid in the core of the cast strip downstream of the mold, and means are further provided responsive to said detectors and sensor for controlling both the rate of pouring the liquid metal, and the start-up and rate of withdrawal of the cast strip to ensure the continuous presence of a liquid metal core in said cast strip downstream of said mold, for signalling when the distribution ports of the pouring tube become submerged, and for thereafter during casting maintaining a predetermined optimum operating surface level of said metal bath.

    摘要翻译: 提供了用于其的设备和方法,用于连续铸造带状金属(优选钢)的启动,其中将液态金属倒入具有用于监测瞬时表面水平的检测器装置的扩口型连续铸造带状模具中 形成在模具的扩口区域中的液态金属浴的传感器装置,以及用于感测模具下游铸模的芯体中存在的液体的传感器装置,以及响应于所述检测器和传感器进一步提供装置, 浇注液体金属的速率,铸造带的启动和退出速率,以确保在所述模具下游的所述铸造带中液态金属芯的连续存在,用于当浇注管的分配口变为 浸没,并且此后在铸造期间保持所述金属浴的预定的最佳操作表面水平。

    Method and casting roller plant for the semi-endless or endlers rolling by casting of a metal in particular a steel strip which may be transversely separated as required after solidification
    7.
    发明申请
    Method and casting roller plant for the semi-endless or endlers rolling by casting of a metal in particular a steel strip which may be transversely separated as required after solidification 失效
    用于通过铸造金属,特别是固化后可以根据需要横向分离的钢带的半无限或端基滚动的方法和浇铸辊设备

    公开(公告)号:US20050251989A1

    公开(公告)日:2005-11-17

    申请号:US10518085

    申请日:2003-05-02

    摘要: The invention relates to a method and casting roller plant for the semi-endless or endless rolling by casting of a metal, in particular a steel strip (1a), which may be transversely separated as required after solidification. The casting strip part lengths (20) are fed to a roller furnace (2) for heating and equilibration at the rolling temperature and the partial lengths (20) for rolling out are fed to a rolling train (3) for rolling, whereby the strip casting is continued uninterrupted during the rolling operation. According to the invention, a closer matching of the strip casting and the rolling can be carried out, whereby the casting speed (Vc) is reduced for a roller change such that between the end of rolling a preceding multiple length (21) and the insertion of a new partial length (20) or multiple lengths (21) into the rolling gear a sufficient buffer time for a roller exchange is provided.

    摘要翻译: 本发明涉及一种用于通过铸造金属,特别是钢带(1a)进行半无限循环轧制的方法和浇铸辊设备,其可以在固化后根据需要横向分离。 铸造带部件长度(20)被供给到轧辊炉(2),用于在轧制温度下加热和平衡,并且用于轧制的部分长度(20)被供给到用于轧制的轧制系(3),由此带材 在轧制操作期间铸造继续不间断。 根据本发明,可以进行条带铸造和轧制的更紧密的匹配,由此对于辊的变化,铸造速度(Vcc)减小,使得在轧制前端 提供多个长度(21)和将新的部分长度(20)或多个长度(21)插入到滚动齿轮中用于辊更换的足够的缓冲时间。

    Casting machine for production of casting bars in the shape of billets or blocks
    8.
    发明申请
    Casting machine for production of casting bars in the shape of billets or blocks 审中-公开
    用于生产坯料或块状铸件的铸造机

    公开(公告)号:US20090178777A1

    公开(公告)日:2009-07-16

    申请号:US12383234

    申请日:2009-03-19

    申请人: Hans Streubel

    发明人: Hans Streubel

    IPC分类号: B22D11/12

    CPC分类号: B22D11/1206

    摘要: A casting machine for producing cast strands (2) in shape of billets or ingots includes a continuous casting mold (1) for forming a cast strand (2) that is deflected by a cast radius (R) from a vertical casting direction in horizontal casting direction (13), a straightening region (A) having straightening profiled roller pairs (4, 5, 6) with positive diametrical regions (h, b) or negative diametrical regions (−h, −b) for forming the cast strand with one or several projections (h, b) or recesses (−h, −b); and with at least one pair of straightening profiled rollers (4 to 6) provided on both sides of a tangent point (3) of the cast radius (R) and a soft-reduction region (B) adjoining the straightening region and having at least one roller pair (7, 8, 9) with thickness-reducing smooth rollers.

    摘要翻译: 一种用于生产坯料或铸锭的铸造线(2)的铸造机包括用于形成铸造线(2)的连续铸造模具(1),其从水平铸造中的垂直铸造方向以铸造半径(R)偏转 方向(13),具有矫正成型辊对(4,5,6)的矫直区域(A),其具有正直径区域(h,b)或负直径区域(-h,-b),用于形成铸造线材 或几个突起(h,b)或凹槽(-h,-b); 以及设置在铸模半径(R)的切点(3)的两侧上的至少一对矫正成型辊(4至6)和邻近矫直区域的软还原区域(B),并且至少具有 一个辊对(7,8,9),具有减薄平滑辊。

    Method and continuous casting and rolling plant for semi-endless or endless rolling by casting a metal strand, especially a steel strand, which is cut to length as required after solidification
    9.
    发明授权
    Method and continuous casting and rolling plant for semi-endless or endless rolling by casting a metal strand, especially a steel strand, which is cut to length as required after solidification 失效
    用于通过铸造金属股线,特别是钢绞线的半无限循环轧制方法和连续铸造和轧制设备,其在凝固后根据需要被切割成长度

    公开(公告)号:US07478664B2

    公开(公告)日:2009-01-20

    申请号:US11418411

    申请日:2006-05-04

    IPC分类号: B22D11/12 B21B1/46

    摘要: A method for semi-endless or endless rolling by casting a metal strand, especially a steel strand, which is cut to length as required after solidification, wherein the cut lengths of cast strand are fed into a roller hearth furnace for heating and homogenizing at rolling temperature and are then fed at rolling temperature into a rolling mill to be rolled out. The continuous casting is continued without interruption during the rolling operation, and a sufficient buffer time for a roll change is maintained in the rolling mill. For carrying out a roll change, the casting rate is reduced as a function of the feed rate of the rolling mill and/or the roll-changing time, and/or the buffer length of the roller hearth furnace, and/or the final rolled thickness after the strand has been cut to length.

    摘要翻译: 一种用于通过铸造金属股线,特别是钢绞线的半无限循环轧制方法,其在凝固后根据需要被切割成长度,其中将铸造线的切割长度进料到辊底炉中以在轧制中加热和均化 然后在轧制温度下进料到轧机中轧出。 在轧制操作期间连续铸造继续而不中断,并且在轧机中保持足够的辊更换缓冲时间。 为了进行滚动变更,根据轧机的进给速度和/或滚动转换时间和/或辊底炉的缓冲长度和/或最终轧制的速度,铸造速率降低 股线已被切割成长度后的厚度。

    Method and device for continuously casting ingots, slabs or thin slabs
    10.
    发明授权
    Method and device for continuously casting ingots, slabs or thin slabs 有权
    用于连续铸造锭,板或薄板的方法和装置

    公开(公告)号:US07025118B2

    公开(公告)日:2006-04-11

    申请号:US10476361

    申请日:2002-05-02

    IPC分类号: B22D11/12

    CPC分类号: B22D11/1206

    摘要: A continuously cast strand is subjected to soft reduction between the guide rollers below the mold and between the soft reduction stretch and the mold the strand is subjected to format or thickness reduction between at least one pair of position controlled guide rollers so that independently of the quality of the steel, the casting speed and the spray cooling, the position of the type of the mold cavity and hence the molten steel therein is maintained constant along the soft reduction stretch.

    摘要翻译: 连续铸造的股线在模具下方的引导辊之间以及软压缩拉伸和模具之间经受软压缩,该股线在至少一对位置控制的导向辊之间经受格式或厚度减小,使得独立于质量 的钢,铸造速度和喷雾冷却,模腔的类型以及因此其中的钢水的位置沿柔软的还原拉伸保持恒定。