公开(公告)号:US20210163369A1
公开(公告)日:2021-06-03
申请号:US17173355
申请日:2021-02-11
IPC分类号: C04B41/50 , C04B41/87 , C04B41/00 , C04B35/484 , C04B35/486 , C01B3/36 , B01J12/00 , B01J19/02 , C01B3/38 , C04B35/488 , C04B35/622 , C10J3/72
摘要: A method for producing a refractory lining in a combustion chamber operating in a reducing atmosphere. The lining includes at least one or more Zirconia (Zr)-based refractory lining members comprising one or more Zr-based parts. The Zr-based parts comprise at least 90 wt. %, preferably at least 95 wt. %, of monoclinic ZrO2 and/or partially stabilized ZrO2 and/or fully stabilized ZrO2, wherein the total content of tetragonal and cubic ZrO2 amounts to at least 20 wt. %, preferably more than 35 wt. %, as well as Zr based refractory lining members and methods for manufacturing the Zr based refractory lining members.
-
公开(公告)号:US11795118B2
公开(公告)日:2023-10-24
申请号:US17173335
申请日:2021-02-11
IPC分类号: C04B35/484 , B01J12/00 , B01J19/02 , C04B41/50 , C04B41/87 , C04B41/00 , C04B35/486 , C01B3/36 , C01B3/38 , C04B35/488 , C04B35/622 , C10J3/72 , C04B111/00
CPC分类号: C04B41/5042 , B01J12/005 , B01J19/02 , C01B3/36 , C01B3/386 , C04B35/484 , C04B35/486 , C04B35/4885 , C04B35/62222 , C04B41/009 , C04B41/87 , C10J3/72 , B01J2219/0218 , C01B2203/0261 , C01B2203/1235 , C04B2111/0025 , C04B2235/3217 , C04B2235/3244 , C04B2235/3246 , C04B2235/3418 , C04B2235/604 , C04B2235/72 , C04B2235/76 , C04B2235/762 , C04B2235/765 , C04B2235/77 , C04B2235/786 , C04B2235/96 , C04B2235/9669 , C04B41/009 , C04B35/10 , C04B41/5042 , C04B41/4539
摘要: A refractory lining in a combustion chamber operating in a reducing atmosphere. The lining includes at least one or more Zirconia (Zr)-based refractory lining members comprising one or more Zr-based parts. The Zr-based parts comprise at least 90 wt. %, preferably at least 95 wt. %, of monoclinic ZrO2 and/or partially stabilized ZrO2 and/or fully stabilized ZrO2, wherein the total content of tetragonal and cubic ZrO2 amounts to at least 20 wt. %, preferably more than 35 wt. %, as well as Zr based refractory lining members and methods for manufacturing the Zr based refractory lining members.
-
公开(公告)号:US11713282B2
公开(公告)日:2023-08-01
申请号:US17173355
申请日:2021-02-11
IPC分类号: C04B41/50 , C04B41/87 , C04B35/484 , B01J12/00 , B01J19/02 , C04B41/00 , C04B35/486 , C01B3/36 , C01B3/38 , C04B35/488 , C04B35/622 , C10J3/72 , C04B111/00
CPC分类号: C04B41/5042 , B01J12/005 , B01J19/02 , C01B3/36 , C01B3/386 , C04B35/484 , C04B35/486 , C04B35/4885 , C04B35/62222 , C04B41/009 , C04B41/87 , C10J3/72 , B01J2219/0218 , C01B2203/0261 , C01B2203/1235 , C04B2111/0025 , C04B2235/3217 , C04B2235/3244 , C04B2235/3246 , C04B2235/3418 , C04B2235/604 , C04B2235/72 , C04B2235/76 , C04B2235/762 , C04B2235/765 , C04B2235/77 , C04B2235/786 , C04B2235/96 , C04B2235/9669 , C04B41/009 , C04B35/10 , C04B41/5042 , C04B41/4539
摘要: A method for producing a refractory lining in a combustion chamber operating in a reducing atmosphere. The lining includes at least one or more Zirconia (Zr)-based refractory lining members comprising one or more Zr-based parts. The Zr-based parts comprise at least 90 wt. %, preferably at least 95 wt. %, of monoclinic ZrO2 and/or partially stabilized ZrO2 and/or fully stabilized ZrO2, wherein the total content of tetragonal and cubic ZrO2 amounts to at least 20 wt. %, preferably more than 35 wt. %, as well as Zr based refractory lining members and methods for manufacturing the Zr based refractory lining members.
-
公开(公告)号:US20210188722A1
公开(公告)日:2021-06-24
申请号:US17173335
申请日:2021-02-11
IPC分类号: C04B41/50 , C04B41/87 , C04B41/00 , C04B35/484 , C04B35/486 , C01B3/36 , B01J12/00 , B01J19/02 , C01B3/38 , C04B35/488 , C04B35/622 , C10J3/72
摘要: A refractory lining in a combustion chamber operating in a reducing atmosphere. The lining includes at least one or more Zirconia (Zr)-based refractory lining members comprising one or more Zr-based parts. The Zr-based parts comprise at least 90 wt. %, preferably at least 95 wt. %, of monoclinic ZrO2 and/or partially stabilized ZrO2 and/or fully stabilized ZrO2, wherein the total content of tetragonal and cubic ZrO2 amounts to at least 20 wt. %, preferably more than 35 wt. %, as well as Zr based refractory lining members and methods for manufacturing the Zr based refractory lining members.
-
公开(公告)号:US20230227373A1
公开(公告)日:2023-07-20
申请号:US18190469
申请日:2023-03-27
申请人: Topsoe A/S , P-D Refractories GmbH
IPC分类号: C04B41/50 , C04B41/87 , C04B41/00 , C04B35/484 , C04B35/486 , C01B3/36 , B01J12/00 , B01J19/02 , C01B3/38 , C04B35/488 , C04B35/622 , C10J3/72
CPC分类号: C04B41/5042 , C04B41/87 , C04B41/009 , C04B35/484 , C04B35/486 , C01B3/36 , B01J12/005 , B01J19/02 , C01B3/386 , C04B35/4885 , C04B35/62222 , C10J3/72 , C04B2235/762 , C04B2235/765 , C04B2235/77 , C04B2235/786 , C04B2111/0025
摘要: A refractory lining in a combustion chamber operating in a reducing atmosphere. The lining includes at least one or more Zirconia (Zr)-based refractory lining members comprising one or more Zr-based parts. The Zr-based parts comprise at least 90 wt. %, preferably at least 95 wt. %, of monoclinic ZrO2 and/or partially stabilized ZrO2 and/or fully stabilized ZrO2, wherein the total content of tetragonal and cubic ZrO2 amounts to at least 20 wt. %, preferably more than 35 wt. %, as well as Zr based refractory lining members and methods for manufacturing the Zr based refractory lining members.
-
公开(公告)号:US20190218151A1
公开(公告)日:2019-07-18
申请号:US16332091
申请日:2017-10-09
IPC分类号: C04B41/50 , C04B35/488 , C04B35/622 , C04B41/00 , C04B41/87 , C01B3/38 , B01J12/00 , B01J19/02 , C10J3/72
CPC分类号: C04B41/5042 , B01J12/005 , B01J19/02 , B01J2219/0218 , C01B3/36 , C01B3/386 , C01B2203/0261 , C01B2203/1235 , C04B35/484 , C04B35/486 , C04B35/4885 , C04B35/62222 , C04B41/009 , C04B41/87 , C04B2111/0025 , C04B2235/3217 , C04B2235/3244 , C04B2235/3246 , C04B2235/3418 , C04B2235/604 , C04B2235/72 , C04B2235/76 , C04B2235/762 , C04B2235/765 , C04B2235/77 , C04B2235/786 , C04B2235/96 , C04B2235/9669 , C10J3/72 , C04B35/10 , C04B41/4539
摘要: The present application relates to a refractory lining in a combustion chamber operating in a reducing atmosphere, said lining comprising at least one or more Zirconia (Zr)-based refractory lining members comprising one or more Zr-based parts, wherein the Zr-based parts comprises at least 90 wt. %, preferably at least 95 wt. %, of monoclinic ZrO>2 and/or partially stabilized ZrO>2 and/or fully stabilized ZrO>2, wherein the total content of tetragonal and cubic ZrO>2 amounts to at least 20 wt. %, preferably more than 35 wt. % as well as Zr based refractory lining members and methods for manufacturing said Zr based refractory lining members.
-
-
-
-
-