Method for producing polyisobutene
    1.
    发明授权
    Method for producing polyisobutene 有权
    生产聚异丁烯的方法

    公开(公告)号:US07217773B2

    公开(公告)日:2007-05-15

    申请号:US10542928

    申请日:2004-01-23

    IPC分类号: C08F4/14 C08F110/10

    摘要: A process is described for preparing polyisobutene having a content of terminal vinylidene groups of at least 75 mol % by polymerizing isobutene or isobutenic hydrocarbon mixtures in the liquid phase in the presence of a boron trifluoride complex catalyst of the composition (BF3)a.L1b.L2c.L3d where L1 is water, a primary C1–C5-alkanol and/or a secondary C3–C5-alkanol, L2 is at least one aldehyde and/or one ketone, L3 is an ether having at least 5 carbon atoms, a secondary alkanol having at least 6 carbon atoms, a primary alkanol having at least 6 carbon atoms and/or a tertiary alkanol, the b:a ratio is in the range from 0.9 to 3.0, the c:a ratio is in the range from 0.01 to 0.5, and the d:a ratio is in the range from 0 to 1.0.

    摘要翻译: 描述了一种制备具有至少75mol%的末端亚乙烯基含量的聚异丁烯的方法,通过在液相中聚合异丁烯或异丁烯烃混合物,在三元组配合物催化剂存在下, 描述=“在线公式”end =“lead”?>(BF 3) a β-in-line-formula description =“In-line-formula”=“In- 其中L 1是水,主要C 1 -C 5 - 烷醇和/或 仲C 3 -C 5 - 烷醇,L 2是至少一种醛和/或一种酮,L 3, SUP>是具有至少5个碳原子的醚,具有至少6个碳原子的仲链烷醇,具有至少6个碳原子的伯烷醇和/或叔链烷醇,b:a的比例在0.9至 3.0,c:a的比例在0.01至0.5的范围内,d:a的比例为 范围从0到1.0。

    Isobutene polymer functionalization by means of hydroboration
    6.
    发明授权
    Isobutene polymer functionalization by means of hydroboration 有权
    异丁烯聚合物通过硼氢化合物官能化

    公开(公告)号:US07354976B2

    公开(公告)日:2008-04-08

    申请号:US10543510

    申请日:2004-01-27

    IPC分类号: C08C19/00 C08C8/00

    CPC分类号: C08F8/42 C08F10/10

    摘要: A process is described for functionalizing isobutene polymers having terminal olefinic unsaturation by treating with the reaction product of a borane source with from 0.5 to 1.8 equivalents of an alkene having a molecular weight of less than 250 per mole of borane or by treating the isobutene polymer with the borane source in the presence of the alkene. The reaction mixtures retain low viscosity and good stirrability.

    摘要翻译: 描述了通过用硼烷源的反应产物与0.5至1.8当量的每摩尔硼烷分子量小于250的烯烃或通过用异丁烯聚合物处理异丁烯聚合物进行处理来官能化具有末端烯属不饱和度的异丁烯聚合物的方法 在烯烃存在下的硼烷源。 反应混合物保持低粘度和良好的搅拌能力。

    Method for producing a polyisobutene
    10.
    发明授权
    Method for producing a polyisobutene 失效
    聚异丁烯的制造方法

    公开(公告)号:US07745554B2

    公开(公告)日:2010-06-29

    申请号:US12089930

    申请日:2006-10-13

    IPC分类号: C08F4/14 C08F10/10

    CPC分类号: C08F110/10 C08F4/14

    摘要: The invention relates to a process for preparing polyisobutene having a mean molecular weight Mn of from 400 to 50 000, in particular from 500 to 10 000, by polymerizing isobutene in the presence of a BF3-containing complex catalyst, wherein the polymerization is carried out at least temporarily in the presence of one or more cyclic ethers.

    摘要翻译: 本发明涉及通过在含BF 3的络合物催化剂存在下聚合异丁烯来制备平均分子量Mn为400至50,000,特别是500至10000的聚异丁烯的方法,其中进行聚合 至少暂时存在一种或多种环醚。