SOLID STATE IMAGE SENSOR AND MANUFACTURING METHOD THEREOF
    1.
    发明申请
    SOLID STATE IMAGE SENSOR AND MANUFACTURING METHOD THEREOF 审中-公开
    固态图像传感器及其制造方法

    公开(公告)号:US20110001207A1

    公开(公告)日:2011-01-06

    申请号:US12820655

    申请日:2010-06-22

    IPC分类号: H01L31/0232 H01L31/18

    摘要: A solid state image sensor includes: a first pixel and a second pixel, each including a light receiving portion; a first color filter formed in an upper part of the first pixel on a first main surface side of a semiconductor substrate; a second color filter formed in an upper part of the second pixel on the first main surface side of the semiconductor substrate; a metal interconnect layer formed on a second main surface side of the semiconductor substrate; and a substrate contact connected to the second main surface of the semiconductor substrate, and provided between the metal interconnect layer and the second main surface. The first color filter mainly transmits first light therethrough, and the second color filter mainly transmits second light therethrough. The second light has a shorter wavelength than that of the first light. The substrate contact is not provided in the first pixel.

    摘要翻译: 固态图像传感器包括:第一像素和第二像素,每个包括光接收部分; 形成在半导体衬底的第一主表面侧的第一像素的上部的第一滤色器; 第二滤色器,形成在所述半导体衬底的所述第一主表面侧上的所述第二像素的上部; 形成在所述半导体衬底的第二主表面侧上的金属互连层; 以及与半导体基板的第二主表面连接并设置在金属互连层和第二主表面之间的基板接触。 第一滤色器主要透射第一光,第二滤色器主要透射第二光。 第二光的波长比第一光的波长短。 在第一像素中没有提供衬底接触。

    Solid state imaging device including a semiconductor substrate on which a plurality of pixel cells have been formed
    2.
    发明授权
    Solid state imaging device including a semiconductor substrate on which a plurality of pixel cells have been formed 有权
    固态成像装置,包括其上形成有多个像素单元的半导体基板

    公开(公告)号:US07910966B2

    公开(公告)日:2011-03-22

    申请号:US12425029

    申请日:2009-04-16

    IPC分类号: H01L31/062

    摘要: A solid state imaging device including a pixel region where a plurality of pixel cells 10r1, 10g1-10g3, 10b1-10b2 . . . have been formed. When focusing on a red pixel cell whose color filter has the longer transmission peak wavelength and a blue pixel cell whose color filter has the shorter transmission peak wavelength, the distribution of substrate contacts is denser in a region in the vicinity of a photodiode in the red pixel cell than a region in the vicinity of a photodiode in the blue pixel cell.

    摘要翻译: 一种固态成像装置,包括多个像素单元10r1,10g1-10g3,10b1-10b2的像素区域。 。 。 已经形成。 当滤色器具有较长透射峰值波长的红色像素单元和滤色器具有较短透射峰值波长的蓝色像素单元时,基板触点的分布在红色光电二极管附近的区域中更为密集 像素单元比蓝色像素单元中的光电二极管附近的区域。

    SOLID STATE IMAGING DEVICE INCLUDING A SEMICONDUCTOR SUBSTRATE ON WHICH A PLURALITY OF PIXEL CELLS HAVE BEEN FORMED
    3.
    发明申请
    SOLID STATE IMAGING DEVICE INCLUDING A SEMICONDUCTOR SUBSTRATE ON WHICH A PLURALITY OF PIXEL CELLS HAVE BEEN FORMED 有权
    固体状态成像装置,包括形成多个像素电池的半导体基板

    公开(公告)号:US20090294815A1

    公开(公告)日:2009-12-03

    申请号:US12425029

    申请日:2009-04-16

    IPC分类号: H01L31/112 H01L31/0232

    摘要: A solid state imaging device including a pixel region where a plurality of pixel cells 10r1, 10g1-10g3, 10b1-10b2 . . . have been formed. When focusing on a red pixel cell whose color filter has the longer transmission peak wavelength and a blue pixel cell whose color filter has the shorter transmission peak wavelength, the distribution of substrate contacts is denser in a region in the vicinity of a photodiode in the red pixel cell than a region in the vicinity of a photodiode in the blue pixel cell.

    摘要翻译: 一种固态成像装置,包括多个像素单元10r1,10g1-10g3,10b1-10b2的像素区域。 。 。 已经形成。 当滤色器具有较长透射峰值波长的红色像素单元和滤色器具有较短透射峰值波长的蓝色像素单元时,基板触点的分布在红色光电二极管附近的区域中更为密集 像素单元比蓝色像素单元中的光电二极管附近的区域。

    Ni-base alloy, high-temperature member for steam turbine and welded rotor for turbine using the same, and method for manufacturing the same
    4.
    发明授权
    Ni-base alloy, high-temperature member for steam turbine and welded rotor for turbine using the same, and method for manufacturing the same 有权
    镍基合金,蒸汽轮机的高温部件和使用其的涡轮机的焊接转子及其制造方法

    公开(公告)号:US08883072B2

    公开(公告)日:2014-11-11

    申请号:US12551884

    申请日:2009-09-01

    摘要: The present invention provides, in a γ′ phase precipitation strengthening type Ni-base alloy, an alloy excellent in heat treatment capability and weldability and suitable for joint with a ferritic steel. Further, the present invention provides a welded turbine rotor having the strength, ductility, and toughness simultaneously over the whole welded structure when a precipitation strengthening type Ni-base alloy having a heatproof temperature of 675° C. or higher is joined to a ferritic steel.A Ni-base alloy according to the present invention contains cobalt, chromium, aluminum, carbon, boron, and at least either tungsten or molybdenum with the remainder being nickel and inevitable impurities, having an alloy composition including 12 to 25 percent by mass of Co, 10 to 18 percent by mass of Cr, 2.0 to 3.6 percent by mass of Al, 0.01 to 0.15 percent by mass of C, 0.001 to 0.03 percent by mass of B, the total amount of tungsten and molybdenum being 5.0 to 10 percent by mass.A welded turbine rotor is structured by joining or building up by welding a second Ni-base alloy to a first Ni-base alloy that a γ′ phase solid solution temperature thereof is 900° C. or higher and a creep fracture strength at 675° C. is 100 MPa or more, and further welding a ferritic steel to the second Ni-base alloy. The second Ni-base alloy is a γ′ phase (Ni3Al) precipitation strengthening type Ni-base alloy, a γ′ phase solid solution temperature thereof is 850° C. or lower.

    摘要翻译: 本发明在γ-相析出强化型Ni基合金中提供了热处理能力和焊接性优异的合金,适用于与铁素体钢接合的合金。 此外,本发明提供了一种在整个焊接结构中具有强度,延展性和韧性的焊接式涡轮转子,当耐热温度为675℃以上的析出强化型Ni基合金与铁素体钢 。 根据本发明的镍基合金包含钴,铬,铝,碳,硼,以及至少钨或钼,其余为镍和不可避免的杂质,其合金组成包含12〜25质量%的Co ,10〜18质量%的Cr,2.0〜3.6质量%的Al,0.01〜0.15质量%的C,0.001〜0.03质量%的B,钨和钼的总量为5.0〜10质量% 质量 焊接的涡轮转子通过将第二Ni基合金焊接到γ'相固相温度为900℃以上的第一Ni基合金和675°的蠕变断裂强度下, C为100MPa以上,进一步将铁素体钢焊接到第二Ni基合金。 第二Ni基合金是γ'相(Ni3Al)析出强化型Ni基合金,γ'相固溶温度为850℃以下。

    Nickel base wrought alloy
    5.
    发明授权
    Nickel base wrought alloy 有权
    镍基锻造合金

    公开(公告)号:US08524149B2

    公开(公告)日:2013-09-03

    申请号:US12728292

    申请日:2010-03-22

    IPC分类号: C22C19/05 C22C30/00

    CPC分类号: C22C19/055

    摘要: A nickel base alloy includes: by mass, 0.001 to 0.1% of carbon; 12 to 23% of chromium; 15 to 25% of cobalt; 3.5 to 5.0% of aluminum; 4 to 12% of molybdenum; 0.1 to 7.0% of tungsten; and a total amount of Ti, Ta and Nb being not more than 0.5%. A parameter Ps represented by a formula (1) shown below is 0.6 to 1.6, Ps=−7×[C]−0.1×[Mo]+0.5×[Al]  (1) where [C] indicates an amount of carbon; [Mo] indicates an amount of molybdenum; and [Al] indicates an amount of aluminum, by mass percent.

    摘要翻译: 镍基合金包括:质量计,0.001〜0.1%的碳; 12〜23%的铬; 15〜25%的钴; 3.5〜5.0%的铝; 4〜12%的钼; 0.1〜7.0%的钨; Ti,Ta和Nb的总量不大于0.5%。 由下式(1)表示的参数Ps为0.6〜1.6,Ps = -7×[C] -0.1×[Mo] + 0.5×[Al](1)其中,[C]表示碳数; [Mo]表示钼的量; 和[Al]表示铝的质量%。

    Low-thermal-expansion Ni-based super-heat-resistant alloy for boiler and having excellent high-temperature strength, and boiler component and boiler component production method using the same
    7.
    发明授权
    Low-thermal-expansion Ni-based super-heat-resistant alloy for boiler and having excellent high-temperature strength, and boiler component and boiler component production method using the same 有权
    用于锅炉的低热膨胀Ni基超耐热合金并具有优异的高温强度,以及使用其的锅炉部件和锅炉部件生产方法

    公开(公告)号:US08444778B2

    公开(公告)日:2013-05-21

    申请号:US12675688

    申请日:2008-08-29

    IPC分类号: C22C19/05 C22F1/10

    摘要: Disclosed is a low-thermal-expansion Ni-based super-heat-resistant alloy for a boiler, which has excellent high-temperature strength. The alloy can be welded without the need of carrying out any aging treatment. The alloy has a Vickers hardness value of 240 or less. The alloy comprises (by mass) C in an amount of 0.2% or less, Si in an amount of 0.5% or less, Mn in an amount of 0.5% or less, Cr in an amount of 10 to 24%, one or both of Mo and W in such an amount satisfying the following formula: Mo+0.5 W=5 to 17%, Al in an amount of 0.5 to 2.0%, Ti in an amount of 1.0 to 3.0%, Fe in an amount of 10% or less, and one or both of B and Zr in an amount of 0.02% or less (excluding 0%) for B and in an amount of 0.2% or less (excluding 0%) for Zr, with the remainder being 48 to 78% of Ni and unavoidable impurities.

    摘要翻译: 公开了一种用于锅炉的低热膨胀Ni基超耐热合金,其具有优异的高温强度。 可以焊接合金,而不需要进行任何时效处理。 该合金的维氏硬度值为240以下。 该合金含有0.2质量%以下的Si(以质量计),0.5%以下的Si,0.5%以下的Mn,10〜24%的Cr,1种或2种 的Mo和W的量满足下式:Mo + 0.5W = 5〜17%,Al为0.5〜2.0%,Ti为1.0〜3.0%,Fe为10% 以下的B和Zr中的一种或两种,B的含量为0.02%以下(不包括0%),Zr的含量为0.2%以下(不含0%),余量为48〜78 %的Ni和不可避免的杂质。

    Ni-Fe based super alloy, process of producing the same and gas turbine
    8.
    发明授权
    Ni-Fe based super alloy, process of producing the same and gas turbine 有权
    Ni-Fe基超级合金,其制造方法和燃气轮机

    公开(公告)号:US08043068B2

    公开(公告)日:2011-10-25

    申请号:US11206131

    申请日:2005-08-18

    IPC分类号: F01D5/14

    摘要: A Ni—Fe based super alloy having high strength and toughness at high temperatures even when used in high-temperature environments, and a process of producing the super alloy. A turbine disk using the super alloy, a process of producing the turbine disk, a turbine spacer using the super alloy, and a process of producing the turbine spacer, as well as a gas turbine are also provided. The Ni—Fe based super alloy contains not more than 0.03% by weight of C, 14-18% of Cr, 15-45% of Fe, 0.5-2.0% of Al, not more than 0.05% of N, 0.5 to 2.0% of Ti, 1.5-5.0% of Nb, and Ni as a main ingredient.

    摘要翻译: 即使在高温环境下使用时,也能够在高温下具有高强度和韧性的Ni-Fe系超合金,以及超合金的制造方法。 还提供了使用超级合金的涡轮盘,制造涡轮盘的方法,使用超级合金的涡轮间隔件,以及制造涡轮间隔件的工艺以及燃气轮机。 Ni-Fe基超合金含有不超过0.03重量%的Cr,14-18%的Cr,15-45%的Fe,0.5-2.0%的Al,不超过0.05的N,0.5-2.0 Ti的%,Nb的1.5〜5.0%,Ni为主要成分。

    NI-BASE ALLOY, HIGH-TEMPERATURE MEMBER FOR STEAM TURBINE AND WELDED ROTOR FOR TURBINE USING THE SAME, AND METHOD FOR MANUFACTURING THE SAME
    10.
    发明申请
    NI-BASE ALLOY, HIGH-TEMPERATURE MEMBER FOR STEAM TURBINE AND WELDED ROTOR FOR TURBINE USING THE SAME, AND METHOD FOR MANUFACTURING THE SAME 有权
    NI-BASE合金,用于蒸汽涡轮机的高温部件和使用该涡轮机的涡轮机的焊接转子及其制造方法

    公开(公告)号:US20100059146A1

    公开(公告)日:2010-03-11

    申请号:US12551884

    申请日:2009-09-01

    摘要: The present invention provides, in a γ′ phase precipitation strengthening type Ni-base alloy, an alloy excellent in heat treatment capability and weldability and suitable for joint with a ferritic steel. Further, the present invention provides a welded turbine rotor having the strength, ductility, and toughness simultaneously over the whole welded structure when a precipitation strengthening type Ni-base alloy having a heatproof temperature of 675° C. or higher is joined to a ferritic steel.A Ni-base alloy according to the present invention contains cobalt, chromium, aluminum, carbon, boron, and at least either tungsten or molybdenum with the remainder being nickel and inevitable impurities, having an alloy composition including 12 to 25 percent by mass of Co, 10 to 18 percent by mass of Cr, 2.0 to 3.6 percent by mass of Al, 0.01 to 0.15 percent by mass of C, 0.001 to 0.03 percent by mass of B, the total amount of tungsten and molybdenum being 5.0 to 10 percent by mass.A welded turbine rotor is structured by joining or building up by welding a second Ni-base alloy to a first Ni-base alloy that a γ′ phase solid solution temperature thereof is 900° C. or higher and a creep fracture strength at 675° C. is 100 MPa or more, and further welding a ferritic steel to the second Ni-base alloy. The second Ni-base alloy is a γ′ phase (Ni3Al) precipitation strengthening type Ni-base alloy, a γ′ phase solid solution temperature thereof is 850° C. or lower.

    摘要翻译: 本发明在γ-相析出强化型Ni基合金中提供了热处理能力和焊接性优异的合金,适用于与铁素体钢接合的合金。 此外,本发明提供了一种在整个焊接结构中具有强度,延展性和韧性的焊接式涡轮转子,当耐热温度为675℃以上的析出强化型Ni基合金与铁素体钢 。 根据本发明的镍基合金包含钴,铬,铝,碳,硼,以及至少钨或钼,其余为镍和不可避免的杂质,其合金组成包含12〜25质量%的Co ,10〜18质量%的Cr,2.0〜3.6质量%的Al,0.01〜0.15质量%的C,0.001〜0.03质量%的B,钨和钼的总量为5.0〜10质量% 质量 焊接的涡轮转子通过将第二Ni基合金焊接到γ'相固相温度为900℃以上的第一Ni基合金和675°的蠕变断裂强度下, C为100MPa以上,进一步将铁素体钢焊接到第二Ni基合金。 第二Ni基合金是γ'相(Ni3Al)析出强化型Ni基合金,γ'相固溶温度为850℃以下。