摘要:
A process for producing an aromatic polyester having an increased degree of polymerization. The process comprises reacting a hydroxyl-terminated, substantially linear, fiber-forming aromatic polyester having an aromatic dicarboxylic acid as a main acid component at an elevated temperature with a bi-cyclic imino ester compound of formula [I] or formula [II]. According to the process, the molecular chains of the aromatic polyester are bonded to each other by the terminal hydroxyl groups thereof to form rapidly the aromatic polyester having an increased degree of polymerization.
摘要:
A laminated film structure composed of a polyester film and an electroconductive metal layer laminated to at least one surface of the polyester resin film, characterized in that said polyester film is an unstretched film of a cured aromatic polyester having a crosslinking degree of not less than 70%, a swelling degree of not more than 30 and an elongation at room temperature of not less than 10%; and a process for producing said film structure.
摘要:
A process for producing an aromatic polyester having an increased degree of polymerization, which comprises reacting a substantially linear, fiber forming aromatic polyester containing terminal hydroxyl groups and having an aromatic dicarboxylic acid as a main acid component at an elevated temperature with a bis-cyclic imino ether compound of the formula [I] such as 2,2'-bis(2-oxazoline), 2,2'-bis(5,6-dihydro-4H-1,3-oxadine) thereby bonding the molecular chains of the aromatic polyester to each other by the terminal carboxyl groups thereof to rapidly form said aromatic polyester having an increased degree of polymerization.Said reaction can be carried out under atmospheric or elevated pressure.According to the process, an aromatic polyester having a low terminal caboxyl concentration and an increased degree of polymerization can be obtained.
摘要:
The invention relates to a resin composition comprising 100 parts by weight polyamide 4.6 resin and 2 to 200 parts by weight of a polyamide amide resin.The composition has improved HDT in wet state and improved impact resistance in dry state.
摘要:
The arylene sulfide ketone copolymers according to the present invention have mainly recurring units which are represented by formulas (I) and (II), ##STR1## The arylene sulfide ketone copolymers have a high glass transition point and excellent moldability and can be produced with industrial advantage.
摘要:
A process for producing a thermoset resin, which comprises reacting (A) an organic compound containing at least two groups selected from the class consisting of alcoholic hydroxyl groups, aromatic amino groups and aromatic aminomethyl groups, and (B) a poly(cyclic iminoether) in the presence of (C) a compound acting as an acid catalyst, at an elevated temperature.
摘要:
A polyamideimide having an inherent viscosity of above 0.48 which comprises a unit of the following formula (II) ##STR1## and a unit of the following formula (IV) ##STR2## as main units forming the molecular chains of the polyamideimide, and an intimate mixture of the polyamideimide and a plasticizing material for the polyamideimide.
摘要:
A process for producing a shaped article of polyamide which comprises (1) melt-shaping an intimate mixture of 100 parts by weight of a polyamide having hexamethylene terephthalamide as main recurring units and 20 to 500 parts by weight of an aromatic hydroxy compound, and then (2) removing the aromatic hydroxy compound from the resulting shaped article by extraction.
摘要:
A process for producing a film-like or fibrous structure of an aromatic polyester, which comprises(1) forming an unstretched film-like or fibrous structure by melt-shaping a blend comprising 100 parts by weight of (A) an aromatic polyester having a high degree of polymerization derived from an aromatic dicarboxylic acid as a main acid component and an aliphatic diol and/or an alicyclic diol as a main glycol component and (B) 3 to 300 parts by weight of a low-molecular-weight compound being substantially non-reactive with the aromatic polyester (A) and having a boiling point of at least about 200.degree. C. under atmospheric pressure and a molecular weight of not more than 1,000,(2) stretching the resulting film-like or fibrous structure,(3) extracting at least a major portion of the low-molecular-weight compound from the stretched film-like or fibrous structure by using an organic solvent which does not substantially dissolve the aromatic polyester under the extracting conditions, and(4) if desired, heat-setting the film-like or fibrous structure after the stretching step (2) and/or the extracting step (3).The film-like or fibrous structure of an aromatic polyester prepared by the process substantially contains no low-molecular-weight compound or contains the low-molecular-weight compound in an amount of up to about 1 part by weight at most per 100 parts by weight of the aromatic polyester.
摘要:
An aromatic polyester:(1) consisting essentially of a polymer unit A of the formula (1), ##STR1## a polymer unit B of the formula (2), ##STR2## and a polymer unit C of the formula (3), ##STR3## the above polymer units being bonded together forming ester linkages in a polymer chain,(2) the polymer unit C being contained in an amount of 10 to 35 mol % based of the total amount of the polymer units B and C,(3) the polyester being semicrystalline,(4) the polyester having an inherent viscosity, measured in a phenol/1,1,2,2-tetrachloroethane mixed solvent (weight ratio=60/40) at 35.degree. C., of at least 0.3; a process for its production; and a resin composition containing it.