Method for producing a modified propylene polymer
    1.
    发明授权
    Method for producing a modified propylene polymer 失效
    改性丙烯聚合物的制造方法

    公开(公告)号:US07795353B2

    公开(公告)日:2010-09-14

    申请号:US11270453

    申请日:2005-11-10

    IPC分类号: C08F110/04

    摘要: Disclosed is a method for producing a modified propylene polymer, the method comprising heating a mixture of 100 parts by weight of a propylene polymer (A) defined below and from 0.1 to 50 parts by weight of an ethylenically unsaturated bond-containing monomer (B) in the presence of from 0.01 to 20 parts by weight of an organic peroxide (C); propylene polymer (A) being a propylene polymer composed of from 0.5 to 90% by weight of a propylene polymer component (A1) having an intrinsic viscosity [η], as measured in tetralin at 135° C., of from 5 dl/g to 15 dl/g and from 10 to 99.5% by weight of a propylene polymer component (A2) having an intrinsic viscosity [η], as measured in tetralin at 135° C., of not less than 0.1 dl/g but less than 5 dl/g.

    摘要翻译: 公开了一种制备改性丙烯聚合物的方法,该方法包括加热100重量份下文定义的丙烯聚合物(A)和0.1-50重量份含烯属不饱和键的单体(B)的混合物, 在有机过氧化物(C)为0.01〜20重量份的情况下, 丙烯聚合物(A)是丙烯聚合物,其由0.5至90重量%的丙烯聚合物组分(A1)在135℃下在四氢化萘中测得的特性粘度[η]为5dl / g至15dl / g和10至99.5wt%的在135℃下在四氢化萘中测得的特性粘度[η]的丙烯聚合物组分(A2)不小于0.1dl / g,但 小于5dl / g。

    Method for producing a modified propylene polymer
    2.
    发明申请
    Method for producing a modified propylene polymer 失效
    改性丙烯聚合物的制造方法

    公开(公告)号:US20060148995A1

    公开(公告)日:2006-07-06

    申请号:US11270453

    申请日:2005-11-10

    IPC分类号: C08F263/00

    摘要: Disclosed is a method for producing a modified propylene polymer, the method comprising heating a mixture of 100 parts by weight of a propylene polymer (A) defined below and from 0.1 to 50 parts by weight of an ethylenically unsaturated bond-containing monomer (B) in the presence of from 0.01 to 20 parts by weight of an organic peroxide (C); propylene polymer (A) being a propylene polymer composed of from 0.5 to 90% by weight of a propylene polymer component (A1) having an intrinsic viscosity [η], as measured in tetralin at 135° C., of from 5 dl/g to 15 dl/g and from 10 to 99.5% by weight of a propylene polymer component (A2) having an intrinsic viscosity [η], as measured in tetralin at 135° C., of not less than 0.1 dl/g but less than 5 dl/g.

    摘要翻译: 公开了一种制备改性丙烯聚合物的方法,该方法包括加热100重量份下文定义的丙烯聚合物(A)和0.1-50重量份含烯属不饱和键的单体(B)的混合物, 在有机过氧化物(C)为0.01〜20重量份的情况下, 丙烯聚合物(A)是丙烯聚合物,其由0.5至90重量%的丙烯聚合物组分(A1)在135℃下在四氢化萘中测得的特性粘度η为5dl / g 至15dl / g和10至99.5wt%的丙烯聚合物组分(A2),其特性粘度η在135℃下在四氢化萘中测得为不小于0.1dl / g但小于 5 dl / g。

    Olefin Polymer Composition Powder and Modified Olefin Polymer
    3.
    发明申请
    Olefin Polymer Composition Powder and Modified Olefin Polymer 审中-公开
    烯烃聚合物组合物粉末和改性烯烃聚合物

    公开(公告)号:US20080033076A1

    公开(公告)日:2008-02-07

    申请号:US11667315

    申请日:2005-11-10

    摘要: Disclosed is an olefin polymer composition powder having excellent powder properties which is useful as a raw material for a modified olefin polymer having high modification degree. Also disclosed is a modified olefin polymer having high modification degree obtained from such an olefin polymer composition powder. Specifically disclosed is an olefin polymer composition powder containing 100 parts by weight of an olefin polymer powder (A), 0.1-20 parts by weight of an ethylenically unsaturated bond-containing monomer (B), 0.1-20 parts by weight of an organic peroxide (C) and 0.1-20 parts by weight of an organic porous powder (D). Also specifically disclosed is a modified olefin polymer obtained by heating such a powder.

    摘要翻译: 公开了一种具有优异粉末性质的烯烃聚合物组合物粉末,其可用作具有高改性度的改性烯烃聚合物的原料。 还公开了由这种烯烃聚合物组合物粉末获得的具有高改性度的改性烯烃聚合物。 具体公开了一种烯烃聚合物组合物粉末,其含有100重量份的烯烃聚合物粉末(A),0.1-20重量份的含烯属不饱和键的单体(B),0.1-20重量份的有机过氧化物 (C)和0.1-20重量份的有机多孔粉末(D)。 还具体公开了通过加热这种粉末获得的改性烯烃聚合物。

    Organic electroluminescent element, method for manufacturing the organic electroluminescent element, and light emitting display device
    4.
    发明授权
    Organic electroluminescent element, method for manufacturing the organic electroluminescent element, and light emitting display device 失效
    有机电致发光元件,有机电致发光元件的制造方法以及发光显示装置

    公开(公告)号:US08497497B2

    公开(公告)日:2013-07-30

    申请号:US12883263

    申请日:2010-09-16

    IPC分类号: H01L35/24

    CPC分类号: H01L51/5048 H01L51/5221

    摘要: Disclosed is an organic electroluminescent element having an element structure that can reduce damage to an organic layer during electrode formation and can facilitate the injection of charges from the electrode into the organic layer. The organic electroluminescent element includes an anode, a cathode, and an organic layer held between the anode and the cathode. The organic layer contains a luminescent material. The organic electroluminescent element further includes a transparent protective layer provided between the anode or the cathode and the organic layer. The transparent protective layer contains a bipolar charge transport organic compound and an electron-accepting compound. The transparent protective layer is formed in a period between after the formation of the organic layer and before the formation of the anode or the cathode on the organic layer.

    摘要翻译: 公开了一种有机电致发光元件,其具有可以在电极形成期间减少对有机层的损伤的元件结构,并且可以促进电荷从电极注入到有机层中。 有机电致发光元件包括阳极,阴极和保持在阳极和阴极之间的有机层。 有机层含有发光材料。 有机电致发光元件还包括设置在阳极或阴极与有机层之间的透明保护层。 透明保护层含有双极电荷输送有机化合物和电子接受性化合物。 透明保护层是在有机层形成之后和在有机层上形成阳极或阴极之间的期间形成的。

    Flexible substrate and organic device using the same
    5.
    发明申请
    Flexible substrate and organic device using the same 失效
    柔性基板和使用相同的有机器件

    公开(公告)号:US20050236985A1

    公开(公告)日:2005-10-27

    申请号:US11106346

    申请日:2005-04-14

    摘要: The present invention provides a flexible substrate, which has solvent resistance, a high level of gas barrier properties, a high level of flexibility, high heat resistance, and a high level of transparency, and is suitable, for example, for use in a wet coating process of an organic device material, and an organic device using the same. The flexible substrate comprises a metal oxide polymer-containing layer and a three-dimensionally crosslinked polymer layer stacked in that order on at least one side of a very thin glass. The metal oxide polymer is a silicon oxide polymer, and the metal oxide polymer-containing layer underlying the three-dimensionally crosslinked polymer layer is neither swollen nor dissolved in an aromatic organic solvent.

    摘要翻译: 本发明提供一种柔性基材,其具有耐溶剂性,高水平的阻气性,高水平的柔韧性,高耐热性和高水平的透明性,并且适用于例如用于湿 有机器件材料的涂布工艺,以及使用其的有机器件。 柔性基材包括含金属氧化物聚合物的层和在非常薄的玻璃的至少一面上依次层叠的三维交联的聚合物层。 金属氧化物聚合物是氧化硅聚合物,三维交联聚合物层下面的含金属氧化物聚合物的层既不溶胀也不溶解在芳族有机溶剂中。

    Method for producing modified propylene polymer
    6.
    发明授权
    Method for producing modified propylene polymer 有权
    改性丙烯聚合物的制备方法

    公开(公告)号:US08716408B2

    公开(公告)日:2014-05-06

    申请号:US13425595

    申请日:2012-03-21

    IPC分类号: C08F8/00 C08F8/02

    CPC分类号: C08F255/02

    摘要: Disclosed is a method for producing a modified propylene polymer that exhibits low flowability and also exhibits little fluctuation in melt flow rate compared with the melt flow rate of the propylene polymer before modification, the method involving a heat treatment step of subjecting a mixture comprising 100 parts by weight of a propylene polymer (A), from 0.1 to 50 parts by weight of an ethylenically unsaturated bond-containing compound (B), and from 0.01 to 20 parts by weight of an organic peroxide (C) whose decomposition temperature at which the half-life thereof becomes 1 minute is lower than 120° C. to heat treatment by using an extruder at a temperature lower than the decomposition temperature of the organic peroxide (C) at which the half-life thereof becomes 1 minute.

    摘要翻译: 本发明公开了一种改性丙烯聚合物的制造方法,其特征在于,与改性前的丙烯类聚合物的熔体流动速率相比,流动性低,熔体流动速率变动不大,涉及热处理工序的方法, 的丙烯聚合物(A),0.1〜50重量份的含烯属不饱和键的化合物(B)和0.01〜20重量份的有机过氧化物(C),其分解温度为 其半衰期为1分钟低于120℃,通过使用挤出机在低于半衰期为1分钟的有机过氧化物(C)的分解温度的温度下进行热处理。

    Process for producing solid product, solid catalyst component, and catalyst for olefin polymerization, and process for producing olefin polymer
    7.
    发明授权
    Process for producing solid product, solid catalyst component, and catalyst for olefin polymerization, and process for producing olefin polymer 失效
    生产固体产品,固体催化剂组分和烯烃聚合催化剂的方法,以及烯烃聚合物的制备方法

    公开(公告)号:US06683139B2

    公开(公告)日:2004-01-27

    申请号:US10025708

    申请日:2001-12-26

    IPC分类号: C08F416

    CPC分类号: C08F10/00 C08F4/6567

    摘要: There are provided (1) a process for producing a solid product, which comprises the step of reducing a titanium compound represented by the following formula [I] with an organomagnesium compound in the presence of an organosilicon compound having an Si—O bond, an inorganic fine particle and optionally an ester compound, (2) a process for producing a solid catalyst component, which comprises the step of contacting the solid product obtained by the above process, a halogenation ability-carrying halogeno compound, and an inner electron donor compound, (3) a process for producing a catalyst, which comprises the step of contacting the solid catalyst component obtained by the above process, an organoaluminum compound, and an outer electron donor compound, and (4) a process for producing an olefin polymer, which comprises the step of polymerizing an olefin in the presence of the catalyst obtained by the above process.

    摘要翻译: 提供(1)固体产物的制造方法,其包括在有Si-O键的有机硅化合物的存在下,用有机镁化合物还原下述式[I]表示的钛化合物的工序, 无机细颗粒和任选的酯化合物,(2)固体催化剂组分的制备方法,其包括使通过上述方法获得的固体产物,含卤化能力的卤代化合物和内部电子给体化合物 (3)制备催化剂的方法,其包括使通过上述方法获得的固体催化剂组分与有机铝化合物和外电子给体化合物接触的步骤,和(4)烯烃聚合物的制备方法, 其包括在通过上述方法获得的催化剂存在下聚合烯烃的步骤。

    Flexible substrate and organic device using the same
    8.
    发明授权
    Flexible substrate and organic device using the same 失效
    柔性基板和使用相同的有机器件

    公开(公告)号:US07812530B2

    公开(公告)日:2010-10-12

    申请号:US11106346

    申请日:2005-04-14

    IPC分类号: H01J1/62 H01J63/04 B32B9/00

    摘要: The present invention provides a flexible substrate, which has solvent resistance, a high level of gas barrier properties, a high level of flexibility, high heat resistance, and a high level of transparency, and is suitable, for example, for use in a wet coating process of an organic device material, and an organic device using the same. The flexible substrate comprises a metal oxide polymer-containing layer and a three-dimensionally crosslinked polymer layer stacked in that order on at least one side of a very thin glass. The metal oxide polymer is a silicon oxide polymer, and the metal oxide polymer-containing layer underlying the three-dimensionally crosslinked polymer layer is neither swollen nor dissolved in an aromatic organic solvent.

    摘要翻译: 本发明提供一种柔性基材,其具有耐溶剂性,高水平的阻气性,高水平的柔韧性,高耐热性和高水平的透明性,并且适用于例如用于湿 有机器件材料的涂布工艺,以及使用其的有机器件。 柔性基材包括含金属氧化物聚合物的层和在非常薄的玻璃的至少一面上依次层叠的三维交联的聚合物层。 金属氧化物聚合物是氧化硅聚合物,三维交联聚合物层下面的含金属氧化物聚合物的层既不溶胀也不溶解在芳族有机溶剂中。

    FPC with via holes with filler being welded to suspension and drive apparatus
    9.
    发明授权
    FPC with via holes with filler being welded to suspension and drive apparatus 有权
    带通孔的FPC与填料焊接到悬架和驱动装置

    公开(公告)号:US07542242B2

    公开(公告)日:2009-06-02

    申请号:US10959429

    申请日:2004-10-07

    IPC分类号: G11B5/48

    摘要: A suspension includes a flexure constituted by a metal plate member, for supporting a head slider provided with at least one head element, a load beam provided with a top end section and constituted by a metal plate member, for supporting the flexure at the top end section, and an individual FPC member attached to the flexure and the load beam and provided with trace conductors to be electrically connected to the at least one head element of the head slider. The FPC member includes a plurality of via holes provided with metal fillers filled therein, the metal fillers in the respective via holes are welded to the flexure and/or the load beam, and the FPC member is fixed to the flexure and/or the load beam at least by means of the welding.

    摘要翻译: 悬架包括由金属板构件构成的挠曲件,用于支撑设置有至少一个头部元件的头部滑块,设置有顶端部分并由金属板构件构成的负载梁,用于在顶端支撑弯曲部 以及附接到挠曲件和负载梁的单独的FPC构件,并且设置有电连接到头滑块的至少一个头元件的迹线导体。 FPC部件包括设置有填充有金属填充物的多个通孔,各通路孔中的金属填充物焊接到挠曲部和/或负载梁上,FPC部件固定在挠曲部和/或负载部 至少通过焊接。

    Polypropylene resin composition and molded article comprising the same
    10.
    发明授权
    Polypropylene resin composition and molded article comprising the same 有权
    聚丙烯树脂组合物和包含其的模制品

    公开(公告)号:US09102820B2

    公开(公告)日:2015-08-11

    申请号:US12055442

    申请日:2008-03-26

    摘要: A polypropylene resin composition is disclosed which contains a propylene polymer (A) selected from the group consisting of propylene homopolymers (A-1) and propylene-ethylene block copolymers (A-2) which are propylene-ethylene block copolymers each of which is composed of a propylene homopolymer component and a propylene-ethylene random copolymer component and has an intrinsic viscosity of from 2 to 8 dl/g, an ethylene-α-olefin copolymer (B) defined below, the amount of the polymer (A) and the amount of the copolymer (B) each being based on the combined amount of the polymer (A) and the copolymer (B) which is an ethylene-α-olefin copolymer having a melt index, as measured at 190° C., of from 1 to 40 g/10 min, and a petroleum resin (C-1) or a terpene resin (C-2) having a glass transition temperature of 90° C. or lower.