公开(公告)号:US10086557B2
公开(公告)日:2018-10-02
申请号:US14139482
申请日:2013-12-23
Applicant: INDUSTRIAL TECHNOLOGY RESEARCH INSTITUTE
Inventor: Cheng-Hsing Fan , Chun-Yen Chen , Ming-Tsong Leu , Chien-Pang Wu
IPC: C08L67/00 , C08L67/02 , C08L67/03 , C08G63/12 , C08G63/123 , C08G63/127 , C08G63/137 , C08G63/16 , C08G63/18 , C08G63/183 , C08G63/199 , B29C47/00 , B29C47/36 , B29C47/40 , B29C47/88 , B29C55/00 , B29C55/02 , B29C55/10 , B29C55/12 , B29D11/00 , B32B27/36 , B29C55/16 , C08J5/18 , B29K67/00 , B29K105/00 , B29L7/00 , B29L11/00
Abstract: Disclosed is a method for manufacturing a film. 50 wt % to 85 wt % of a first polyester and 50 wt % to 15 wt % of a second polyester are dried and mixed to form a mixture. The first polyester is polyethylene terephthalate (PET), polyethylene naphthalate (PEN), or combinations thereof. The second polyester is copolymerized of 1 part by mole of terephthalic acid, m parts by mole of 1,4-cyclohexanedimethanol (1,4-CHDM), n parts by mole of 1,3-cyclohexanedimethanol (1,3-CHDM), and o parts by mole of ethylene glycol (EG). m+n+o=1, 0≤o≤0.4, 0.6≤m+n≤1, and 0.06≤n/m≤1.31. The mixture is melted and blended to form a polyester composition, which is extruded to form a sheet. The sheet is then biaxially stretched to obtain a film. The biaxially stretched film is then treated with a thermal setting.
-
公开(公告)号:US09163139B2
公开(公告)日:2015-10-20
申请号:US13727522
申请日:2012-12-26
Applicant: INDUSTRIAL TECHNOLOGY RESEARCH INSTITUTE
Inventor: Chien-Pang Wu , Jyh-Horng Wu , Kuo-Chen Shih , Chi-Yuan Hung , Chia-Hao Li , Yao-Zu Wu , Chuh-Yung Chen
CPC classification number: C08L53/00 , C08F297/00 , C08J5/18 , C08J2367/04 , C08J2453/00 , C08L67/00 , C08L67/04
Abstract: An extended film and a manufacturing method thereof are provided. The extended film includes a poly(lactic acid) and a block copolymer, wherein the block polymer includes a first block, a second block and a third block that connected with each other by chemical bonds. The extended film is formed by steps of mixing poly(lactic acid) and the block copolymer to form a mixture, compressing the mixture to form a board body and extending the board body to form an extended film, thereby forming an extended film having properties of high thermal-resistance and high transparency, the film thus obtained is applicable for packaging use.
Abstract translation: 提供了一种延伸膜及其制造方法。 延伸膜包括聚(乳酸)和嵌段共聚物,其中嵌段聚合物包括通过化学键彼此连接的第一嵌段,第二嵌段和第三嵌段。 延伸膜通过混合聚(乳酸)和嵌段共聚物以形成混合物的步骤形成,压缩混合物以形成板体并延伸板体以形成延伸膜,由此形成延伸膜,其具有 高耐热性和高透明性,因此得到的膜适用于包装用途。
-
公开(公告)号:US09963533B2
公开(公告)日:2018-05-08
申请号:US14978968
申请日:2015-12-22
Applicant: INDUSTRIAL TECHNOLOGY RESEARCH INSTITUTE
Inventor: Chien-Pang Wu , Li-Cheng Jheng , Chia-Hao Li , Jyh-Horng Wu , Hsi-Hsin Shih
IPC: C08F236/12 , C08L63/00 , C08G81/02
CPC classification number: C08F236/12 , C08G81/025 , C08L63/00 , C08L2205/06 , C08L53/00 , C08L87/005
Abstract: A copolymer is provided, which includes a chemical structure of: R is C1-6 alkylene group. T is a terminal group including C1-6 alkyl group, C3-6 cycloalkyl group, or C6-12 aromatic group. l is 0.05 to 0.3, m is 0.1 to 0.2, n is 0.5 to 0.8, l+m+n=1, x is 40 to 100, and o is 10 to 120. An epoxy resin composite is also provided, which includes 100 parts by weight of epoxy resin and 1 to 20 parts by weight of toughness enhancer such as the above copolymer.
-
-