发明人: Tien-Heng HUANG , Yu-Han WU , Kuo-Chuang CHIU
IPC分类号: C04B35/488 , C04B35/622 , H01L23/00
摘要: A ceramic material includes zirconia toughened alumina (ZTA), which is doped with zinc ions and other metal ions, in which the other metal ions are chromium (Cr) ions, titanium (Ti) ions, gadolinium (Gd) ions, manganese (Mn) ions, cobalt (Co) ions, iron (Fe) ions, or a combination thereof. The ceramic material may have a hardness of 1600 Hv10 to 2200 Hv10 and a bending strength of 600 MPa to 645 MPa. The ceramic material can be used as wire bonding capillary.
-
公开(公告)号:US20210198154A1
公开(公告)日:2021-07-01
申请号:US17133270
申请日:2020-12-23
发明人: Kuo-Chuang CHIU , Tzu-Yu LIU , Tien-Heng HUANG , Tzu-Chi CHOU , Cheng-Ting LIN
IPC分类号: C04B35/64 , C04B35/14 , C04B35/628
摘要: A method of forming low-k material is provided. The method includes providing a plurality of core-shell particles. The core of the core-shell particles has a first ceramic with a low melting point. The shell of the core-shell particles has a second ceramic with a low melting point and a low dielectric constant. The core-shell particles are sintered and molded to form a low-k material. The shell of the core-shell particles is connected to form a network structure of a microcrystal phase.
-
公开(公告)号:US20240217878A1
公开(公告)日:2024-07-04
申请号:US18170367
申请日:2023-02-16
发明人: Tien-Heng HUANG , Yu-Han WU , Kuo-Chuang CHIU
CPC分类号: C04B35/18 , C04B35/64 , C04B2235/3298 , C04B2235/3409 , C04B2235/3463 , C04B2235/723 , C04B2235/728
摘要: A method of forming a ceramic material includes providing a mixture of solid powder, which includes precursors of crystalline aluminum silicate, amorphous fluxing agent, and amorphous modifier. The method also sinters the mixture of solid powder at 1600° C. to 1800° C. to form the ceramic material, which includes 100 parts by weight of the crystalline aluminum silicate having a chemical formula of AlSixO1.5+2x, wherein x is 0.21 to 0.35, 10 to 15 parts by weight of the amorphous fluxing agent, and 5 to 10 parts by weight of the amorphous modifier.
-
公开(公告)号:US20230202928A1
公开(公告)日:2023-06-29
申请号:US17564082
申请日:2021-12-28
发明人: Tien-Heng HUANG , Yu-Han WU , Kuo-Chuang CHIU , Chieh-Yu YANG
IPC分类号: C04B35/10
CPC分类号: C04B35/10 , C04B2235/3217 , C04B2235/3244 , C04B2235/3224 , C04B2235/3275 , C04B2235/3241 , C04B2235/3232 , C04B2235/3262 , C04B2235/3279
摘要: A ceramic material includes zirconia toughened alumina (ZTA) doped with scandium (Sc) ions. ZTA can be further doped with other metal ions, and the other metal ions include cobalt (Co) ions, chromium (Cr) ions, zinc (Zn) ions, titanium (Ti) ions, manganese (Mn) ions, nickel (Ni) ions, or a combination thereof. The ceramic material can be used as a ceramic object, such as a wire bonding capillary, a heat dissipation plate, a denture tooth, orthopedic implants, direct bonded copper, or a high-temperature co-fired ceramic.
-
-
-