Applicant: INEOS STYROLUTION GROUP GMBH
Inventor: Norbert NIESSNER , Gisbert MICHELS , Frank EISENTRAEGER , Shridhar MADHAV , Kirit GEVARIA , Pratik BHAVSAR , KwanHee LEE
IPC: C08L25/12
Abstract: A heat resistant ABS thermoplastic molding composition with reduced odor can be employed for automotive interior applications if it comprises a graft copolymer (A) based on a diene rubber latex substrate with a SAN graft sheath; a SAN matrix polymer (B) and specific amounts of additives such as fatty acid amides or fatty acid esters,metal oxides such as MgO, CaO or ZnO, antioxidants and a silicon oil having a kinematic viscosity in the range of from 25000 to 80000 centi Stokes.
-
公开(公告)号:US20190119487A1
公开(公告)日:2019-04-25
申请号:US16094650
申请日:2017-04-18
Applicant: INEOS STYROLUTION GROUP GMBH
Inventor: Janna MICHAELIS DE VASCONCELLOS , Norbert NIESSNER , KwanHee LEE , Gisbert MICHELS
IPC: C08L51/04 , C08L55/02 , C08L23/08 , C08F212/10 , C08F220/44 , B29C48/00 , C08K3/26 , C08K3/34
Abstract: Thermoplastic molding composition scan be advantageously used in hydrofluoro olefin containing areas, comprising components A, B, C and, D: 10 to 35 wt.-% ABS graft rubber A obtained by emulsion polymerization, 50 to 75 wt.-% SAN copolymer B, 4 to 20 wt.-% copolymer C from ethylene and C1-C6-alkyl(meth)acrylate, and 4 to 20 wt.-% ABS graft rubber copolymer D obtained by mass polymerization.
-
公开(公告)号:US20210108069A1
公开(公告)日:2021-04-15
申请号:US16970033
申请日:2019-02-13
Applicant: INEOS STYROLUTION GROUP GMBH
Inventor: Norbert NIESSNER , Gisbert MICHELS , KwanHee LEE , Shridhar MADHAV , Kirit GEVARIA , Nirmalendu DEBATA
Abstract: High heat resistant ABS molding compositions for use in the automotive sector, electronics, and household or healthcare sector comprising: (A) 15 to 35 wt.-% ABS graft copolymer (A); (B) 15 to 35 wt.-% a-methylstyrene/acrylonitrile copolymer (B) (weight ratio 95:5 to 50:50); (C) 20 to 40 wt.-% styrene/acrylonitrile copolymer (C) (weight ratio 95:5 to 50:50; Mw 150,000 to 300,000); (D) 10 to 30 wt.-% random terpolymer (D) made from 13 to 27 wt.-% α, β ethylenically unsaturated cyclic anhydride, 60 to 74 wt.-% aromatic vinyl monomer, and 13 to 27 wt.-% maleimide monomer); (E) 0.1 to 5 wt.-%, of at least one elastomeric block copolymer (E) comprising a vinylaromatic monomer block S and an elastomeric random diene/vinylaromatic onomer block B/S; hard phase proportion is 1 to 40 vol.-% and the diene proportion is less than 50 wt.-%; and (F) 0 to 5 wt.-% of further additives and/or processing aids (F).
-
公开(公告)号:US20190119481A1
公开(公告)日:2019-04-25
申请号:US16094789
申请日:2017-04-18
Applicant: INEOS STYROLUTION GROUP GMBH
Inventor: Janna MICHAELIS DE VASCONCELLOS , Norbert NIESSNER , KwanHee LEE , Gisbert MICHELS
CPC classification number: C08L25/12 , C08L2205/025 , C08L2205/035 , C08L2205/06 , F25D23/066 , C08L55/02 , C08L53/02
Abstract: Thermoplastic molding compositions can be used in hydrofluoro olefin containing areas, comprising components A, B, C and D: 10 to 35 wt.-% ABS graft rubber copolymer A obtained by emulsion polymerization; 50 to 70 wt.-% SAN copolymer B; 4 to 20 wt.-% elastomeric SBC block copolymer C, and 4 to 20 wt.-% ABS graft rubber copolymer D obtained by mass polymerization.
-
-
-