Grain aggregate and producing method thereof, and light-diffusing agent
    1.
    发明授权
    Grain aggregate and producing method thereof, and light-diffusing agent 失效
    颗粒聚集体及其制备方法和光扩散剂

    公开(公告)号:US06610405B2

    公开(公告)日:2003-08-26

    申请号:US09847367

    申请日:2001-05-03

    IPC分类号: B32B516

    摘要: A grain aggregate is formed by bonding a plurality of cross-linking polymeric grains via a substance (binder) having a reactive functional group, and alternatively, the grain aggregate is formed by bonding at least two different types of a plurality of grains, thus providing the grain aggregate having the improved heat resistance, solvent resistance, strength and light-diffusing properties. Further, a light-diffusing agent made up of the grain aggregate has the improved light-diffusing properties. Therefore, when applying a light-diffusing mold article including the light-diffusing agent to, for example, a backlight of a liquid crystal display device, high brightness and a wide angle of visibility can be attained. Further, by spray drying of a dispersion liquid containing the grain aggregate, the grain aggregate can be produced with ease.

    摘要翻译: 通过通过具有反应性官能团的物质(粘合剂)将多个交联聚合物颗粒结合而形成颗粒聚集体,或者,通过粘结至少两种不同类型的多个颗粒形成颗粒聚集体,从而提供 所述颗粒聚集体具有改善的耐热性,耐溶剂性,强度和光扩散性能。 此外,由粒状集合体构成的光扩散剂具有改善的光扩散性。 因此,当将例如包含光扩散剂的光扩散模制品应用于例如液晶显示装置的背光源时,可以获得高亮度和广视角。 此外,通过喷雾干燥含有颗粒聚集体的分散液,可以容易地制备颗粒聚集体。

    Thermosetting resin potting composition
    2.
    发明授权
    Thermosetting resin potting composition 有权
    热固性树脂灌封组合物

    公开(公告)号:US06169136A

    公开(公告)日:2001-01-02

    申请号:US09134564

    申请日:1998-08-14

    IPC分类号: C08K300

    CPC分类号: C08K3/36

    摘要: The present invention provides a thermosetting resin potting composition with low melt viscosity and good flowability even though it contains large amount of an inorganic filler containing sphere silica powder as a main component. With this construction, the present invention has solved the problem residing in the prior art that, when the content of an inorganic filler is increased, the viscosity of a potting composition is increased and its flowability is lowered. In the present invention, the sphere silica particles in the inorganic filler have at least one particle group, and the particle group has an average particle diameter of 0.01 to 10 &mgr;m and a coefficient of particle diameter variation of 10 percent or smaller. More preferably, the sphere silica particles have two or more particle groups. In this case, the average particle diameter of the larger particle group is 1.4 times or larger than that of its adjacent and smaller particle group.

    摘要翻译: 本发明提供即使含有大量含有球状二氧化硅粉末的无机填充剂作为主要成分的熔融粘度低,流动性好的热固性树脂灌封组合物。 利用这种结构,本发明解决了现有技术中存在的问题:当无机填料的含量增加时,灌封组合物的粘度增加,流动性降低。在本发明中,球状二氧化硅 无机填料中的粒子具有至少一个粒子群,粒子群的平均粒径为0.01〜10μm,粒径变化系数为10%以下。 更优选地,球状二氧化硅颗粒具有两个或更多个颗粒组。 在这种情况下,较大粒子群的平均粒径为其相邻且较小粒子群的平均粒径的1.4倍以上。

    Silica base particles and production process for same
    3.
    发明授权
    Silica base particles and production process for same 失效
    二氧化硅基体颗粒和生产工艺相同

    公开(公告)号:US6150434A

    公开(公告)日:2000-11-21

    申请号:US208259

    申请日:1998-12-09

    IPC分类号: C08K9/04 C08K9/00

    CPC分类号: C08K9/04

    摘要: Provided is a silica base particle having an average particle diameter of 0.01 to 10 .mu.m, wherein carboxylic esters are present on the surface of the above particle in a proportion falling in a range of 0.05 to 10% by weight based on the weight of the above particle. A polyester film containing the above silica base particles shows an excellent lubricant property and scratch resistance.

    摘要翻译: 本发明提供平均粒径为0.01〜10μm的二氧化硅基粒子,其中羧酸酯以上述粒子的重量为基准,为0.05〜10重量% 颗粒以上。 含有上述二氧化硅基础颗粒的聚酯膜显示出优异的润滑性和耐擦伤性。

    Calcined silica particle and manufacturing method of same
    4.
    发明申请
    Calcined silica particle and manufacturing method of same 审中-公开
    煅烧二氧化硅颗粒及其制备方法

    公开(公告)号:US20070160520A1

    公开(公告)日:2007-07-12

    申请号:US11710445

    申请日:2007-02-26

    IPC分类号: C01B33/12 B60C1/00

    摘要: Provided is a calcined silica particle and a manufacturing method of the same, the calcined silica particle having a low hygroscopicity, and a narrow range of particle size distribution, and substantially even particle diameter, and containing little of large-diameter fused aggregation of the particulates of the calcined silica particle. A silica particle is obtained by hydrolyzing and condensing a hydrolyzable silicon compound in an organic solvent containing water, for example, at a reaction temperature ranging from 0° C. to 50° C., and then dried. Then, the silica particle is calcined at a temperature ranging from 1000° C. to 1200° C. It is preferable that the organic solvent contains the silicon compound in a range between 0.05 to 1.2 mol/L, the water in a range between 2.0 to 25.0 mol/L, and a catalyst in a range between 0.8 to 9.4 mol/L. The calcined silica particle has an average particle diameter ranging between 0.04 μm and 5.0 μm; a standard deviation of the average particle diameter of 1.3 μm or less; a moisture absorption amount of 0.2 wt % or less, measured after the calcined silica particle is kept for 1 day in an environment at 30° C. and at 90% relative humidity; and a content of a fused aggregation of the calcined silica particle of 0.02 wt % or less, the fused aggregation having a particle diameter of 20 μm or more.

    摘要翻译: 提供了煅烧二氧化硅颗粒及其制造方法,煅烧二氧化硅颗粒具有低吸湿性,窄范围的粒度分布,基本上均匀的粒径,并且几乎不含有微粒的大直径熔融聚集体 的煅烧二氧化硅颗粒。 通过在含水的有机溶剂中,例如在0℃至50℃的反应温度下水解和缩合可水解的硅化合物而获得二氧化硅颗粒,然后干燥。 然后,将二氧化硅粒子在1000℃〜1200℃的温度范围内进行煅烧。优选有机溶剂含有0.05〜1.2mol / L的硅化合物,2.0〜 至25.0mol / L,催化剂为0.8〜9.4mol / L。 煅烧二氧化硅颗粒的平均粒径在0.04μm和5.0μm之间; 平均粒径的标准偏差为1.3μm以下; 在30℃,90%相对湿度的环境下,煅烧二氧化硅粒子保持1天后测定的0.2重量%以下的吸湿量; 和煅烧二氧化硅颗粒的熔融聚集物的含量为0.02重量%以下,熔融聚集体的粒径为20μm以上。

    AMORPHOUS SILICA AND PROCESS FOR PRODUCING SAME
    6.
    发明申请
    AMORPHOUS SILICA AND PROCESS FOR PRODUCING SAME 审中-公开
    非晶硅和其生产方法

    公开(公告)号:US20120202923A1

    公开(公告)日:2012-08-09

    申请号:US13502850

    申请日:2010-10-20

    IPC分类号: C08L63/00 B29C39/18

    摘要: Provided are amorphous silica particles for application to industrial fields where there are increasing desires for high purity and colorlessness. The amorphous silica particles are produced through the steps of hydrolysis of an alkoxide, vacuum drying, and firing. The amorphous silica particles have been reduced in coloration and in Fe content, which is causative of coloration of the silica, and can meet the desires. The amorphous silica is characterized by having an Fe content of 20 ppm or less.

    摘要翻译: 提供了用于工业领域的无定形二氧化硅颗粒,其中对于高纯度和无色性的需求日益增加。 无定形二氧化硅颗粒通过醇盐水解,真空干燥和烧制的步骤制备。 无定形二氧化硅颗粒的着色和Fe含量已经降低,这是二氧化硅着色的原因,并且可以满足欲望。 无定形二氧化硅的特征在于Fe含量为20ppm以下。

    Process for preparing an aqueous resin dispersion and an aqueous resin
dispersion obtained by the process
    7.
    发明授权
    Process for preparing an aqueous resin dispersion and an aqueous resin dispersion obtained by the process 失效
    制备水性树脂分散体的方法和通过该方法获得的水性树脂分散体

    公开(公告)号:US5543456A

    公开(公告)日:1996-08-06

    申请号:US311341

    申请日:1994-09-23

    IPC分类号: C08F6/00 C08L61/02

    CPC分类号: C08F6/003

    摘要: A process for preparing an aqueous resin dispersion includes the steps of copolymerizing a polymeric monomer whose ratio of (meth) acrolein to a total amount of the (meth) acrolein and a vinyl monomer is in the range from 10 weight % to 80 weight % in an organic solvent to obtain a copolymer solution, dispersing the obtained copolymer solution in an aqueous medium and removing an unreacted (meth) acrolein. Since the above process can extremely reduce contents of the unreacted (meth) acrolein and of an oligomer whose number-average molecular weight is less than 1000, an aqueous resin dispersion where problems of a pungent smell, toxicological properties, etc. due to the (meth) acrolein and the oligomer are eliminated can be provided.

    摘要翻译: 制备水性树脂分散体的方法包括以下步骤:(甲基)丙烯醛与(甲基)丙烯醛和乙烯基单体的总量的比例为10重量%至80重量%的聚合单体的共聚 得到共聚物溶液,将得到的共聚物溶液分散在水性介质中,除去未反应的(甲基)丙烯醛。 由于上述方法可以极大地降低未反应的(甲基)丙烯醛和数均分子量小于1000的低聚物的含量,所以由于((甲基)丙烯醛和/ 甲基)丙烯醛和低聚物被除去。

    Method for production of cyclohexanecarboguanamine
    10.
    发明授权
    Method for production of cyclohexanecarboguanamine 失效
    生产环己烷甲酰胺的方法

    公开(公告)号:US4973689A

    公开(公告)日:1990-11-27

    申请号:US279938

    申请日:1988-12-05

    IPC分类号: C07D251/18

    CPC分类号: C07D251/18

    摘要: In a method for the production of cyclohexanecarboguanamine by the reaction of cyanocyclohexane with dicyandiamide in an organic solvent possessing a hydroxyl group in the molecular unit thereof at a temperature in the range of 90.degree. to 200.degree. C. in the presence of a basic catalyst, the improvement which comprises carrying out the reaction using 0.60 to 0.95 mol of dicyandiamide per mol of cyanocyclohexane in an atmosphere substantially incapable of producing any effect of oxygen.