摘要:
A connection structure of a superconducting layer of an embodiment incudes a first superconducting member including a first superconducting layer, and extends in a first direction, a second superconducting member including a second superconducting layer facing the first superconducting layer, and extends in the first direction, the second superconducting member having a first region, a second region, and a third region which is separated in the second direction from the second region, and a connection layer that contains a rare earth element (RE), barium (Ba), copper (Cu), and oxygen (O), and connects the first superconducting layer and the second superconducting layer. The first superconducting layer is present in a third direction between the second region and the third region, the third direction being perpendicular to the first direction and perpendicular to the second direction.
摘要:
A connection structure for a superconducting layer according to an embodiment includes a first superconducting layer; a second superconducting layer; and a connection layer disposed between the first superconducting layer and the second superconducting layer, the connection layer including crystal grains containing a rare earth element (RE), barium (Ba), copper (Cu), and oxygen (O), the crystal grains having a grain size distribution including a bimodal distribution. The bimodal distribution includes a first distribution including a first peak and a second distribution including a second peak. A first grain size corresponding to the first peak is larger than a second grain size corresponding to the second peak. Among the crystal grains, crystal grains having a grain size corresponding to the first distribution include a crystal grain having a plate shape or a flat shape.
摘要:
A two-stage heat regenerating cryogenic refrigerator may include: a vacuum vessel; a first and second cylinder in the vessel; the second cylinder coaxially connected to the first cylinder; a 1st regenerator in the first cylinder and accommodating heat regenerating material (HRM) 1; and a second regenerator in the 2nd cylinder accommodating HRM 2, HRM 2 including HRM particles, each HRM particle including a metal element and a heat regenerating substance including an oxide or oxysulfide and having a maximum specific heat at ≤20 K of ≥0.3 J/cm3·K; each HRM particle including a 1st and 2nd region, the 2nd region being closer to each HRM particle's outer edge than the 1st, and the 2nd region having a higher metal element concentration than the 1st, the 1st and 2nd region containing the heat regenerating substance.
摘要:
According to an embodiment, a cryogenic regenerator material contains a silver oxide. A molar ratio of silver atoms to oxygen atoms contained in the cryogenic regenerator material: Ag/O is 1.0 or more and 4.0 or less. The cryogenic regenerator material contains at least one selected from AgO, Ag2O and Ag3O as the silver oxide.
摘要:
A magnetic material is disclosed, which includes magnetic particles containing at least one magnetic metal selected from the group including Fe, Co and Ni, and at least one non-magnetic metal selected from Mg, Al, Si, Ca, Zr, Ti, Hf, Zn, Mn, rare earth elements, Ba and Sr; a first coating layer of a first oxide that covers at least a portion of the magnetic particles; oxide particles of a second oxide that is present between the magnetic particles and constitutes an eutectic reaction system with the first oxide; and an oxide phase that is present between the magnetic particles and has an eutectic structure of the first oxide and the second oxide.
摘要:
Provided is a method for producing a magnetic material. The method includes preparing magnetic metal particles containing at least one magnetic metal selected from a first group consisting of Fe, Co and Ni, and at least one non-magnetic metal selected from a second group consisting of Mg, Al, Si, Ca, Zr, Ti, Hf, Zn, Mn, Ba, Sr, Cr, Mo, Ag, Ga, Sc, V, Y, Nb, Pb, Cu, In, Sn and rare earth elements, pulverizing and reaggregating the magnetic metal particles, and thereby forming composite particles containing a magnetic metal phase and an interstitial phase, and heat-treating the composite particles at a temperature of from 50° C. to 800° C. The particle size distribution of the magnetic metal particles in the preparing magnetic metal particles has two or more peaks.
摘要:
A radio wave absorber according to an embodiment includes a plurality of metal particles including at least one kind of magnetic metal element selected from a first group of Fe, Co, and Ni. Each of the plurality of metal particles has a linear expansion coefficient of 1×10−6/K or more and 10×10−6/K or less. The radio wave absorber also includes a binding layer binding the metal particles and having higher resistance than the metal particle, wherein a volume filling ratio of the metal particles in the radio wave absorber is 10% or more and 50% or less.
摘要:
A connection structure of a superconducting layer according to an embodiment includes a first superconducting layer, a second superconducting layer, and a connection layer provided between the first superconducting layer and the second superconducting layer and including a first substance containing a rare earth element, barium, copper, and oxygen and a second substance containing a metal element, in which a first region per unit area at a first interface between the first superconducting layer and the connection layer is 1% or more and 50% or less where the second substance and the first superconducting layer are in contact with each other, and a second region per unit area at a second interface between the second superconducting layer and the connection layer is 1% or more and 50% or less where the second substance and the second superconducting layer are in contact with each other.
摘要:
Provided is a magnetic material including a plurality of flat particles containing a magnetic metal, and a matrix phase disposed around the flat particles and having higher electrical resistance than the flat particles. In a cross-section of the magnetic material, the aspect ratio of the flat particles is 10 or higher. If the major axis of one of the flat particles is designated as L and the length of a straight line connecting two endpoints of the flat particle is designated as W, the proportion of the area surrounded by the outer peripheries of parts in which flat particles satisfying the relationship: W ≤0.95×L are continuously laminated, is 10% or more of the cross-section.
摘要:
A magnetic metal particle aggregate includes a plurality of magnetic metal particles including at least one magnetic metal selected from a first group consisting of Fe, Co, and Ni. The plurality of magnetic metal particles are partly bound with each other, and an average particle diameter of the plurality of magnetic metal particles is 10 nm or more and 50 nm or less. The magnetic metal particle aggregate has an average particle diameter of 15 nm or more and 200 nm or less.