摘要:
A composition of a stabilized fibroblast growth factor (FGF), which contains an aluminum salt of cyclodextrin sulfate to stabilize FGF. FGF can be stabilized by forming a composition of FGF and an aluminum salt of cyclodextrin sulfate, and can be stably prepared into formulations.
摘要:
A steel for a welded structure includes the following composition: by mass %, C at a C content [C] of 0.010 to 0.065%; Si at a Si content [Si] of 0.05 to 0.20%; Mn at a Mn content [Mn] of 1.52 to 2.70%; Ni at a Ni content [Ni] of 0.10% to 1.50%; Ti at a Ti content [Ti] of 0.005 to 0.015%; O at an O content [O] of 0.0010 to 0.0045%; N at a N content [N] of 0.002 to 0.006%; Mg at a Mg content [Mg] of 0.0003 to 0.003%; Ca at a Ca content [Ca] of 0.0003 to 0.003%; and the balance composed of Fe and unavoidable impurities. A steel component parameter PCTOD is 0.065% or less, and a steel component hardness parameter CeqH is 0.235% or less.
摘要:
A method of production of 780 MPa class high strength steel plate excellent low temperature toughness comprising heating a steel slab of containing, by mass %, C: 0.06 to 0.15%, Si: 0.05 to 0.35%, Mn: 0.60 to 2.00%, P: 0.015% or less, S: 0.015% or less, Cu: 0.1 to 0.5%, Ni: 0.1 to 1.5%, Cr: 0.05 to 0.8%, Mo: 0.05 to 0.6%, Nb: less than 0.005%, V: 0.005 to 0.060%, Ti: less than 0.003%, Al: 0.02 to 0.10%, B: 0.0005 to 0.003%, and N: 0.002 to 0.006% to 1050° C. to 1200° C. in temperature, hot rolling ending at 870° C. or more, waiting for 10 seconds to 90 seconds, then cooling from 840° C. or more in temperature by a 5° C./s or more cooling rate to 200° C., then tempering at 450° C. to 650° C. in temperature for 20 minutes to 60 minutes.
摘要:
A method of production of 780 MPa class high strength steel plate excellent low temperature toughness comprising heating a steel slab of containing, by mass %, C: 0.06 to 0.15%, Si: 0.05 to 0.35%, Mn: 0.60 to 2.00%, P: 0.015% or less, S: 0.015% or less, Cu: 0.1 to 0.5%, Ni: 0.1 to 1.5%, Cr: 0.05 to 0.8%, Mo: 0.05 to 0.6%, Nb: less than 0.005%, V: 0.005 to 0.060%, Ti: less than 0.003%, Al: 0.02 to 0.10%, B: 0.0005 to 0.003%, and N: 0.002 to 0.006% to 1050° C. to 1200° C. in temperature, hot rolling ending at 870° C. or more, waiting for 10 seconds to 90 seconds, then cooling from 840° C. or more in temperature by a 5° C./s or more cooling rate to 200° C., then tempering at 450° C. to 650° C. in temperature for 20 minutes to 60 minutes.
摘要:
A steel for a welded structure includes the following composition: by mass %, C at a C content [C] of 0.010 to 0.065%; Si at a Si content [Si] of 0.05 to 0.20%; Mn at a Mn content [Mn] of 1.52 to 2.70%; Ni at a Ni content [Ni] of 0.10% to 1.50%; Ti at a Ti content [Ti] of 0.005 to 0.015%; 0 at an O content [O] of 0.0010 to 0.0045%; N at a N content [N] of 0.002 to 0.006%; Mg at a Mg content [Mg] of 0.0003 to 0.003%; Ca at a Ca content [Ca] of 0.0003 to 0.003%; and the balance composed of Fe and unavoidable impurities. A steel component parameter PCTOD is 0.065% or less, and a steel component hardness parameter CeqH is 0.235% or less.
摘要:
The present invention is to provide a viscous preparation for dental use which comprises basic fibroblast growth factor (bFGF) as an effective ingredient, and further a thickener; a kit for preparing the viscous preparation for dental use; and a method for preparing the viscous preparation for dental use.
摘要:
A steel for a welded structure includes the following composition: by mass %, C at a C content [C] of 0.015 to 0.045%; Si at a Si content [Si] of 0.05 to 0.20%; Mn at a Mn content [Mn] of 1.5 to 2.0%; Ni at a Ni content [Ni] of 0.10 to 1.50%; Ti at a Ti content [Ti] of 0.005 to 0.015%; O at an O content [O] of 0.0015 to 0.0035%; and N at a N content [N] of 0.002 to 0.006%, and a balance composed of Fe and unavoidable impurities. In the steel for a welded structure, the P content [P] is limited to 0.008% or less, the S content [S] is limited to 0.005% or less, the Al content [Al] is limited to 0.004% or less, the Nb content [Nb] is limited to 0.005% or less, the Cu content [Cu] is limited to 0.24% or less, the V content [V] is limited to 0.020% or less, and a steel composition parameter PCTOD is 0.065% or less, and a steel composition hardness parameter CeqH is 0.235% or less.
摘要:
The present invention provides a high strength thick steel plate for marine structures superior in weldability and low temperature toughness of the HAZ, which is able to be produced at a low cost without use of a complicated method of production, and a method of production of the same, that is, steel for welded structures excellent in low temperature toughness of the weld heat affected zone and a method of production of the same characterized by casting molten steel containing, by mass %, C: 0.03 to 0.12%, Si: 0.05 to 0.30%, Mn: 1.2 to 3.0%, P: 0.015% or less, S: 0.001 to 0.015%, Cu+Ni: 0.10% or less, Al: 0.001 to 0.050%, Ti: 0.005 to 0.030%, Nb: 0.005 to 0.10%, and N: 0.0025 to 0.0060% by the continuous casting method, making the cooling rate from near the solidification point to 800° C. in the secondary cooling at that time 0.06 to 0.6° C./s, hot rolling the obtained slab, and cooling it from a temperature of 800° C. or more.
摘要:
The present invention provides high strength steel having unprecedentedly superior CTOD (fracture toughness) properties satisfying not only the CTOD properties of the FL zone at −60° C., but also the CTOD properties of the ICHAZ zone in small and medium heat input multilayer welding etc. and a method of production of the same.The steel of the present invention is steel superior in CTOD properties of the heat-affected zone containing, by mass %, C: 0.015 to 0.045%, Si: 0.05 to 0.2%, Mn: 1.5 to 2.0%, Cu: 0.25 to 0.5%, Ni: 0.7 to 1.5%, P: 0.008% or less, S: 0.005% or less, Al: 0.004% or less, Ti: 0.005 to 0.015%, Nb: 0.005% or less, 0: 0.0015 to 0.0035%, and N: 0.002 to 0.006%, PCTOD: 0.065 or less, CeqH: 0.235 or less and the balance consisting of Fe and unavoidable impurities.
摘要:
The present invention provides a high strength thick steel plate for marine structures superior in weldability and low temperature toughness of the HAZ, which is able to be produced at a low cost without use of a complicated method of production, and a method of production of the same, that is, steel for welded structures excellent in low temperature toughness of the weld heat affected zone and a method of production of the same characterized by casting molten steel containing, by mass%, C: 0.03 to 0.12%, Si: 0.05 to 0.30%, Mn: 1.2 to 3.0%, P: 0.015% or less, S: 0.001 to 0.015%, Cu+Ni: 0.10% or less, Al: 0.001 to 0.050%, Ti: 0.005 to 0.030%, Nb: 0.005 to 0.10%, and N: 0.0025 to 0.0060% by the continuous casting method, making the cooling rate from near the solidification point to 800° C. in the secondary cooling at that time 0.06 to 0.6° C./s, hot rolling the obtained slab, and cooling it from a temperature of 800° C. or more.