Blow molding polyethylene resins
    1.
    发明申请
    Blow molding polyethylene resins 审中-公开
    吹塑聚乙烯树脂

    公开(公告)号:US20070027276A1

    公开(公告)日:2007-02-01

    申请号:US11190481

    申请日:2005-07-27

    IPC分类号: C08F4/06

    摘要: Disclosed herein are various processes, including continuous fluidized-bed gas-phase polymerization processes for making a high strength, high density polyethylene copolymer, comprising (including): contacting monomers that include ethylene and optionally at least one non-ethylene monomer with fluidized catalyst particles in a gas phase in the presence of hydrogen gas at an ethylene partial pressure of 100 psi or more and a polymerization temperature of 105° C. or less to produce a polyethylene copolymer having a density of 0.945 g/cc or more and an ESCR Index of 1.0 or more wherein the catalyst particles are prepared at an activation temperature of 700° C. or less, and include silica, chromium, and titanium.

    摘要翻译: 本文公开了各种方法,包括用于制备高强度,高密度聚乙烯共聚物的连续流化床气相聚合方法,包括(包括):使包含乙烯和任选的至少一种非乙烯单体的单体与流化催化剂颗粒接触 在气相存在下,在乙烯分压为100psi以上且聚合温度为105℃以下的氢气存在下,生成密度为0.945g / cc以上的聚乙烯共聚物和ESCR指数 为1.0以上,其中催化剂颗粒在700℃或更低的活化温度下制备,并且包括二氧化硅,铬和钛。

    Hindered polyalicyclic alkyl catalysts and their use in a gas-phase polymerization reactor
    2.
    发明申请
    Hindered polyalicyclic alkyl catalysts and their use in a gas-phase polymerization reactor 有权
    受阻的多环脂族烷基催化剂及其在气相聚合反应器中的应用

    公开(公告)号:US20060128908A1

    公开(公告)日:2006-06-15

    申请号:US11249193

    申请日:2005-10-13

    IPC分类号: C08F2/00

    摘要: Embodiments of the present invention include a method of polymerizing olefins comprising contacting olefins with a catalyst composition made by the process of combining a hindered polyalicyclic alkyl catalyst precursor with a particulate inorganic oxide for a deposition time greater than 2 hours to form a catalyst composition. Embodiments of the present invention also include catalyst compositions comprising a hindered polyalicyclic alkyl catalyst precursor made by the process of combining the hindered polyalicyclic alkyl catalyst precursor with a particulate inorganic oxide for a deposition time greater than 2 hours to form the catalyst composition. In one embodiment, the hindered polyalicyclic alkyl catalyst precursor is formed by first combining an acid, a compound having the formula RX, and a metal oxide selected from the group consisting of Group 3 to Group 10 oxide compounds to produce a catalyst precursor; characterized in that R is selected from the group consisting of hindered polyalicyclic alkyls, and substituted derivatives thereof, and X is selected from the group consisting of any suitable leaving group.

    摘要翻译: 本发明的实施方案包括使烯烃聚合的方法,其包括使烯烃与通过将受阻多环脂族烷基催化剂前体与颗粒无机氧化物结合沉积时间大于2小时的方法制备的催化剂组合物形成催化剂组合物。 本发明的实施方案还包括催化剂组合物,其包含通过将受阻多环脂族烷基催化剂前体与颗粒无机氧化物结合沉积时间大于2小时的方法制备的受阻多环脂族烷基催化剂前体,以形成催化剂组合物。 在一个实施方案中,受阻多环脂族烷基催化剂前体通过首先组合酸,具有式RX的化合物和选自第3族至第10族氧化物化合物的金属氧化物以形成催化剂前体而形成; 其特征在于R选自受阻多环脂族烷基及其取代衍生物,X选自任何合适的离去基团。

    Condensing mode operation of gas-phase polymerization reactor
    3.
    发明申请
    Condensing mode operation of gas-phase polymerization reactor 审中-公开
    气相聚合反应器的冷凝模式运行

    公开(公告)号:US20050137364A1

    公开(公告)日:2005-06-23

    申请号:US10745456

    申请日:2003-12-23

    IPC分类号: C08F210/16 C08F2/00

    摘要: A continuous gas fluidized bed polymerization process for the production of a polymer from a monomer including continuously passing a gaseous stream comprising the monomer through a fluidized bed reactor in the presence of a catalyst under reactive conditions; withdrawing a polymeric product and a stream comprising unreacted monomer gases; cooling said stream comprising unreacted monomer gases to form a mixture comprising a gas phase and a liquid phase and reintroducing said mixture into said reactor with sufficient additional monomer to replace that monomer polymerized and withdrawn as the product, wherein said liquid phase is vaporized, and wherein the stream comprises an induced condensing agent selected from the group consisting of alkanes, cycloalkanes, and mixtures thereof, the induced condensing agent having a normal boiling point less than 25° C.

    摘要翻译: 一种用于从单体制备聚合物的连续气流流化床聚合方法,包括在反应条件下,在催化剂存在下连续通过包含单体的气流通过流化床反应器; 取出聚合物和包含未反应的单体气体的物流; 冷却所述物流包含未反应的单体气体以形成包含气相和液相的混合物,并用足够的其它单体将所述混合物重新引入所述反应器,以代替作为产物聚合和取出的单体,其中所述液相被蒸发,其中 该流包含选自烷烃,环烷烃及其混合物的诱导缩合剂,所述诱导的缩合剂的标准沸点低于25℃。