摘要: Disclosed is an adhesive composition including 100 parts by weight of lignin, 150 to 400 parts by weight of epoxy resin, and 7.5 to 200 parts by weight of flexibilizer. The lignin and the flexibilizer can be pre-reacted to enhance the physical properties, e.g. glass transition temperature (Tg) and flexural endurance (MIT), of the cured adhesive composition. Furthermore, the adhesive composition and a flexible metal foil can be laminated to form a flexible substrate.
摘要翻译: 公开了一种粘合剂组合物,其包含100重量份的木质素,150至400重量份的环氧树脂和7.5至200重量份的增韧剂。 木质素和增韧剂可以预反应以增强物理性质,例如 玻璃化转变温度(Tg)和弯曲耐久性(MIT)。 此外,粘合剂组合物和柔性金属箔可以层压以形成柔性基底。
-
公开(公告)号:US20120277349A1
公开(公告)日:2012-11-01
申请号:US13233521
申请日:2011-09-15
申请人: Cheng-Han HSIEH , Yung-Chan LIN , En-Nan LIU
发明人: Cheng-Han HSIEH , Yung-Chan LIN , En-Nan LIU
CPC分类号: C09K21/14 , C08H6/00 , C08L63/00 , C08L97/005 , C08L2201/02 , C08L77/00 , C08L77/06
摘要: Disclosed is a flame retardant agent, including a nitrogen-based lignin formed by reacting 1 part by weight of lignin, 0.8 to 2.4 parts by weight of a nitrogen-containing compound, and 0.3 to 0.9 parts by weight of an aldehyde under an alkaline condition. The flame retardant agent can be added to thermoplastic or thermosetting resins to form flame retardant materials.
摘要翻译: 公开了一种阻燃剂,其包括在碱性条件下使1重量份的木质素,0.8至2.4重量份的含氮化合物和0.3至0.9重量份的醛反应形成的氮基木质素 。 可以将阻燃剂加入到热塑性或热固性树脂中以形成阻燃材料。
-