Rubber composition containing modified conjugated diene-based polymer bonded to fullerene
    3.
    发明申请
    Rubber composition containing modified conjugated diene-based polymer bonded to fullerene 审中-公开
    含有与富勒烯键合的改性共轭二烯类聚合物的橡胶组合物

    公开(公告)号:US20060270784A1

    公开(公告)日:2006-11-30

    申请号:US10553963

    申请日:2004-04-28

    IPC分类号: C08L9/00

    CPC分类号: B82Y30/00 B60C1/00 C08L19/006

    摘要: A rubber composition obtained by compounding thereinto a rubber component containing 0.5 to 100% by weight of a modified conjugated diene-based polymer having a fullerene bonded thereto in the molecule and having a weight average molecular weight of 50,000 or more excellent processability, superior balance of modulus and heat buildup, excellent cold flowability and superior tan δ balance.

    摘要翻译: 通过在分子中配合含有0.5〜100重量%的具有与其结合的富勒烯的改性共轭二烯系聚合物,重均分子量为50,000以上,优异的加工性的橡胶组合物,优异的平衡性 模量和热积累,优异的冷流动性和优异的tanδ平衡。

    Process for production of rubber composition
    4.
    发明授权
    Process for production of rubber composition 失效
    橡胶组合物生产工艺

    公开(公告)号:US6077899A

    公开(公告)日:2000-06-20

    申请号:US952486

    申请日:1997-11-19

    IPC分类号: C08L15/00 C08L9/06 C08L9/00

    CPC分类号: C08L15/00 C08K3/04 C08L9/00

    摘要: (i) A starting rubber (A) comprising a terminal-modified and/or coupled diene rubber and having an average glass transition temperature TgA (.degree. C.) is mixed with a specific amount of the reinforcing agent are mixed at a temperature of at least 135.degree. C., followed by adding a starting rubber (B) comprising a terminal unmodified diene rubber and having a specific average glass transition temperature TgB (.degree. C.), and the remaining reinforcing agent and a softening agent; (ii) a starting diene rubber (A') having a specific weight average molecular weight Mw(A') and average glass transition temperature TgA' (.degree. C.) is contacted with a reinforcing agent, followed by adding a starting diene rubber (B') having a specific weight average molecular weight Mw(B) and average glass transition temperature TgB' (.degree. C.), and a softening agent to produce a rubber composition; or (iii) 100 parts by weight of a starting rubber comprising a starting rubber (A") comprising 20 to 100% by weight of a terminal-modified and/or coupled diene rubber and a starting rubber (B") comprising a terminal-unmodified and/or uncoupled rubber are mixed with a specific carbon black (X) in specific amounts at a temperature of at least 135.degree. C., followed by adding the starting rubber (B") and the remaining carbon black and a softening agent.

    摘要翻译: PCT No.PCT / JP96 / 03635 Sec。 371日期:1997年11月19日 102(e)日期1997年11月19日PCT Filted 1996年12月12日PCT公布。 第WO97 / 48766号公报 日期1997年12月24日(i)将具有平均玻璃化转变温度TgA(℃)的末端改性和/或偶合二烯橡胶的起始橡胶(A)与特定量的增强剂混合 在至少135℃的温度下混合,然后加入包含末端未改性二烯橡胶并具有比平均玻璃化转变温度TgB(℃)的起始橡胶(B),剩余的增强剂和软化 代理人 (ii)具有比重重均分子量Mw(A')和平均玻璃化转变温度TgA'(℃)的起始二烯橡胶(A')与增强剂接触,然后加入起始二烯橡胶( 具有比重重均分子量Mw(B)和平均玻璃化转变温度TgB'(℃)的软化剂B')和软化剂以产生橡胶组合物; 或(iii)100重量份的起始橡胶,其包含起始橡胶(A“),其包含20至100重量%的末端改性和/或偶合的二烯橡胶和起始橡胶(B”),其包含 末端未改性和/或未偶联的橡胶与特定碳黑(X)在至少135℃的温度下以特定量混合,随后加入起始橡胶(B“)和剩余的炭黑和 软化剂。