Polyphenylene sulfide composition and method of producing the same
    1.
    发明授权
    Polyphenylene sulfide composition and method of producing the same 失效
    聚苯硫醚组合物及其制备方法

    公开(公告)号:US4935473A

    公开(公告)日:1990-06-19

    申请号:US279098

    申请日:1988-12-02

    IPC分类号: C08L81/02 C08G75/02 C08K5/544

    摘要: The present invention discloses a composition comprising a mixture containing 100 parts by weight of substantially linear polyphenylene sulfide which is treated with an aqueous solution of an acid or a salt of a strong acid and a weak base and which has not less than 70 mol % of a repeating unit of ##STR1## 0.05 to 5 parts by weight of at least one aminoalkoxysilane compound and, if necessary, 0.01 to 3 parts by weight of a releasing agent, the mixture being kneaded under heating at a temperature higher than the melting point of the polyphenylene sulfide, said composition exhibiting excellent impact strength and weld strength and providing molded product with small amount of flash generated during molding. The invention also discloses a composition which further comprises a fibrous reinforcing material and/or an inorganic powdered or granular filler, according to necessity, as well as disclosing a method of producing said composition.

    Process for producing readily crystallizable arylenesulfide resin
composition containing organic acid or anhydride
    4.
    发明授权
    Process for producing readily crystallizable arylenesulfide resin composition containing organic acid or anhydride 失效
    制备含有机酸或酸酐的容易结晶的芳基硫醚树脂组合物的方法

    公开(公告)号:US4699975A

    公开(公告)日:1987-10-13

    申请号:US836509

    申请日:1986-03-05

    摘要: A readily crystallizable arylenesulfide resin composition is produced by adding, to 100 parts by weight of an arylenesulfide polymer, 0.01 to 10.0 parts of an organic acid or organic acid anhydride having a high boiling or melting point such as 2,6-naphthalene dicarboxylic acid, and then heating the mixture to a temperature not lower than the melting point of the polymer. The resulting resin composition is characterized in that its crystallization from its glass state and molten state is very rapid, in that it forms very fine spherulite structures, and in that it has a high degree of crystallization, a very crystallizable character, and other desirable characteristics.

    摘要翻译: 通过向100重量份的芳基硫化物聚合物中加入0.01至10.0重量份具有高沸点或高沸点的有机酸或有机酸酐的化合物,例如2,6-萘二甲酸, 然后将混合物加热至不低于聚合物熔点的温度。 所得树脂组合物的特征在于,其玻璃态和熔融态的结晶非常快,因为其形成非常细的球晶结构,并且其具有高结晶度,非常可结晶的特性和其它所需特性 。

    Thermoformed polyarylene sulfide container
    5.
    发明授权
    Thermoformed polyarylene sulfide container 失效
    热成型聚芳硫醚容器

    公开(公告)号:US5187257A

    公开(公告)日:1993-02-16

    申请号:US902556

    申请日:1992-06-22

    IPC分类号: B29C51/00 B29D7/01 C08G75/02

    摘要: Disclosed herein is a crystallized, thin-wall container which is excellent in heat-resistance, oil-resistance, chemical stability under high temperature and high humidity and gas impermeability, is particularly suitable for heating foodstuffs packaged in it in electronic range, electric oven, etc. and is obtained by thermoforming a substantially amorphous sheet which has a crystallinity index of below 15% and an elongation of not less than 100% at room temperature and is obtained from a poly(arylene sulfide) which has a substantially linear structure, has not less thant 70 wt % of a repeating unit of ##STR1## and a logarithmic viscosity number of 0.2 to 1.0 in a solution of 1-chloronaphthalene (concentration of 0.4 g/dl at a temperature of 208.degree. C.) and a process for producing the container.

    摘要翻译: 本发明公开了一种结晶化的薄壁容器,其耐热性,耐油性,在高温和高湿度下的化学稳定性和气体不渗透性优异,特别适用于加热包装在电子范围,电烤箱中的食品, 并且通过在室温下热成型具有低于15%的结晶度指数和不小于100%的伸长率的基本上无定形的片材并且由具有基本上线性结构的聚(亚芳基硫醚)获得,具有 在1-氯萘(温度为208℃的浓度为0.4g / dl)的溶液中,不少于70重量%的重复单元“IMAGE”,对数粘度为0.2至1.0, 生产容器。

    Process for production of poly(arylene thioether) containing phthalic
anhydride groups
    7.
    发明授权
    Process for production of poly(arylene thioether) containing phthalic anhydride groups 失效
    含有邻苯二甲酸酐基团的聚(亚芳基硫醚)的制备方法

    公开(公告)号:US5554723A

    公开(公告)日:1996-09-10

    申请号:US35342

    申请日:1993-03-19

    IPC分类号: C08G75/02 C08G75/14

    CPC分类号: C08G75/02

    摘要: A process for the production of a poly(arylene thioether) containing phthalic anhydride groups wherein a dihalogen-substituted aromatic compound is reacted with an alkali metal sulfide in a polar organic solvent containing water to produce the poly(arylene thioether) is disclosed. This process comprises causing a monohalogen-substituted phthalic compound to exist in a polymerization reaction system, and controlling a ratio, a/b of the number of moles, a of the charged dihalogen-substituted aromatic compound to the number of moles, b of the charged alkali metal sulfide within a range of 0.8

    摘要翻译: 公开了一种制备含有邻苯二甲酸酐基团的聚(亚芳基硫醚)的方法,其中将二卤素取代的芳族化合物与碱金属硫化物在含水的极性有机溶剂中反应以制备聚(亚芳基硫醚)。 该方法包括使单卤素取代的邻苯二甲酸化合物存在于聚合反应体系中,并且控制加入的二卤代芳香族化合物的摩尔数a / b与摩尔数b的摩尔数 带电的碱金属硫化物在0.8

    Composition of polyarylene thioether
    9.
    发明授权
    Composition of polyarylene thioether 失效
    聚亚芳基硫醚的组成

    公开(公告)号:US4859734A

    公开(公告)日:1989-08-22

    申请号:US176155

    申请日:1988-03-31

    IPC分类号: C08L81/02 C08K3/34 C08K7/02

    CPC分类号: C08K3/346

    摘要: Disclosed herein is a composition of polyarylene thioether prepared by combining 0.001 to 10 parts by weight of kaoline of the mean particle diameter of 0.03 to 2 .mu.m with 100 parts by weight of polyarylene thioether having the repeating unit of ##STR1## as the main constituent. The composition of polyarylene thioether has a high crystallization rate and forms a minute spherulite structure. Moreover, the composition having a short molding cycle at the time of melt molding, generates a small amount of the flash and gives the molded products excellent in mechanical properties.Disclosed herein also is a composition prepared by further combining an inorganic filler and/or a fibrous filler with the above-mentioned composition of polyarylene thioether.

    Polyarylene thioether composition containing polyarylene ether
nucleating agent
    10.
    发明授权
    Polyarylene thioether composition containing polyarylene ether nucleating agent 失效
    聚亚芳基硫醚组合物含聚亚芳基醚成核剂

    公开(公告)号:US4837294A

    公开(公告)日:1989-06-06

    申请号:US182172

    申请日:1988-04-15

    IPC分类号: C08L81/02

    CPC分类号: C08L81/02

    摘要: Disclosed herein is a polyarylene thioether composition comprising: 100 parts by weight of a polyarylene thioether (A) which contains not less than 70 wt % of a repeating unit of ##STR1## and 0.01 to 15 parts by weight of a polyarylene thioether (B), which is a nucleating agent and contains not less than 50 wt % of a repeating unit of ##STR2## as the main constituent and has a melting point of not lower than 290.degree. C. or a melt crystallization temperature of not lower than 220.degree. C. This composition may further comprise 0.1 to 300 parts by weight of an inorganic filler and/or a fibrous filler. A 50% crystallization time, t.sub.1/2, at 250.degree. C. of the polyarylene thioether composition is not more than 1/1.5 of the 50% crystallization time of a polyarylene thioether which does not contain the polyarylene thioether (B) Accordingly, its melt molding cycle is short and its molded product has a high strength.