Detection of mercury in biological samples
    1.
    发明申请
    Detection of mercury in biological samples 审中-公开
    检测生物样品中的汞

    公开(公告)号:US20050208670A1

    公开(公告)日:2005-09-22

    申请号:US10805599

    申请日:2004-03-22

    IPC分类号: G01N27/42 G01N33/00 G01N33/12

    CPC分类号: G01N33/12 G01N27/42

    摘要: A device and method for determining mercury levels in a biological sample containing mercury. The biological sample is at least partially dissolved in an acidic solution to release at least a portion of the mercury contained therein. The partially dissolved biological sample is exposed to an anode and cathode under an electromotive force causing at least a portion of the mercury released from the biological sample to adhere to a surface of the cathode. The cathode being exposed to an alkaline metal salt to create a mercury-alkaline metal amalgam. This cathode is then electrically connected to a reference electrode whereby the extent of the amalgam is a measure of the level of mercury in the biological sample.

    摘要翻译: 用于测定含汞生物样品中汞含量的装置和方法。 生物样品至少部分地溶解在酸性溶液中以释放其中所含的汞的至少一部分。 部分溶解的生物样品在电动势下暴露于阳极和阴极,导致从生物样品释放的至少一部分汞粘附到阴极的表面。 阴极暴露于碱金属盐以产生汞 - 碱金属汞齐。 然后将该阴极电连接到参比电极,由此汞齐的程度是生物样品中汞水平的量度。

    Decreasing allergenicity of natural latex rubber prior to vulcanization
    2.
    发明申请
    Decreasing allergenicity of natural latex rubber prior to vulcanization 审中-公开
    硫化前降低天然胶乳的过敏原

    公开(公告)号:US20070083036A1

    公开(公告)日:2007-04-12

    申请号:US11249887

    申请日:2005-10-12

    IPC分类号: C08G16/02

    CPC分类号: C08C1/04

    摘要: A method for reducing allergenicity of natural latex rubber. The natural latex rubber, prior to its vulcanization, is admixed with silica compounds dissolved an alkali solution to denature the antigenic protein thus reducing the total protein level. Alternatively, liquid sodium silicate is added directly to natural rubber latex to reduce antigenic protein value. Ideally, when fumed silica is used as the silica compound, it is characterized as having a density of approximately 2.2 g/cm2 and surface area of 255 m2/g.

    摘要翻译: 降低天然乳胶橡胶过敏原的方法。 将天然乳胶橡胶在其硫化之前与溶解碱溶液的二氧化硅化合物混合以使抗原蛋白质变性,从而降低总蛋白质水平。 或者,将液体硅酸钠直接加入到天然橡胶胶乳中以降低抗原蛋白的价值。 理想情况下,当使用热解二氧化硅作为二氧化硅化合物时,其特征在于密度为约2.2g / cm 2,表面积为255m 2 / g。

    Process for the desulphurization and upgrading fuel oils
    3.
    发明授权
    Process for the desulphurization and upgrading fuel oils 失效
    燃油脱硫和升级工艺

    公开(公告)号:US06797126B2

    公开(公告)日:2004-09-28

    申请号:US10116257

    申请日:2002-04-03

    IPC分类号: C07C100

    摘要: A method of desulphurizing and cracking of hydrocarbons to produce fuel oil. The fuel oil is first admixed with a sensitizer and solid source of hydrogen and, preferably, with a catalyst and a desulphurizing agent. The admixture is then subjected to microwave energy. The method acts to reduce the sulphur content of the fuel oil and cracks the fuel oil into a useful source of clean, burnable energy.

    摘要翻译: 一种碳氢化合物脱硫和裂化生产燃料油的方法。 燃料油首先与敏化剂和固体氢源混合,优选与催化剂和脱硫剂混合。 然后将混合物进行微波能量。 该方法用于减少燃料油中的硫含量并将燃料油裂解成清洁,可燃的能量的有用来源。

    ANTI-VIRAL WASH
    4.
    发明申请
    ANTI-VIRAL WASH 审中-公开
    反法律洗礼

    公开(公告)号:US20160136202A1

    公开(公告)日:2016-05-19

    申请号:US14939337

    申请日:2015-11-12

    申请人: Travis Honeycutt

    发明人: Travis Honeycutt

    IPC分类号: A61K33/42 A61K33/00 A61K33/08

    摘要: An anti-viral wash composition composed of approximately 0.005% to 1.0% (wt.) aluminum hydroxide, approximately 0.1% to 0.001% (wt) sodium bicarbonate and approximately 0.1% to 0.001% (wt) trisodium phosphate.

    摘要翻译: 由大约0.005%至1.0%(重量)氢氧化铝,约0.1%至0.001%(wt)碳酸氢钠和约0.1%至0.001%(wt)磷酸三钠组成的抗病毒洗涤组合物。

    Decreasing allergenicity of natural latex rubber prior to vulcanization
    5.
    发明授权
    Decreasing allergenicity of natural latex rubber prior to vulcanization 有权
    硫化前降低天然胶乳的过敏原

    公开(公告)号:US07056970B2

    公开(公告)日:2006-06-06

    申请号:US11096421

    申请日:2005-04-04

    申请人: Travis Honeycutt

    发明人: Travis Honeycutt

    IPC分类号: C08K3/10

    CPC分类号: C08C1/04

    摘要: A method for reducing allergenicity of natural latex rubber. The natural latex rubber, prior to its vulcanization, is admixed with aluminum hydroxide to denature the antigenic protein thus reducing the total protein level considerably. Lignin or fumed silica can also be mixed with the aluminum hydroxide to reduce the protein value in latex. Ideally, the aluminum hydroxide is characterized as having a density of approximately 2.42 g/cm3 and molecular weight of 78.00.

    摘要翻译: 降低天然乳胶橡胶过敏原的方法。 天然乳胶橡胶在其硫化之前与氢氧化铝混合以使抗原蛋白质变性,从而显着降低总蛋白水平。 木质素或热解二氧化硅也可以与氢氧化铝混合以降低胶乳中的蛋白质值。 理想地,氢氧化铝的特征在于密度约为2.42g / cm 3,分子量为78.00。

    DECREASING ALLERGENICITY OF NATURAL LATEX RUBBER PRIOR TO VULCANIZATION
    7.
    发明申请
    DECREASING ALLERGENICITY OF NATURAL LATEX RUBBER PRIOR TO VULCANIZATION 有权
    降低天然橡胶的耐久性

    公开(公告)号:US20050277722A1

    公开(公告)日:2005-12-15

    申请号:US11096421

    申请日:2005-04-04

    申请人: Travis Honeycutt

    发明人: Travis Honeycutt

    IPC分类号: C08C1/04 C08K3/10

    CPC分类号: C08C1/04

    摘要: A method for reducing allergenicity of natural latex rubber. The natural latex rubber, prior to its vulcanization, is admixed with aluminum hydroxide to denature the antigenic protein thus reducing the total protein level considerably. Lignin or fumed silica can also be mixed with the aluminum hydroxide to reduce the protein value in latex. Ideally, the aluminum hydroxide is characterized as having a density of approximately 2.42 g/cm3 and molecular weight of 78.00.

    摘要翻译: 降低天然乳胶橡胶过敏原的方法。 天然乳胶橡胶在其硫化之前与氢氧化铝混合以使抗原蛋白质变性,从而显着降低总蛋白水平。 木质素或热解二氧化硅也可以与氢氧化铝混合以降低胶乳中的蛋白质值。 理想地,氢氧化铝的特征在于密度约为2.42g / cm 3,分子量为78.00。

    Decreasing allergenicity of natural latex rubber prior to vulcanization
    10.
    发明申请
    Decreasing allergenicity of natural latex rubber prior to vulcanization 审中-公开
    硫化前降低天然胶乳的过敏原

    公开(公告)号:US20100267896A1

    公开(公告)日:2010-10-21

    申请号:US11988498

    申请日:2005-07-14

    申请人: Travis Honeycutt

    发明人: Travis Honeycutt

    IPC分类号: C08G63/91

    摘要: A method for reducing allergenicity of natural latex rubber. The natural latex rubber, prior to its vulcanization, is admixed with aluminum hydroxide to denature the antigenic protein thus reducing the total protein level considerably. Lignin or fumed silica can also be mixed with the aluminum hydroxide to reduce the protein value in latex. Ideally, the aluminum hydroxide is characterized as having a density of approximately 2.42 g/cm3 and molecular weight of 78.00.

    摘要翻译: 降低天然乳胶橡胶过敏原的方法。 天然乳胶橡胶在其硫化之前与氢氧化铝混合以使抗原蛋白质变性,从而显着降低总蛋白水平。 木质素或热解二氧化硅也可以与氢氧化铝混合以降低胶乳中的蛋白质值。 理想地,氢氧化铝的特征在于密度约为2.42g / cm 3,分子量为78.00。