摘要:
A piezoelectric ceramic 10 composed mainly of a three-component solid solution represented by the following general formula (1), wherein x, y and z in general formula (1) satisfy the following formulas (2), (3), (4) and (5). x(Bi1/2Na1/2)TiO3−y(Bi1/2Li1/2)TiO3−z(Bi1/2K1/2)TiO3 (1) 0.80≦x≦0.96 (2) 0.02≦y≦0.08 (3) 0.01≦z≦0.15 (4) x+y+z=1 (5)
摘要:
A piezoelectric ceramic 10 composed mainly of a three-component solid solution represented by the following general formula (1), wherein x, y and z in general formula (1) satisfy the following formulas (2), (3), (4) and (5). x(Bi1/2Na1/2)TiO3-y(Bi1/2Li1/2)TiO3-z(Bi1/2K1/2)TiO3 (1) 0.80≦x≦0.96 (2) 0.02≦y≦0.08 (3) 0.01≦z≦0.15 (4) x+y+z=1 (5)
摘要:
A piezoelectric composition includes a compound represented by a general expression Bi4Ti3O12—SrBi4Ti4O15 as a main component; and Mn or a Mn compound as an additive. A Mn content is less than 1.0% by mass based on a main component amount.
摘要:
A piezoelectric ceramic composition which has a large electromechanical coupling factor and is excellent in heat resisting properties is provided. As additives, Cr, Al and Si are contained together in the piezoelectric ceramic composition including a perovskite compound which contains Pb, Zr and Ti as main components. Preferably, Cr, Al and Si are respectively contained in a content of 0.05 to 0.50 wt % in terms of Cr2O3, in a content of 0.005 to 1.500 wt % in terms of Al2O3, and in a content of 0.005 to 0.100 wt % in terms of SiO2. By simultaneously including these three elements and setting the contents thereof to fall within the above mentioned ranges, the electromechanical coupling factor kt can be 30% or more, and ΔFr, which is the rate of change in resonant frequency Fr between before and after application of an external thermal shock, can be 0.5% or less in absolute value.
摘要翻译:提供了具有大的机电耦合系数并且耐热性优异的压电陶瓷组合物。 作为添加剂,包含Pb,Zr和Ti作为主要成分的钙钛矿型化合物的压电陶瓷组合物中含有Cr,Al,Si。 优选地,Cr,Al和Si分别以Cr 2 Al 3 O 3含量为0.05〜0.50重量%,含量为0.005〜1.500重量% 以Al 2 O 3 3计,含量为0.005〜0.100重量%,以SiO 2 2计。 通过同时包含这三个要素并将其内容设定在上述范围内,机电耦合系数kt可以为30%以上,作为施加前后的谐振频率Fr的变化率的DeltaFr 外部热冲击的绝对值可以为0.5%以下。
摘要:
A piezoelectric ceramic composition including a perovskite-type oxide, wherein the perovskite-type oxide has Na, K, Li, Ba and Sr at the A site and Nb, Ta and Zr at the B site, and has a crystal phase transition in a temperature range of −50 to 150° C., the crystal phase transition being accompanied by an endotherm of no greater than 4 J/g, as well as a piezoelectric element 20 provided with a piezoelectric ceramic 1 that contains the piezoelectric ceramic composition.
摘要:
According to a preferred embodiment, the piezoelectric ceramic includes a complex oxide having the composition represented by formula (1) or (2), and Mn at 0.2-1.2 mass % or 0.2-3 mass %, respectively, in terms of MnCO3. (Pb1-aA1a)TixZr1-x-y-z-b(Zn1/3A22/3)y(Yb1/2A21/2)zSnbO3 (1) (Pb1-aA1a)TixZr1-x-y-b(Zn1/3A22/3)ySnbO3 (2) [In formula (1), A1 represents at least one element selected from the group consisting of Ca, Sr and Ba, and A2 is at least one element selected from the group consisting of Nb, Ta and Sb, and includes at least Nb. In formula (2), A1 represents at least one element selected from among Ca, Sr and Ba, A2 represents at least one element selected from among Nb and W, and A2 includes at least Nb.]
摘要:
Provided is a piezoelectric ceramic 1 containing a compound represented by the following general formula (1), as a main component and at least one element selected from Mn, Fe and Cu in an amount of 0.04 to 0.6% by mass based on the main component, and a vibrator 10 having the piezoelectric ceramic 1 and electrodes 2, 3. CaxBa1−xTiO3 (1) where, x satisfies 0.05≦x≦0.20.
摘要:
The piezoelectric element 20 of the invention comprises a pair of electrodes 2,3 and a piezoelectric ceramic 1 comprising as the major component a solid solution of the two components KNbO3 and BaTiO3. In the solid solution, the molar ratio of KNbO3 is 0.5-0.9 with respect to the total of the two components.
摘要:
The piezoelectric element 20 of the invention comprises a pair of electrodes 2,3 and a piezoelectric ceramic 1 comprising as the major component a solid solution of the two components KNbO3 and BaTiO3. In the solid solution, the molar ratio of KNbO3 is 0.5-0.9 with respect to the total of the two components.
摘要:
A piezoelectric ceramic composition including a perovskite-type oxide, wherein the perovskite-type oxide has Na, K, Li, Ba and Sr at the A site and Nb, Ta and Zr at the B site, and has a crystal phase transition in a temperature range of −50 to 150° C., the crystal phase transition being accompanied by an endotherm of no greater than 4 J/g, as well as a piezoelectric element 20 provided with a piezoelectric ceramic 1 that contains the piezoelectric ceramic composition.